# US 2006/0113354 A1 · Method and installation for dip coating of a metal strip, in particular of a steel strip

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0113354 A1
- Document ID: US20060113354A1
- Status: Published application
- Kind: A1
- Application number: 11/275,935
- Filed: 2006-02-06
- Published: 2006-06-01
- Earliest claimed: 2000-11-10
- Assignees: Usinor
- Inventors: Didier DAUCHELLE; Hugues Baudin; Patrice Lucas; Laurent Gacher; Yves Prigent
- Web page: https://patentgrep.com/patent/US20060113354A1

## CPC

- C23C 2/00: Hot-dipping or immersion processes for applying the coating material in the molten state without affecting the shape; Apparatus therefor
- C23C 2/325: {Processes or devices for cleaning the bath}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A process for the continuous dip-coating of a metal strip (1) in a tank (11) containing a liquid metal bath (12), in which process the metal strip (1) is made to run continuously through a duct (13), the lower part of which is immersed in the liquid metal bath (12), in order to define with the surface of the bath a liquid seal (14). In the region where the strip (1) leaves the liquid metal bath (12), the liquid metal is isolated from the surface of the bath in an isolating enclosure (20), the metal oxide particles and intermetallic compound particles are recovered by the liquid metal flowing from this region into the enclosure (20), and the particles are extracted from this enclosure (20). Also, a plant for implementing the process.

## Claims

### Claim 1

A process for the continuous dip-coating of a metal strip (1) in a tank (11) containing a liquid metal bath (12), in which process
the metal strip (1) is made to run continuously, in a protective atmosphere, through a duct (13), the lower part (13a) of which is immersed in the liquid metal bath (12) in order to define with the surface of the bath, and inside the duct (13), a liquid seal (14),
the metal strip (1) is deflected around a deflector roller (15) placed in the metal bath (12), and
the coated metal strip (1) is wiped on leaving the metal bath (12),
characterised in that,
in a region (17) where the strip (1) leaves the liquid metal bath (12), the liquid metal is isolated from the surface of the bath in an isolating enclosure (20) having an internal wall with an upper edge,
the metal strip is positioned with respect to the upper edge of the internal wall of the enclosure,
metal oxide particles and intermetallic compound particles are recovered by the liquid metal flowing from this region (17) into the enclosure (20), the drop in height of the liquid metal (12) in this enclosure being maintained higher than 50 mm in order to prevent the metal oxide particles and intermetallic compound particles from rising as a countercurrent to the flow of liquid metal, and
the particles are extracted from this enclosure (20).

### Claim 2 (depends on 1)

The process according to claim 1, characterised in that the drop in height of the liquid metal in the enclosure (20) is greater than 100 mm.

### Claim 3 (depends on 1)

The process according to claim 1, characterised in that the internal wall (23) of the enclosure (20) has a lower part flared out towards the bottom of the tank (11) and an upper part parallel to the metal strip (1).

### Claim 4 (depends on 1)

The process according to claim 1, characterised in that the upper edge (23a) of the internal wall (23) of the enclosure (20) is straight.

### Claim 5 (depends on 1)

The process according to claim 1, characterised in that the upper edge (23a) of the internal wall (23) of the enclosure (20) comprises, in the longitudinal direction, a succession of hollows (26) and projections (27).

### Claim 6 (depends on 5)

The process according to claim 5, characterised in that the hollows (26) and the projections (27) are in the form of circular arcs.

### Claim 7 (depends on 5)

The process according to claim 5, characterised in that the distance between the hollows (26) and the projections (27) is of the order of 150 mm.

### Claim 8 (depends on 5)

The process according to claim 5, characterised in that the difference in height between the hollows (26) and the projections (27) is between 5 and 10 mm.

### Claim 9 (depends on 8)

The process according to claim 8, characterised in that the distance between the hollows (26) and the projections (27) is of the order of 150 mm.

### Claim 10 (depends on 1)

The process according to claim 1, characterised in that the upper edge (23a) of the internal wall (23) of the enclosure (20) is tapered.