# US 2006/0079387 A1 · High homogeneity silica glass prepared through a sol-gel procedure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0079387 A1
- Document ID: US20060079387A1
- Status: Published application
- Kind: A1
- Application number: 10/549,680
- Filed: 2004-03-12
- Published: 2006-04-13
- Earliest claimed: 2003-03-21
- Inventors: Fulvio Costa; Lorenzo Costa; Massimo Sparpaglione
- Web page: https://patentgrep.com/patent/US20060079387A1

## CPC

- C03B 19/12: by liquid-phase reaction processes
- C03C 1/006: {to produce glass through wet route}
- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- C03C 2201/02: Pure silica glass, e.g. pure fused quartz
- C03C 2203/26: using alkoxides
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

The present invention relates to a Si2O glass characterized by a high homogeneity, prepared through a sol-gel procedure.

## Claims

### Claim 1

(canceled)

### Claim 2

A silica glass characterized by the following specific properties:
a) light internal transmittance in the wave length between 185 nm and 193 nm higher than 85%;
b) light internal transmittance in the wave length between 193 nm and 2600 nm higher than 99.5%;
c) light internal transmittance in the wave length between 2600 nm and 2730 nm higher than 99%;
d) light internal transmittance in the wave length between 2730 nm and 3200 nm higher than 85%;
e) no streak, material of class 4 or better according to the rule DIN ISO 10110-4;
f) no strip;
g) no signal in the shadography (no shadow or intensity change);
and wherein said silica glass is made by a sol gel process.

### Claim 3 (depends on 2)

The silica glass of claim 2, wherein said sol gel process includes a step in which said sol gel is thermally treated at a temperature of 800° C.-1500° C. to increase its density.

### Claim 4 (depends on 3)

The silica gel of claim 3, wherein thermal treatment is carried out in a controlled atmosphere containing traces of water.

### Claim 5 (depends on 4)

The silica gel of claim 4, wherein said sol gel process further comprises the steps of:
a) preparing a sol from a silicon alcoxide;
b) allowing or inducing the hydrolysis of the sol prepared in step a);
c) drying the gel obtained in step b).