# US 2006/0076652 A1 · Method of forming a field effect transistor comprising a stressed channel region

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0076652 A1
- Document ID: US20060076652A1
- Status: Published application
- Kind: A1
- Application number: 11/125,046
- Filed: 2005-05-09
- Published: 2006-04-13
- Earliest claimed: 2004-09-30
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Joerg Hohage; Hartmut Ruelke; Kai Frohberg
- Web page: https://patentgrep.com/patent/US20060076652A1

## CPC

- H10D 30/792: {comprising applied insulating layers, e.g. stress liners}
- H10D 84/0128: {Manufacturing their channels}
- H10D 84/0135: {Manufacturing their gate conductors}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 30/0212: {using self-aligned silicidation}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A semiconductor structure comprises a transistor element formed in a substrate. A stressed layer is formed over the transistor element. The stressed layer has a predetermined tensile intrinsic stress of about 900 MPa or more. Due to this high intrinsic stress, the stressed layer exerts considerable elastic forces to the channel region of the transistor element. Thus, tensile stress is created in the channel region. The tensile stress leads to an increase of the electron mobility in the channel region.

## Claims

### Claim 1

A method of forming a semiconductor structure, comprising:
providing a substrate comprising a transistor element; and
forming a stressed layer over said transistor element, said stressed layer having a predetermined tensile intrinsic stress of at least about 900 MPa.

### Claim 2 (depends on 1)

The method of claim 1, wherein said predetermined tensile intrinsic stress is at least about 1000 MPa.

### Claim 3 (depends on 1)

The method of claim 1, wherein said predetermined tensile intrinsic stress is at least about 1100 MPa.

### Claim 4 (depends on 1)

The method of claim 1, wherein said predetermined tensile intrinsic stress is in a range from about 900 MPa to about 1200 MPa.

### Claim 5 (depends on 1)

The method of claim 1, wherein said stressed layer comprises silicon nitride.

### Claim 6 (depends on 1)

The method of claim 1, wherein said formation of said stressed layer comprises performing a plasma enhanced chemical vapor deposition process.

### Claim 7 (depends on 6)

The method of claim 6, wherein said plasma enhanced chemical vapor deposition process is performed at a temperature of about 400° C. or more.

### Claim 8 (depends on 6)

The method of claim 6, wherein said plasma enhanced chemical vapor deposition process is performed at a temperature of about 450° C. or more.

### Claim 9 (depends on 6)

The method of claim 6, wherein said plasma enhanced chemical vapor deposition process is performed at a temperature of about 500° C. or more.

### Claim 10 (depends on 6)

The method of claim 6, wherein said plasma enhanced chemical vapor deposition process is performed substantially without a bias voltage.

### Claim 11 (depends on 6)

The method of claim 6, wherein performing said plasma enhanced chemical vapor deposition process comprises providing a flow of ammonia and a flow of silane, a ratio between said flow of silane and said flow of ammonia being at least about 0.6.

### Claim 12 (depends on 6)

The method of claim 6, wherein performing said plasma enhanced chemical vapor deposition process comprises:
providing a flow of silane, a ratio between said flow of silane and a volume of a reactor vessel being about 0.013 sccm/cm3;
providing a flow of ammonia, a ratio between said flow of ammonia and said volume of said reactor vessel being about 0.02 sccm/cm3; and
providing a flow of nitrogen, a ratio between said flow of nitrogen and said volume of said reactor vessel being about 0.66 sccm/cm3.

### Claim 13 (depends on 6)

The method of claim 6, wherein said plasma enhanced chemical vapor deposition process is performed at a pressure of about 4.8 Torr.

### Claim 14 (depends on 6)

The method of claim 6, wherein performing said plasma enhanced chemical vapor deposition process comprises applying a radio-frequency alternating voltage, a ratio between a power of said radio-frequency alternating voltage and an area of a surface of said substrate having a value of about 0.2 W/cm2 or less.

### Claim 15 (depends on 1)

The method of claim 1, wherein said stressed layer is formed on a source region and a drain region of said transistor element.

### Claim 16 (depends on 1)

The method of claim 1, further comprising forming at least one contact via through said stressed layer, said contact via being located over said transistor element.

### Claim 17 (depends on 1)

The method of claim 1, wherein said transistor element is an N-type transistor.

