# US 2006/0076680 A1 · Submicron contact fill using a CVD TiN barrier and high temperature PVD aluminum alloy deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0076680 A1
- Document ID: US20060076680A1
- Status: Published application
- Kind: A1
- Application number: 11/030,035
- Filed: 2005-01-06
- Published: 2006-04-13
- Earliest claimed: 2004-09-30
- Assignees: Microchip Technology Incorporated
- Inventors: Jacob Williams; Harold Kline
- Web page: https://patentgrep.com/patent/US20060076680A1

## CPC

- H10W 20/035: {combinations of barrier, adhesion or liner layers, e.g. multi-layered barrier layers}
- H10W 20/038: {covering conductive structures (H10W20/037 takes precedence)}
- H10W 20/047: {by introducing additional elements therein}
- H10W 20/048: {by using plasmas or gaseous environments, e.g. by nitriding}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A submicron contact opening fill using a chemical vapor deposition (CVD) TiN liner/barrier and a high temperature, e.g., greater than about 385° C., physical vapor deposition (PVD) aluminum alloy layer that substantially fills the submicron contact.

## Claims

### Claim 1

A method for forming a contact on a substrate of a semiconductor integrated circuit, said method comprising the steps of:
a) forming an opening in an insulating layer over a contact area on a semiconductor integrated circuit substrate;
b) cleaning the opening and the contact area;
c) depositing a layer of titanium (Ti) by ionized metal plasma (IMP) physical vapor deposition (PVD) in the opening and on the contact area;
d) depositing a layer of titanium nitride (TiN) by chemical vapor deposition (CVD) on the layer of Ti deposited in step c);
e) forming titanium silicide (TiSi2) (C 54) at the contact area by rapid thermal processing;
f) depositing another layer of titanium nitride (TiN) by chemical vapor deposition (CVD) on the layer of titanium nitride (TiN) deposited in step d) and on the TiSi2 (C 54) formed in step e);
g) depositing another layer of titanium (Ti) by physical vapor deposition (PVD) on the another layer of TiN deposited in step f);
h) depositing a layer of aluminum alloy by physical vapor deposition (PVD) on the layer of Ti deposited in step g), wherein the thickness of the layer of the deposited aluminum alloy is sufficient to substantially fill the opening; and
i) depositing a layer of anti-reflective metal on the aluminum alloy deposited in step h).

### Claim 2

The method according to 1, further comprising the step of stuffing the layers of TiN deposited in steps d) and f) with nitrogen.

### Claim 3

The method according to 2, wherein the nitrogen is obtained from ammonia (NH3) and nitrogen (N2) gases.

### Claim 4

The method according to 3, wherein the step of stuffing nitrogen is the step of stuffing nitrogen at a temperature of about 500 degrees Celsius.

### Claim 5

The method according to 1, wherein the deposited layer of ionized metal plasma (IMP) titanium (Ti) of step c) is from about 50 to about 150 Angstroms in thickness.

### Claim 6

The method according to 1, wherein the deposited layer of ionized metal plasma (IMP) titanium (Ti) of step c) is about 100 Angstroms in thickness.

### Claim 7

The method according to 1, wherein the deposited layer of titanium nitride (TiN) of step d) is from about 50 to about 150 Angstroms in thickness.

### Claim 8

The method according to 1, wherein the deposited layer of titanium nitride (TiN) of step d) is about 100 Angstroms in thickness.

### Claim 9

The method according to 1, wherein the step of forming titanium silicide (TiSi2) (C 54) at the contact area by rapid thermal processing is done at a temperature of about 750 degrees Celsius.

### Claim 10

The method according to 1, wherein the deposited another layer of titanium nitride (TiN) of step f) is from about 50 to about 150 Angstroms in thickness.

### Claim 11

The method according to 1, wherein the deposited another layer of titanium nitride (TiN) of step f) is about 100 Angstroms in thickness.

### Claim 12

The method according to 1, wherein the deposited another layer of titanium (Ti) of step g) is from about 400 to about 1500 Angstroms in thickness.

### Claim 13

The method according to 1, wherein the deposited another layer of titanium (Ti) of step g) is about 700 Angstroms in thickness.

### Claim 14

The method according to 1, wherein the deposited layer of aluminum alloy of step h) is from about 2,000 to about 10,000 Angstroms in thickness.

### Claim 15

The method according to 1, wherein the deposited layer of aluminum alloy of step h) is about 5,000 Angstroms in thickness.

### Claim 16

The method according to 1, wherein the step of depositing the layer of aluminum alloy is done at a temperature higher than 385 degrees Celsius.

### Claim 17

The method according to 1, wherein the layer of aluminum alloy comprises aluminum, silicon and copper.

### Claim 18

The method according to 1, wherein the layer of aluminum alloy comprises aluminum, about one percent silicon and about 0.5 percent copper.

### Claim 19

The method according to 1, wherein the anti-reflective metal of step i) comprises TiN.

### Claim 20

The method according to 1, wherein the anti-reflective metal of step i) comprises molybdenum silicide (MoSix).

### Claim 21

The method according to 1, wherein the anti-reflective metal of step i) comprises molybdenum silicide (MoSi2.35).

### Claim 22

A method for forming a contact on a substrate of a semiconductor integrated circuit, said method comprising the steps of:
a) forming an opening in an insulating layer over a contact area on a semiconductor integrated circuit substrate;
b) cleaning the opening and the contact area;
c) depositing a layer of titanium (Ti) by ionized metal plasma (IMP) physical vapor deposition (PVD) in the opening and on the contact area to a thickness of about 50 to about 150 Angstroms;
d) depositing a layer of titanium nitride (TiN) by chemical vapor deposition (CVD) on the layer of Ti deposited in step c) to a thickness of about 50 to about 150 Angstroms;
e) forming titanium silicide (TiSi2) (C 54) at the contact area by rapid thermal processing at a temperature of about 750 degrees Celsius;
f) depositing another layer of titanium nitride (TiN) by chemical vapor deposition (CVD) on the layer of titanium nitride (TiN) deposited in step d) and on the TiSi2 (C 54) formed in step e) to a thickness of about 50 to about 150 Angstroms;
g) stuffing the layers of TiN deposited in steps d) and f) with nitrogen at a temperature of about 500 degrees Celsius;
h) depositing another layer of titanium (Ti) by physical vapor deposition (PVD) on the another layer of TiN deposited in step f) to a thickness of about 400 to about 1500 Angstroms;
i) depositing a layer of aluminum alloy by physical vapor deposition (PVD) on the layer of Ti deposited in step h) to a thickness of about 2,000 to about 10,000 Angstroms at a temperature higher than 385 degrees Celsius, wherein the thickness of the layer of the deposited aluminum alloy is sufficient to substantially fill the opening; and
j) depositing a layer of anti-reflective metal on the aluminum alloy deposited in step i).

### Claim 23 (depends on 1)

A semiconductor apparatus comprising a contact formed by the method of claim 1.

### Claim 24 (depends on 22)

A semiconductor apparatus comprising a contact formed by the method of claim 22.