# US 2006/0078790 A1 · Solid electrolytes based on lithium hafnium phosphate for active metal anode protection

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0078790 A1
- Document ID: US20060078790A1
- Status: Published application
- Kind: A1
- Application number: 11/245,472
- Filed: 2005-10-05
- Published: 2006-04-13
- Earliest claimed: 2004-10-05
- Assignees: PolyPlus Battery Company
- Inventors: Yevgeniy Nimon; Lutgard De Jonghe; Steven Visco
- Web page: https://patentgrep.com/patent/US20060078790A1

## CPC

- H01M 4/664: {Ceramic materials}
- H01M 4/366: {as layered products}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 50/434: Ceramics
- H01M 50/437: Glass
- H01M 50/497: Ionic conductivity
- H01M 2300/0071: Oxides
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Active metal electrochemical structure, in particular an active metal negative electrode (anode) protected with an ionically conductive protective architecture incorporating a glassy, ceramic or glass-ceramic solid electrolyte material based on lithium hafnium phosphate, and associated electrochemical devices and methods, provides advantages over conventional structures. The protective architecture prevents the active metal from deleterious reaction with the environment on the other (cathode) side of the architecture, which may include aqueous, air or organic liquid electrolytes and/or electrochemically active materials.

## Claims

### Claim 1

An electrochemical device structure, comprising:
an active metal anode having a first surface and a second surface; and
a protective architecture on the first surface of the anode, the architecture having a first component ionically conductive and chemically compatible with the active metal on a side in contact with the active metal anode, and second component substantially impervious, ionically conductive and chemically compatible with active metal corrosive environments on the other side;
wherein the architecture comprises a glassy, ceramic or glass-ceramic solid electrolyte material based on lithium hafnium phosphate.

### Claim 2 (depends on 1)

The structure of claim 1, wherein the protective architecture comprises a composite, the composite comprising,
a first material in contact with the anode, the first material being ionically conductive and chemically compatible with the active metal; and
a second material in contact with the first material, the second material comprising the glassy, ceramic or glass-ceramic solid electrolyte material based on lithium hafnium phosphate and being substantially impervious, ionically conductive and chemically compatible with the first material and active metal corrosive environments;
wherein the ionic conductivity of the composite is at least 10−7 S/cm.

### Claim 3 (depends on 1)

The structure of claim 1, wherein an active metal anode comprises a material selected from the group consisting of active metal, active metal-ion, active metal alloying metal, and active metal intercalating material.

### Claim 4 (depends on 2)

The structure of claim 2, wherein the first material comprises a material selected from the group consisting of active metal nitrides, active metal phosphides, and active metal halides, and active metal phosphorus oxynitride glass.

### Claim 5 (depends on 4)

The structure of claim 4, wherein the first material comprises a material selected from the group consisting of Li3N, Li3P and LiI, LiBr, LiCl, LiF, and LiPON.

### Claim 6 (depends on 2)

The structure of claim 2, wherein the protective composite is a laminate of discrete layers of the first material and the second material.

### Claim 7 (depends on 2)

The structure of claim 2, wherein the protective composite comprises a gradual transition between the first material and the second material.

### Claim 8 (depends on 1)

The structure of claim 1, wherein the active metal electrode is lithium or a lithium alloy.

### Claim 9 (depends on 1)

The structure of claim 1, wherein the protective architecture comprises:
an ionically conductive protective architecture on a first surface of the anode the architecture comprising,
an active metal ion conducting separator layer comprising a non-aqueous anolyte, the separator layer being chemically compatible with the active metal, and in contact with the anode, and
a substantially impervious ionically conductive layer, comprising a glassy, ceramic or glass-ceramic solid electrolyte material based on lithium hafnium phosphate, chemically compatible with the separator layer and with aqueous environments, and in contact with the separator layer.

### Claim 10 (depends on 9)

The structure of claim 9, wherein the separator layer comprises a semi-permeable membrane impregnated with a non-aqueous.

### Claim 11 (depends on 10)

The structure of claim 10, wherein the semi-permeable membrane is a micro-porous polymer.

### Claim 12 (depends on 11)

The structure of claim 11, wherein the anolyte is in the liquid phase.

