# US 2006/0078755 A1 · Weldable high strength Al-Mg-Si alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0078755 A1
- Document ID: US20060078755A1
- Status: Published application
- Kind: A1
- Application number: 11/147,375
- Filed: 2005-06-08
- Published: 2006-04-13
- Earliest claimed: 2001-07-23
- Assignees: Corus Aluminium Walzprodukte GmbH
- Inventors: Rinze Benedictus; Guido Weber; Alfred Haszler; Christian Keidel
- Web page: https://patentgrep.com/patent/US20060078755A1

## CPC

- C22C 21/02: with silicon as the next major constituent
- C22F 1/043: of alloys with silicon as the next major constituent
- Y10T 428/12764: Next to Al-base component
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to a weldable, high-strength aluminium alloy wrought product, which may be in the form of a rolled, extruded or forged form, containing the elements, in weight percent, Si 0.8 to 1.3, Cu 0.2 to 1.0, Mn 0.5 to 1.1, Mg 0.45 to 1.0, Ce 0.01 to 0.25, and preferably added in the form of a Misch Metal, Fe 0.01 to 0.3, Zr<0.25, Cr<0.25, Zn<1.4, Ti<0.25, V<0.25, others each<0.05 and total<0.15, balance aluminium. The invention relates also to a method of manufacturing such an aluminium alloy product.

## Claims

### Claim 1

Weldable, high-strength aluminium alloy wrought product, containing the elements, in weight percent:
Si 0.8-1.3
Cu 0.2-0.5
Mn 0.5-1.1
Mg 0.45-1.0
Ce 0.01-0.25,
Fe 0.01-0.3
Zr<0.25
Cr<0.25
Zn<1.4
Ti<0.25
V<0.25
others each<0.05, total<0.15
balance aluminium

### Claim 2 (depends on 1)

Product in accordance with claim 1, wherein the Si level is in the range of 1.0 to 1.15%.

### Claim 3 (depends on 1)

Product in accordance with claim 1, wherein the Cu level is in the range of 0.25 to 0.5%.

### Claim 4

(canceled)

### Claim 5 (depends on 1)

Product in accordance with claim 1, wherein the Mn level is in the range of 0.6 to 0.8%.

### Claim 6 (depends on 1)

Product in accordance with claim 1, wherein the Mg level is in the range of 0.6 to 0.85%.

### Claim 7 (depends on 1)

Product in accordance with claim 1, wherein the Ti level is in the range of 0.06 to 0.2%.

### Claim 8 (depends on 1)

Product in accordance with claim 1, wherein the Zn level is in a range of less than 0.4%.

### Claim 9 (depends on 1)

Product in accordance with claim 1, wherein the Fe level is in the range of 0.01 to 0.25%.

### Claim 10 (depends on 1)

Product in accordance with claim 1, wherein the Ce level is in the range of 0.01 to 0.15%.

### Claim 11 (depends on 1)

Product in accordance with claim 1, wherein the product has a more than 80% recrystallised microstructure.

### Claim 12 (depends on 1)

Product in accordance with claim 1, wherein the alloy having been aged to the T6 temper in an ageing cycle which comprises exposure to a temperature of between 150 and 210° C. for a period between 0.5 and 30 hours, to thereby produce an aluminium alloy product characterised by an intergranular corrosion after an MIL-H-6088 test which is present to a depth less than 200 μm.

### Claim 13 (depends on 1)

Product in accordance with claim 1, wherein the product has a single or multiple cladding thereon selected from the group consisting of:
(i) the cladding is of a higher purity aluminium alloy than said product;
(ii) the cladding is of the Aluminium Association AA1000-series;
(iii) the cladding is of the Aluminium Association AA4000-series;
(iv) the cladding is of the Aluminium Association AA6000-series; and
(v) the cladding is of the Aluminium Association AA7000-series.

### Claim 14 (depends on 13)

Product in accordance with claim 13, wherein the alloy product has a cladding thereon on one side of the Aluminium Association AA1000-series and on the other side thereon of the Aluminium Association AA4000-series.

### Claim 15 (depends on 1)

Product in accordance with claim 1, wherein the Ce is added as a MM.

### Claim 16 (depends on 1)

Product in accordance with claim 1, wherein the Mn level is in the range of 0.65 to 0.78%.

### Claim 17 (depends on 1)

Product in accordance with claim 1, wherein the Mg level is in the range of 0.6 to 0.75%.

### Claim 18 (depends on 1)

Product in accordance with claim 1, wherein the Ti level is in the range of 0.07 to 0.2%.

### Claim 19 (depends on 1)

Product in accordance with claim 1, wherein the Fe level is in the range of 0.01 to 0.2%.

### Claim 20 (depends on 1)

Product in accordance with claim 1, wherein the product is in the form of a rolled product,

### Claim 21 (depends on 1)

Product in accordance with claim 1, wherein the product is a structural component of an aircraft.

### Claim 22 (depends on 1)

Product in accordance with claim 1, wherein the product is aircraft skin material.

### Claim 23 (depends on 1)

A method of producing the weldable, high-strength alloy wrought product according to claim 1, comprises the sequential process steps of:
(a) providing stock having a chemical composition according to claim 1,
(b) preheating or homogenising the stock,
(c) hot working the stock,
(d) optionally cold working the stock, solution heat treating the stock,
(e) quenching the stock to minimise uncontrolled precipitation of secondary phases, and
(f) ageing the quenched stock to provide an alloy product in a T4 temper or in a T6 temper.

### Claim 24 (depends on 23)

The method according to claim 23, wherein the hot working comprises hot rolling the stock.

### Claim 25 (depends on 23)

The method according to claim 23, comprising the step of the cold working the stock.

### Claim 26 (depends on 25)

The method of claim 25, wherein the cold working comprises cold rolling the stock.

### Claim 27 (depends on 1)

Product manufactured by a method comprising the sequential steps of:
(a) providing stock having a chemical composition according to claim 1,
(b) preheating or homogenising the stock,
(c) hot working the stock,
(d) optionally cold working the stock solution heat treating the stock,
(e) quenching the stock to minimise uncontrolled precipitation of secondary phases, and
(f) ageing the quenched stock to provide an alloy product in a T4 temper or in a T6 temper,
wherein the product is a structural component of an aircraft.

### Claim 28 (depends on 1)

Product manufactured by a method comprising the sequential steps of:
(a) providing stock having a chemical composition according to claim 1,
(b) preheating or homogenising the stock,
(c) hot working the stock,
(d) optionally cold working the stock, solution heat treating the stock,
(e) quenching the stock to minimise uncontrolled precipitation of secondary phases, and
(f) ageing the quenched stock to provide an alloy product in a T4 temper or in a T6 temper,
wherein the product is aircraft skin material.

### Claim 29 (depends on 1)

Product in accordance with claim 1, wherein said product comprises zero weight-percent of Zr.

### Claim 30 (depends on 1)

Product in accordance with claim 1, wherein the Mn level is in the range of 0.65 to 0.8%.

### Claim 31 (depends on 1)

Product in accordance with claim 1, wherein the Ti level is in the range of 0.07 to 0.16%.

### Claim 32 (depends on 1)

Product in accordance with claim 1, wherein the V level is in the range of 0.06 to 0.20%.

### Claim 33 (depends on 1)

Product in accordance with claim 1, wherein the V level is in the range of 0.07 to 0.16%.

### Claim 34 (depends on 1)

Product in accordance with claim 1, wherein the product has a more than 90% recrystallized microstructure.