# US 2006/0079094 A1 · Method for microstructuring flat glass substrates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0079094 A1
- Document ID: US20060079094A1
- Status: Published application
- Kind: A1
- Application number: 11/243,443
- Filed: 2005-10-04
- Published: 2006-04-13
- Earliest claimed: 2004-10-10
- Assignees: Schott AG
- Inventors: Bianca Schreder; Rainer Liebald; Edgar Pawlowski; Dirk Sprenger; Dietrich Mund; Juergen Leib
- Web page: https://patentgrep.com/patent/US20060079094A1

## CPC

- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

In the method for microstructuring flat glass substrates a substrate surface of a glass substrate is coated with at least one structured mask layer and subsequently exposed to a chemically reactive ion etching process (RIE) with at least one chemical etching gas. In order to provide the same or a higher quality etching and etching rate even for economical types of glass the chemical etching gas is mixed with at least one noble gas, so that the proportion of sputtering etching in the ion etching process is significantly increased.

## Claims

### Claim 1

A method for microstructuring flat glass substrates, said method comprising the steps of:
a) coating a substrate surface of a flat glass substrate with at least one structured mask layer;
b) mixing a chemical etching gas with at least one noble gas in a mixture ratio of the chemical etching gas to the at least one noble gas of from 2:1 to 6:1 in order to form an etching gas mixture; and
c) performing a chemically reactive ion etching process in which the substrate surface coated with the at least one structured mask layer is exposed to the etching gas mixture;
wherein the proportion of sputtering etching occurring in the ion etching process is significantly increased by the presence of the at least one noble gas in the etching gas mixture but a major portion of the etching gas mixture consists of the chemical etching gas.

### Claim 2 (depends on 1)

The method as defined in claim 1, wherein the chemical etching gas used as reaction gas contains CF4 or CHF3 as principal component.

### Claim 3 (depends on 1)

The method as defined in claim 1, wherein the at least one noble gas used as sputtering gas comprises argon.

### Claim 4 (depends on 1)

The method as defined in claim 1, wherein the mixture ratio is from 2:1 to 4:1.

### Claim 5 (depends on 1)

The method as defined in claim 1, wherein the mixture ratio is about 3:1.

### Claim 6 (depends on 1)

The method as defined in claim 1, wherein said flat glass is a multi-component glass containing at least three ingredients.

### Claim 7 (depends on 6)

The method as defined in claim 6, wherein the multi-component glass comprises boron oxide, aluminum oxide and at least one alkali oxide.

### Claim 8 (depends on 1)

The method as defined in claim 1, wherein said flat glass contains SiO2 and B2O3 and a sum total of said SiO2 and B2O3 present in the flat glass is from 60 to 95 percent by weight.

### Claim 9 (depends on 1)

The method as defined in claim 1, wherein said flat glass contains Al2O3, B2O3 and/or TiO2 and a sum total of said Al2O3, B2O3 and/or TiO2 present in the flat glass is from 5 to 40 percent by weight.

### Claim 10 (depends on 1)

The method as defined in claim 1, wherein the chemically reactive ion etching process is performed with a process gas pressure of 30 mtorr to 60 mtorr.

### Claim 11 (depends on 1)

The method as defined in claim 1, wherein said substrate surface is coated with a metal layer and the metal layer is subjected to a structuring process.

### Claim 12 (depends on 11)

The method as defined in claim 11, wherein said metal layer is a chromium layer.

### Claim 13 (depends on 11)

The method as defined in claim 11, wherein said metal layer is applied to the substrate surface using a magnetron sputtering process.

### Claim 14 (depends on 11)

The method as defined in claim 11, wherein the metal layer has a thickness such that metal layer is completely etched away in subsequent ion etching processes.

### Claim 15 (depends on 11)

The method as defined in claim 11, wherein the metal layer is structured by a photolithographic process.

### Claim 16 (depends on 11)

The method as defined in claim 11, wherein a resist layer is applied to the metal layer, said resist layer is illuminated and then developed and subsequently illuminated metal regions are etched away.

### Claim 17 (depends on 16)

The method as defined in claim 16, further comprising a soft-bake treatment after etching away the resist layer and/or a hard-bake treatment after developing the resist layer.

### Claim 18 (depends on 11)

The method as defined in claim 11, further comprising removing metal mask layer residue after the ion etching process by wet chemical methods.