# US 2006/0078485 A1 · Process of making a water dispersible titanium dioxide pigment useful in paper laminates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0078485 A1
- Document ID: US20060078485A1
- Status: Published application
- Kind: A1
- Application number: 10/540,605
- Filed: 2003-12-26
- Published: 2006-04-13
- Earliest claimed: 2002-12-30
- Inventors: Erik Thiele; John Bolt; Scott Mehr
- Web page: https://patentgrep.com/patent/US20060078485A1

## CPC

- C09C 1/3653: {Treatment with inorganic compounds}
- C09C 1/3661: {Coating}
- D21H 17/69: modified, e.g. by association with other compositions prior to incorporation in the pulp or paper
- C01P 2004/84: one phase coated with the other
- D21H 17/675: {Oxides, hydroxides or carbonates}
- Y10T 428/24934: including paper layer
- Y10T 428/257: Iron oxide or aluminum oxide
- C09C: TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS, TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES (treatment of materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone C04B14/00, C04B18/00, C04B20/00); PREPARATION OF CARBON BLACK {; PREPARATION OF INORGANIC MATERIALS WHICH ARE NO SINGLE CHEMICAL COMPOUNDS AND WHICH ARE MAINLY USED AS PIGMENTS OR FILLERS}
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention relates to a process for making a titanium dioxide pigment having consisting of titanium dioxide and single layer of inorganic surface treatment consisting of aluminum phosphate wherein the pigment is characterized by and isoelectric point which is greater than pH 6 and a negative zeta potential of at a pH of 7.5 or more.

## Claims

### Claim 1

A process for making a water dispersible titanium dioxide pigment comprising:
(a) mixing dry titanium dioxide pigment with water to form a mixture having a pigment concentration of from about 14 to 40 weight percent based on the weight of the mixture then adjusting the pH of this mixture to about 7 with aqueous sodium hydroxide;
(b) heating the mixture from step (a) to a temperature of about 40° C.;
(c) adding to the mixture from step (a) simultaneously and at a rate such that the pH of the resulting mixture is maintained at about 7 throughout this step (c) from about 0.15 to 0.65 moles of phosphoric acid per kilogram of dry pigment and at least a portion of sodium aluminate aqueous solution required to react with the phosphoric acid to form aluminum phosphate;
(d) adding any remaining aqueous sodium aluminate solution required to react with unreacted phosphoric acid added in step (c) to complete the formation of aluminum phosphate simultaneously with a solution of hydrochloric acid wherein the rate of addition of aluminate solution and that of the acid solution is adjusted so that that the pH of the resulting mixture from and in this step (d) is maintained in a range from 5 to 8; and
(e) curing the mixture from step (d) for from about 10 to 30 minutes.

### Claim 2 (depends on 1)

The process of claim 1 wherein in step (c) the addition of aqueous sodium aluminate is made so that the ratio of the moles of phosphorous added to the moles of aluminum added is from about 0.2 to 0.9.

### Claim 3 (depends on 1)

The process of claim 1 wherein in step (c) the addition of aqueous sodium aluminate is made so that the ratio of the moles of phosphorous added to the moles of aluminum added is from about 0.25 to 0.6.

### Claim 4 (depends on 1)

The process of claim 1 wherein in step (c) the addition of aqueous sodium aluminate is made so that the ratio of the moles of phosphorous added to the moles of aluminum added is about 0.5.

### Claim 5 (depends on 1)

The process of claim 1 wherein the amount of phosphoric acid added in step (c) is from about 0.23 to 0.52 moles per kilogram of pigment.

### Claim 6 (depends on 1)

The process of claim 1 wherein the amount of phosphoric acid added in step (c) is about 0.40 moles per kilogram of pigment.

### Claim 7 (depends on 1)

The process of claim 1 wherein the amount of phosphoric acid added in step (c) is about 0.44.

### Claim 8 (depends on 1)

The process according to claim 1 wherein in place of step (c), (i) first adding the phosphoric acid solution to the mixture from step (a) without the simultaneous addition of aqueous sodium aluminate, and then (ii) adding the solution of the sodium aluminate in an amount sufficient to raise the pH of the mixture from step (i) to a pH of about 7.

### Claim 9

A light fast titanium dioxide pigment consisting of titanium dioxide and single layer of inorganic surface treatment consisting of aluminum phosphate wherein the pigment is characterized by and isoelectric point which is greater than pH 6 and a negative zeta potential of less than negative 20 at a pH of 7.5 or more.

### Claim 10

A titanium dioxide pigment consisting of titanium dioxide and single layer of inorganic surface treatment consisting of aluminum phosphate wherein the pigment is characterized by an isoelectric point which is greater than pH 6 and a negative zeta potential of less than negative 20 at a pH of 7.5 or more made by a process comprising:
(a) mixing dry titanium dioxide pigment with water to form a mixture having a pigment concentration of from about 14 to 40 weight percent based on the weight of the mixture then adjusting the pH of this mixture to about 7 with aqueous sodium hydroxide;
(b) heating the mixture from step (a) to a temperature of about 40° C.;
(c) adding to the mixture from step (a) simultaneously and at a rate such that the pH of the resulting mixture is maintained at about 7 throughout this step (c) from about 0.15 to 0.65 moles of phosphoric acid per kilogram of dry pigment and at least a portion of sodium aluminate aqueous solution required to react with the phosphoric acid to form aluminum phosphate;
(d) adding any remaining aqueous sodium aluminate solution required to react with unreacted phosphoric acid added in step (c) to complete the formation of aluminum phosphate simultaneously with a solution of hydrochloric acid wherein the rate of addition of aluminate solution and that of the acid solution is adjusted so that that the pH of the resulting mixture from and in this step (d) is maintained in a range from 5 to 8; and
(e) curing the mixture from step (d) for from about 10 to 30 minutes.

### Claim 11 (depends on 10)

The pigment of claim 10 wherein the dry titanium dioxide in step (a) is rutile.

### Claim 12 (depends on 1)

The process of claim 1 or wherein following step (e) the mixture is filtered and the pigment recovered and washed and dried then micronized at a temperature of from 200 to 420° C.

### Claim 13 (depends on 9)

A laminate paper containing titanium dioxide pigment of claim claim 9.

### Claim 14 (depends on 9)

A paper laminate comprising paper pulp and a titanium dioxide pigment of claim 9.