# US 2006/0081530 A1 · Highly microporous polymers and methods for producing and using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0081530 A1
- Document ID: US20060081530A1
- Status: Published application
- Kind: A1
- Application number: 11/040,277
- Filed: 2005-01-20
- Published: 2006-04-20
- Earliest claimed: 2004-01-20
- Assignees: Boundless Corp.
- Inventors: Kirby Beard
- Web page: https://patentgrep.com/patent/US20060081530A1

## CPC

- B01D 67/00091: {by evaporation}
- B01D 39/1692: {Other shaped material, e.g. perforated or porous sheets}
- B01D 69/02: characterised by their properties
- B01D 71/301: {Polyvinylchloride}
- B01D 71/34: Polyvinylidene fluoride
- C08J 5/18: Manufacture of films or sheets
- H01M 50/426: Fluorocarbon polymers
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- H01M 50/491: Porosity
- H01M 50/494: Tensile strength
- H01M 50/497: Ionic conductivity
- B01D 2323/082: Cooling
- B01D 2325/20: Specific permeability or cut-off range
- B01D 2325/26: Electrical properties
- C08J 2327/16: Homopolymers or copolymers of vinylidene fluoride
- Y02E 60/10: Energy storage using batteries
- Y10T 428/249921: Web or sheet containing structurally defined element or component
- Y10T 428/249979: Specified thickness of void-containing component [absolute or relative] or numerical cell dimension
- Y10T 442/2033: Coating or impregnation formed in situ [e.g., by interfacial condensation, coagulation, precipitation, etc.]
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention provides microporous polymers and methods for producing and using the same. In particular, microporous polymers of the present invention are highly porous as indicated by a Gurley air permeability flow rate of about 4 seconds or less per mL of air flow per 25 micron of microporous polymer thickness per square inch.

## Claims

### Claim 1

A microporous polymer comprising:
(a) a first surface;
(b) a bulk matrix;
(c) a second surface; and
(d) a plurality of micropores extending from said first surface through said bulk matrix and to said second surface thereby providing a fluid communication between said first and second surfaces,
wherein said microporous polymer has a Gurley air permeability flow rate of about 4 seconds or less per mL of air flow per 25 microns of microporous polymer thickness per square inch of surface area.

### Claim 2 (depends on 1)

The microporous polymer of claim 1, wherein the composition of said polymer comprises carbon and a group selected from hydrogen, halogen, oxygen, nitrogen, sulfur and a combination thereof.

### Claim 3 (depends on 2)

The microporous polymer of claim 2, wherein the composition of said polymer comprises halogen.

### Claim 4 (depends on 3)

The microporous polymer of claim 3, wherein the halogen is selected from the group consisting of chloride, fluoride, and a mixture thereof.

### Claim 5 (depends on 2)

The microporous polymer of claim 2, wherein said polymer is a semicrystalline polymer.

### Claim 6 (depends on 2)

The microporous polymer of claim 2, wherein said polymer is selected from the group consisting of:
polyvinylidene fluoride, polyethylene, polyvinyl chloride, polyacrylonitrile, polymethyl methacrylate, polyvinylidene fluoride-hexafluoropropylene copolymer, ethylene-acrylic acid copolymer, ethylene-styrene copolymer, styrene-butadiene copolymer, styrene-isoprene copolymer, polydiene, polyalkane, polyacrylic, polyvinyl ether, polyvinyl alcohol, polyacetal, polyvinyl ketone, polyvinyl halide, polyvinyl nitril, polyvinyl ester, polystyrene, polyphenylene, polyoxide, polycarbonate, polyester, polyanhydride, polyurethane, polysulfonate, polysulfide, polysulfone, polyamide, and a mixture of two or more thereof.

### Claim 7 (depends on 1)

The microporous polymer of claim 1, wherein said polymer comprises polyvinylidene fluoride, polyvinyl chloride, polylvinylidene fluoride-hexafluoropropylene copolymer or a mixture thereof.

### Claim 8 (depends on 7)

The microporous polymer of claim 7, wherein said polymer comprises at least about 80% polyvinylidene fluoride.

### Claim 9 (depends on 1)

The microporous polymer of claim 1, wherein the thickness of said polymer is about 5 mm or less.

### Claim 10 (depends on 9)

The microporous polymer of claim 9, wherein said polymer is a thin film.

### Claim 11 (depends on 10)

The microporous polymer of claim 10, wherein the thickness of said thin film is about 100 μm or less.

### Claim 12 (depends on 10)

The microporous polymer of claim 10, wherein the tensile strength of said thin film is at least about 100 psi.

### Claim 13 (depends on 1)

The microporous polymer of claim 1, wherein the average pore size is about 10 μm or less.

