Polyethylene terephthalate for molding and production the same
AssigneePet Rebirth Co., Ltd.
InventorsShuji Inada, Kikuchi Sato
Life of this patent
Estimating the term…
Loading patent…
AssigneePet Rebirth Co., Ltd.
InventorsShuji Inada, Kikuchi Sato
Estimating the term…
There is provided a method for producing a polyethylene terephthalate for molding which has a low content of cyclic trimer. The present invention is a method for producing a polyethylene terephthalate for molding which comprises (1) a condensation step of condensing bis(2-hydroxyethyl)terephthalate having an ion content of 10 ppm or less and an acid value of 30 mgKOH/g or less to produce an oligomer having an average polymerization degree of 4 to 10, (2) a melt-polymerization step of melt-polymerizing the oligomer to produce a prepolymer having an intrinsic viscosity of 0.50 to 0.65, and (3) a solid-state polymerization step of crystallizing pellets of the prepolymer and then solid-state polymerizing the prepolymer at a temperature of 190 to 230° C. to produce a polyethylene terephthalate having an intrinsic viscosity of not lower than 0.65; and a polyethylene terephthalate for molding which is obtained by the method and has specific properties.
A method for producing a polyethylene terephthalate for molding, comprising:
A polyethylene terephthalate for molding, having:
Dependencies are inferred from the claim text.