# US 2006/0137717 A1 · Method for removing impurities grown on a phase shift mask

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0137717 A1
- Document ID: US20060137717A1
- Status: Published application
- Kind: A1
- Application number: 11/292,501
- Filed: 2005-12-01
- Published: 2006-06-29
- Earliest claimed: 2004-12-27
- Assignees: Hynix Semiconductor Inc.
- Inventors: Jun Lee
- Web page: https://patentgrep.com/patent/US20060137717A1

## CPC

- G03F 1/82: Auxiliary processes, e.g. cleaning or inspecting
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A method for removing impurities grown on a phase shift mask. The method can advantageously control growth of impurities by further performing HF cleaning and baking after cleaning to minimize the amount of residual chemical ions generated during cleaning. Specifically, the method comprises forming a phase shift mask pattern including a phase shift film and a light-blocking film on a quartz substrate, cleaning the phase shift mask pattern formed on the quartz substrate using a solution containing sulfuric acid ions or ammonium ions, cleaning the cleaned phase shift mask pattern using an aqueous HF solution, and baking the phase shift mask pattern cleaned with the aqueous HF solution.

## Claims

### Claim 1

A method for removing impurities grown on a phase shift mask, comprising:
forming a phase shift mask pattern including a phase shift film and a light-blocking film on a mask substrate;
cleaning the phase shift mask pattern formed on the mask substrate using a solution containing sulfuric acid ions or ammonium ions;
cleaning the cleaned phase shift mask pattern using an aqueous HF solution; and
baking the phase shift mask pattern cleaned with the aqueous HF solution.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the solution containing sulfuric acid ions or ammonium ions is a SPM (H2SO4+H2O2) or a SC-1 (Standard Clean-1) solution.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the aqueous HF solution includes HF and water in a mixing ratio ranging from 100:1 to 500:1.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the baking step is carried out using a hot plate.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the baking is conducted at 400° C. for 5 minutes while N2 gas is supplied at a flow rate of 3 sccm.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the baking is conducted while a gas, including He, is injected into a back surface of the mask on which the phase shift mask pattern is formed.