### Claim 14

A method of producing a microporous polymer comprising:
forming a layer of a polymer solution on a substrate, wherein the polymer solution comprises a liquid and a polymer material that is dissolved in the liquid, and wherein the liquid comprises a high surface tension liquid;
producing a film of gelled polymer from the layer of polymer solution under conditions sufficient to provide a non-wetting, high surface tension solution within the layer of polymer solution; and
removing the liquid from the film of gelled polymer under conditions sufficient to produce the microporous polymer.

### Claim 15 (depends on 14)

The method of claim 14, wherein at least the first 50% of the liquid in the gelled polymer is removed at a temperature near or below the temperature of said gelled polymer forming step.

### Claim 16 (depends on 14)

The method of claim 14, wherein the solubility of the polymer material in the solution is about 25% v/v or less relative to the total volume of the liquid in the solution.

### Claim 17 (depends on 14)

The method of claim 14, wherein the liquid further comprises a low surface tension liquid, wherein said polymer material has a higher solubility in the low surface tension liquid than in the high surface tension liquid.

### Claim 18 (depends on 17)

The method of claim 17, wherein the low surface tension liquid has a higher vapor pressure than the higher surface tension liquid, thereby allowing the low surface tension liquid to evaporate at a faster rate than the high surface tension liquid from the polymer solution.

### Claim 19 (depends on 17)

The method of claim 17, wherein the ratio of the low surface tension liquid relative to the high surface tension liquid is about 99:1 v/v or less.

### Claim 20 (depends on 17)

The method of claim 17, wherein the void volume of the microporous polymer is substantially similar or higher to the relative volumetric ratio between the high surface tension liquid and the combined volume total of the polymer material and the high surface tension liquid.

### Claim 21 (depends on 17)

The method of claim 17, wherein the low surface tension liquid is a ketone, ester, ether, aldehyde, amine, amide, nitrile, cyanate, nitrite, nitrate, nitro- or nitroso- compound, thiol, sulfide, sulfonium, sulfate, sulfonyl compound, sulfinyl compound, thio compounds, or a mixture of two or more thereof

### Claim 22 (depends on 21)

The method of claim 21, wherein the ketone is selected from the group consisting of acetone, methyl ethyl ketone, pentanone, hexanone, cyclic ketone, or a mixture of two or more thereof.

### Claim 23 (depends on 14)

The method of claim 14, wherein the high surface tension liquid is selected from the group consisting of:
acetamide, acetophenone, adiponitrile, aniline, benzaldehyde, benzyl benzoate, benzonitrile, benzophenone, bromine, bromobenzene, tribromomethane, bromophenol, carbon disulfide, chloroacetic acid, chlorobenzene, chlorophenol, diethylaniline, diethylene glycol, dimethylaniline, dimethyl phenyl pyrazolane, dimethyl sulfoxide, diphenylamine, ethylaniline, ethylene bromide, ethylene glycol, formamide, formic acid, furfural, γ-butyrolactone, glycerin, glycerol, methylaniline, methyl benzoate, methylene iodide, nitric acid, nitrobenzene, nitromethane, phenol, phosphorous tribromide, phosphorous tri-iodide, propylene glycol, pyridine, pyridazine, quinoline, sulfuric acid, tetrabromomethane, toluene, xylene, water, and a mixture of two or more thereof.

### Claim 24 (depends on 23)

The method of claim 23, wherein the high surface tension liquid is water.

### Claim 25 (depends on 14)

The method of claim 14, wherein the thickness of the polymer solution layer on the substrate is about 500 μm or less.

### Claim 26 (depends on 14)

The method of claim 14, wherein the substrate is a high surface free energy substrate.

### Claim 27 (depends on 26)

The method of claim 26, wherein the surface free energy of the substrate is at least about 40 dynes/cm at 25° C.

### Claim 28 (depends on 14)

The method of claim 14, wherein the film of gelled polymer is formed at a temperature of about 40° C. or less.

### Claim 29 (depends on 28)

The method of claim 28, wherein the liquid is removed from the gelled polymer at a temperature of about 30° C. or less.

### Claim 30 (depends on 14)

The method of claim 14, wherein the film of gelled polymer is formed at a temperature of about 5° C. or less relative to the dissolution and wetting temperature of the polymer.

### Claim 31 (depends on 14)

The method of claim 14, wherein the liquid is removed at a temperature of about 5° C. or less relative to the dissolution and wetting temperature of the polymer material.

### Claim 32 (depends on 14)

The method of claim 14, wherein the solubility of the polymer material in the liquid is about 10% v/v or less.

### Claim 33 (depends on 14)

The method of claim 14 further comprising admixing the liquid and the polymer material to form the polymer solution, wherein the polymer solution is formed by heating the mixture, subjecting the mixture to high shear mixing, or a combination thereof.

### Claim 34 (depends on 14)

The method of claim 14, wherein the amount of polymer material dissolved in the polymer solution is at least near its saturation limit.