# US 2006/0079041 A1 · Manufacturing method for a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0079041 A1
- Document ID: US20060079041A1
- Status: Published application
- Kind: A1
- Application number: 11/285,012
- Filed: 2005-11-23
- Published: 2006-04-13
- Earliest claimed: 2001-11-30
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Shunpei Yamazaki; Akihisa Shimomura; Hisashi Ohtani; Masaaki Hiroki; Koichiro Tanaka; Aiko Shiga; Mai Akiba; Kenji Kasahara
- Web page: https://patentgrep.com/patent/US20060079041A1

## CPC

- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10D 62/40: Crystalline structures
- H10D 86/0229: {characterised by control of the annealing or irradiation parameters}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/2923: {being conductive materials, e.g. metallic silicides}
- H10P 14/3238: {being insulating materials}
- H10P 14/3248: {consisting of two layers}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3456: {Polycrystalline}
- H10P 14/3806: {using crystallisation-enhancing elements}
- H10P 14/3812: {Shape of mask}
- H10P 14/3816: {Pulsed laser beam}
- H10P 14/382: {Scanning of a beam}
- H10W 46/00: Marks applied to devices, e.g. for alignment or identification
- H10W 46/501: {for use before dicing}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Position control of a crystal grain in accordance with an arrangement of a TFT is achieved, and at the same time, a processing speed during a crystallization process is increased. More specifically, there is provided a manufacturing method for a semiconductor device, in which crystal having a large grain size can be continuously formed through super lateral growth that is artificially controlled and substrate processing efficiency during a laser crystallization process can be increased. In the manufacturing method for a semiconductor device, instead of performing laser irradiation on an entire semiconductor film within a substrate surface, a marker as a reference for positioning is formed so as to crystallize at least an indispensable portion at minimum. Thus, a time period required for laser crystallization can be reduced to make it possible to increase a processing speed for a substrate. The above structure is applied to a conventional SLS method, so that it is possible to solve a problem inherent to the conventional SLS method, in that the substrate processing efficiency is poor.

## Claims

### Claim 1

A manufacturing method for a semiconductor device having a thin film transistor comprising:
forming an amorphous semiconductor film on an insulating surface; and
irradiating a laser light to perform crystallization to a region in which active layers of the thin film transistor is formed,
wherein the laser light is a laser light of pulse oscillation having a repetition frequency of several MHz, and
wherein a direction in which the laser light is moved on the amorphous semiconductor film is parallel to a direction in which carriers move in a channel formation region in the thin film transistor.

### Claim 2 (depends on 1)

The manufacturing method for the semiconductor device according to claim 1, wherein the amorphous semiconductor film is melted over entire thickness through irradiation of the laser light.

### Claim 3 (depends on 1)

The manufacturing method for the semiconductor device according to claim 1, wherein the laser light is a second harmonic, a third harmonic, or a fourth harmonic.

### Claim 4 (depends on 1)

The manufacturing method for the semiconductor device according to claim 1, wherein the laser light is converged onto the amorphous semiconductor film through a cylindrical lens.

### Claim 5 (depends on 1)

The manufacturing method for the semiconductor device according to claim 1, wherein each time the laser light oscillates 1 pulse, a spot position of the laser light on a surface of the amorphous semiconductor film is relatively moved by a fixed distance that is 0.3 μm or more and 5 μm or less.

### Claim 6 (depends on 1)

The manufacturing method for the semiconductor device according to claim 1, wherein a relative movement direction of a spot on the amorphous semiconductor film is perpendicular to a longitudinal direction of the spot.

### Claim 7

A manufacturing method for a semiconductor device having a thin film transistor comprising:
forming an amorphous semiconductor film on an insulating surface;
forming a marker on the amorphous semiconductor film; and
selectively irradiating the laser light to perform crystallization to a region in which an active layer of the thin film transistor is formed, based on information on arrangement of the thin film transistor with the marker used as a reference,
wherein the laser light is a laser light of pulse oscillation having a repetition frequency of several MHz, and
wherein a direction in which the laser light is moved on the amorphous semiconductor film is parallel to a direction in which carriers move in a channel formation region in the thin film transistor.

### Claim 8 (depends on 7)

The manufacturing method for the semiconductor device according to claim 7, wherein the amorphous semiconductor film is melted over entire thickness through irradiation of the laser light.

### Claim 9 (depends on 7)

The manufacturing method for the semiconductor device according to claim 7, wherein the laser light is a second harmonic, a third harmonic, or a fourth harmonic.

### Claim 10 (depends on 7)

The manufacturing method for the semiconductor device according to claim 7, wherein the laser light is converged onto the amorphous semiconductor film through a cylindrical lens.

### Claim 11 (depends on 7)

The manufacturing method for the semiconductor device according to claim 7, wherein each time the laser light oscillates 1 pulse, a spot position of the laser light on a surface of the amorphous semiconductor film is relatively moved by a fixed distance that is 0.3 μm or more and 5 μm or less.

### Claim 12 (depends on 7)

The manufacturing method for the semiconductor device according to claim 7, wherein a relative movement direction of a spot on the amorphous semiconductor film is perpendicular to a longitudinal direction of the spot.

### Claim 13

A manufacturing method for a semiconductor device having a thin film transistor comprising:
forming an amorphous semiconductor film on an insulating surface; and
irradiating a laser light to perform crystallization to a region in which active layers of the thin film transistor is formed,
wherein the laser light is a laser light of pulse oscillation having a repetition frequency of several MHz and emitted from a solid laser oscillation apparatus, and
wherein a direction in which the laser light is moved on the amorphous semiconductor film is parallel to a direction in which carriers move in a channel formation region in the thin film transistor.

### Claim 14 (depends on 13)

The manufacturing method for the semiconductor device according to claim 13, wherein the amorphous semiconductor film is melted over entire thickness through irradiation of the laser light.

### Claim 15 (depends on 13)

The manufacturing method for the semiconductor device according to claim 13, wherein the laser light is a second harmonic, a third harmonic, or a fourth harmonic.

### Claim 16 (depends on 13)

The manufacturing method for the semiconductor device according to claim 13, wherein the laser light is converged onto the amorphous semiconductor film through a cylindrical lens.

### Claim 17 (depends on 13)

The manufacturing method for the semiconductor device according to claim 13, wherein each time the laser light oscillates 1 pulse, a spot position of the laser light on a surface of the amorphous semiconductor film is relatively moved by a fixed distance that is 0.3 μm or more and 5 μm or less.

### Claim 18 (depends on 13)

The manufacturing method for the semiconductor device according to claim 13, wherein a relative movement direction of a spot on the amorphous semiconductor film is perpendicular to a longitudinal direction of the spot.

### Claim 19 (depends on 13)

The manufacturing method for the semiconductor device according to claim 13, wherein the solid laser oscillation apparatus uses semiconductor laser excitation.