# US 2006/0079087 A1 · Method of producing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0079087 A1
- Document ID: US20060079087A1
- Status: Published application
- Kind: A1
- Application number: 11/041,217
- Filed: 2005-01-25
- Published: 2006-04-13
- Earliest claimed: 2004-10-13
- Assignees: Fujitsu Limited
- Inventors: Kazuo Kawamura; Satoshi Inagaki; Takashi Saiki; Ryou Nakamura
- Web page: https://patentgrep.com/patent/US20060079087A1

## CPC

- H10P 14/69394: {the material containing titanium, e.g. TiO2}
- H10D 30/0212: {using self-aligned silicidation}
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 64/0131: {the additional conductive layer comprising a silicide layer formed by the silicidation reaction between the layer of silicon with a metal layer which is not formed by metal implantation}
- H10D 64/663: {the additional layers comprising a silicide layer contacting the layer of silicon, e.g. polycide gates}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/21: {of electrically active species}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of producing a semiconductor device is disclosed that is able to reduce fluctuations of a sheet resistance of a silicide layer in the semiconductor device formed by a salicide process. When depositing a titanium nitride film on a cobalt film in the salicide process, the thickness of the titanium nitride film is set to be sufficiently small so that a nano-grain structure or an amorphous structure is formed in the titanium nitride film. In the titanium nitride film, the titanium composition is enriched.

## Claims

### Claim 1

A method of producing a semiconductor device having a gate width less than 50 nm, comprising:
a step of forming a poly-silicon gate electrode pattern having a gate width less than 50 nm on a semiconductor substrate;
a step of forming a first diffusion region and a second diffusion region on two respective sides of the poly-silicon gate electrode pattern in the semiconductor substrate;
a step of depositing a cobalt film on the semiconductor substrate so as to cover the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern;
a step of depositing a titanium nitride film on the cobalt film; and
a step of, after the step of depositing the titanium nitride film, inducing a reaction between the cobalt film and surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern so as to form a CoSi2 film;
wherein the titanium nitride film is formed such that a crystal grain diameter of the titanium nitride film is less than a thickness of the titanium nitride film.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the grain diameter is less than or equal to 10 nm.

### Claim 3

A method of producing a semiconductor device having a gate width less than 50 nm, comprising:
a step of forming a poly-silicon gate electrode pattern having a gate width less than 50 nm on a semiconductor substrate;
a step of forming a first diffusion region and a second diffusion region on two respective sides of the poly-silicon gate electrode pattern in the semiconductor substrate;
a step of depositing a cobalt film on the semiconductor substrate so as to cover the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern;
a step of depositing a titanium nitride film on the cobalt film; and
a step of, after the step of depositing the titanium nitride film, inducing a reaction between the cobalt film and surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern so as to form a CoSi2 film;
wherein the titanium nitride film is formed to have an amorphous phase.

### Claim 4

A method of producing a semiconductor device having a gate width less than 50 nm, comprising:
a step of forming a poly-silicon gate electrode pattern having a gate width less than 50 nm on a semiconductor substrate;
a step of forming a first diffusion region and a second diffusion region on two respective sides of the poly-silicon gate electrode pattern in the semiconductor substrate;
a step of depositing a cobalt film on the semiconductor substrate so as to cover the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern;
a step of depositing a titanium nitride film on the cobalt film, a composition of said titanium nitride film being denoted as TixNy (x+y=1); and
a step of, after the step of depositing the titanium nitride film, inducing a reaction between the cobalt film and surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern so as to form a CoSi2 film;
wherein the composition of the titanium nitride film satisfies x>y.

### Claim 5 (depends on 4)

The method as claimed in claim 4, wherein the composition of the titanium nitride film satisfies 1.0<x/y<5.0.

### Claim 6 (depends on 4)

The method as claimed in claim 4, wherein composition parameters x and y of the titanium nitride film are set so that an atomic percentage of titanium in the CoSi2 film is not less than 0.1%, and not greater than 1%.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the thickness of the titanium nitride film is less than or equal to 20 nm.

### Claim 8 (depends on 3)

The method as claimed in claim 3, wherein a thickness of the titanium nitride film is less than or equal to 20 nm.

### Claim 9 (depends on 4)

The method as claimed in claim 4, wherein a thickness of the titanium nitride film is less than or equal to 20 nm.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the titanium nitride film is in contact with the cobalt film.

### Claim 11 (depends on 3)

The method as claimed in claim 3, wherein the titanium nitride film is in contact with the cobalt film.

### Claim 12 (depends on 4)

The method as claimed in claim 4, wherein the titanium nitride film is in contact with the cobalt film.

### Claim 13 (depends on 1)

The method as claimed in claim 1, wherein the step of forming the CoSi2 film comprises:
a step of inducing a reaction between the cobalt film and the surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern at a first temperature, so as to form a CoSi film;
a step of removing residues of the cobalt film and the titanium nitride film; and
a step of inducing a reaction between the CoSi film and the surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern at a second temperature higher than the first temperature, so as to convert the CoSi film to the CoSi2 film.

### Claim 14 (depends on 3)

The method as claimed in claim 3, wherein the step of forming the CoSi2 film comprises:
a step of inducing a reaction between the cobalt film and the surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern at a first temperature, so as to form a CoSi film;
a step of removing residues of the cobalt film and the titanium nitride film; and
a step of inducing a reaction between the CoSi film and the surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern at a second temperature higher than the first temperature, so as to convert the CoSi film to the CoSi2 film.

### Claim 15 (depends on 4)

The method as claimed in claim 4, wherein the step of forming the CoSi2 film comprises:
a step of inducing a reaction between the cobalt film and the surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern at a first temperature, so as to form a CoSi film;
a step of removing residues of the cobalt film and the titanium nitride film; and
a step of inducing a reaction between the CoSi film and the surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern at a second temperature higher than the first temperature, so as to convert the CoSi film to the CoSi2 film.

### Claim 16

A semiconductor device, comprising:
a semiconductor substrate;
a poly-silicon gate electrode pattern having a gate width less than 50 nm formed on the semiconductor substrate with a gate insulating film in between; and
a first diffusion region and a second diffusion region in the semiconductor substrate on two respective sides of the poly-silicon gate electrode pattern and on respective outer sides of sidewall insulating films of the poly-silicon gate electrode;
wherein
a CoSi2 film is formed on surfaces of the first-diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern, and
an atomic percentage of titanium in the CoSi2 film is in a range from 0.1% to 1%.