### Claim 13 (depends on 12)

The structure of claim 12, wherein the anolyte comprises a solvent selected from the group consisting of organic carbonates, ethers, esters, formates, lactones, sulfones, sulfolane and combinations thereof.

### Claim 14 (depends on 13)

The structure of claim 13, wherein the anolyte comprises a solvent selected from the group consisting of EC, PC, DEC, DMC, EMC, THF, 2MeTHF, 1,2-DME or higher glymes, sufolane, methyl formate, methyl acetate, and combinations thereof and a supporting salt selected from the group consisting of LiPF6, LiBF4, LiAsF6, LiClO4, LiSO3CF3, LiN(CF3SO2)2 and LiN(SO2C2F5)2.

### Claim 15 (depends on 14)

The structure of claim 14, wherein the anolyte further comprises 1,3-dioxolane.

### Claim 16 (depends on 11)

The structure of claim 11, wherein the anolyte is in the gel phase.

### Claim 17 (depends on 16)

The structure of claim 16, wherein the anolyte comprises a gelling agent selected from the group consisting of PVDF, PVdF-HFP copolymer, PAN, and PEO and mixtures thereof; a plasticizer selected from the group consisting of EC, PC, DEC, DMC, EMC, THF, 2MeTHF, 1,2-DME and mixtures thereof; and a Li salt selected from the group consiting of LiPF6, LiBF4, LiAsF6, LiClO4, LiSO3CF3, LiN(CF3SO2)2 and LiN(SO2C2F5)2.

### Claim 18 (depends on 1)

The structure of claim 1, wherein the substantially impervious ionically conductive component comprises a thin film of the glassy, ceramic or glass-ceramic solid electrolyte material based on lithium hafnium phosphate on another ionically conductive ceramic or glass-ceramic.

### Claim 19 (depends on 18)

The structure of claim 18, wherein the other ionically conductive ceramic or glass-ceramic is based on lithium germanium phosphate.

### Claim 20 (depends on 1)

The structure of claim 1, wherein the glassy, ceramic or glass-ceramic solid electrolyte material based on lithium hafnium phosphate further comprises lithium oxide or other inorganic Li compounds, in particular, Li3PO4 and Li3BO3.

### Claim 21 (depends on 1)

The structure of claim 1, wherein the glassy, ceramic or glass-ceramic solid electrolyte material based on lithium hafnium phosphate is a LiHf2(PO4)3+yLi2O glass ceramic.

### Claim 22 (depends on 1)

The structure of claim 1, wherein the glassy, ceramic or glass-ceramic solid electrolyte material based on lithium hafnium phosphate has a general formula of Li1+xMxHf2−x(PO4)3, wherein M is Cr, In, Fe, Ta, Sc, Lu or Y, wherein 0<X≦0.5.

### Claim 23

A battery cell, comprising:
an active metal anode having a first surface and a second surface;
a cathode structure; and
a protective architecture on the first surface of the anode, the architecture being ionically conductive and chemically compatible with the active metal on a side in contact with the active metal anode, and substantially impervious, ionically conductive and chemically compatible with active metal corrosive environments on the other side;
wherein the architecture comprises a glassy, ceramic or glass-ceramic solid electrolyte material based on lithium hafnium phosphate.

### Claim 24 (depends on 23)

The cell of claim 23, wherein the protective architecture comprises:
an active metal ion conducting separator layer comprising a non-aqueous anolyte, the separator layer being chemically compatible with the active metal, and in contact with the anode, and
a substantially impervious ionically conductive layer, comprising a glassy, ceramic or glass-ceramic solid electrolyte material based on lithium hafnium phosphate, chemically compatible with the separator layer and the cathode structure, and in contact with the cathode structure.

### Claim 25 (depends on 23)

The cell of claim 23, wherein the protective architecture comprises:
a composite, the composite comprising,
a first material in contact with the anode, the first material being ionically conductive and chemically compatible with the active metal; and
a second material in contact with the first material, the second material comprising the glassy, ceramic or glass-ceramic solid electrolyte material based on lithium hafnium phosphate and being substantially impervious, ionically conductive and chemically compatible with the first material and active metal corrosive environments;
wherein the ionic conductivity of the composite is at least 10−7 S/cm.