### Claim 18

A method of forming a semiconductor structure, comprising:
providing a substrate comprising a first transistor element and a second transistor element;
forming a first stressed layer over said first transistor element; and
forming a second stressed layer over said second transistor element, wherein said second stressed layer does not cover said first transistor element;
wherein at least one of said first stressed layer and said second stressed layer has a predetermined tensile intrinsic stress of at least about 900 MPa.

### Claim 19 (depends on 18)

The method of claim 18, wherein said first stressed layer is formed over both said first transistor element and said second transistor element.

### Claim 20 (depends on 18)

The method of claim 18, wherein said first stressed layer does not cover said second transistor element.

### Claim 21 (depends on 18)

The method of claim 18, further comprising:
forming a first dielectric layer over said first transistor element but not over said second transistor element;
forming a second dielectric layer over said substrate; and
planarizing said first dielectric layer and said second dielectric layer;
wherein said second stressed layer is formed after formation of said first dielectric layer and before formation of said second dielectric layer, and a portion of said second dielectric layer located over said first transistor element is removed in said planarization.

### Claim 22 (depends on 18)

The method of claim 18, wherein said at least one of said first stressed layer and said second stressed layer comprises silicon nitride.

### Claim 23 (depends on 18)

The method of claim 18, wherein formation of said at least one of said first stressed layer and said second stressed layer comprises performing a plasma enhanced chemical vapor deposition process.

### Claim 24 (depends on 23)

The method of claim 23, wherein said plasma enhanced chemical vapor deposition process is performed at a temperature of about 400° C. or more.

### Claim 25 (depends on 23)

The method of claim 23, wherein said plasma enhanced chemical vapor deposition process is performed at a temperature of about 450° C. or more.

### Claim 26 (depends on 23)

The method of claim 23, wherein said plasma enhanced chemical vapor deposition process is performed at a temperature of about 500° C. or more.

### Claim 27 (depends on 23)

The method of claim 23, wherein said plasma enhanced chemical vapor deposition process is performed substantially without a bias voltage.

### Claim 28 (depends on 23)

The method of claim 23, wherein performing said plasma enhanced chemical vapor deposition process comprises providing a flow of ammonia and a flow of silane, a ratio between said flow of silane and said flow of ammonia being about 0.6 or more.

### Claim 29 (depends on 23)

The method of claim 23, wherein performing said plasma enhanced chemical vapor deposition process comprises:
providing a flow of silane, a ratio between said flow of silane and a volume of a reactor vessel being about 0.013 sccm/cm3;
providing a flow of ammonia, a ratio between said flow of ammonia and said volume of said reactor vessel being about 0.02 sccm/cm3; and
providing a flow of nitrogen, a ratio between said flow of nitrogen and said volume of said reactor vessel being about 0.66 sccm/cm3.

### Claim 30 (depends on 23)

The method of claim 23, wherein said plasma enhanced chemical vapor deposition process is performed at a pressure of about 4.8 Torr.

### Claim 31 (depends on 23)

The method of claim 23, wherein performing said plasma enhanced chemical vapor deposition process comprises applying a radio-frequency alternating voltage, a ratio between a power of said radio-frequency alternating voltage and an area of a surface of said substrate having a value of about 0.2 W/cm2 or less.

### Claim 32 (depends on 18)

The method of claim 18, wherein said first stressed layer is formed on a source region and a drain region of said first transistor element.

### Claim 33 (depends on 18)

The method of claim 18, further comprising forming at least one first contact via through said first stressed layer and forming at least one second contact via through said second stressed layer, said at least one first contact via being located over said first transistor element, said at least one second contact via being located over said second transistor element.

### Claim 34

A semiconductor structure, comprising:
a substrate comprising a transistor element; and
a stressed layer formed over said transistor element, said stressed layer having a predetermined tensile intrinsic stress of at least about 900 MPa.

### Claim 35 (depends on 34)

The semiconductor structure of claim 34, wherein said predetermined tensile intrinsic stress is at least about 1000 MPa.

### Claim 36 (depends on 34)

The semiconductor structure of claim 34, wherein said predetermined tensile intrinsic stress is at least about 1100 MPa.

### Claim 37 (depends on 34)

The semiconductor structure of claim 34, wherein said predetermined tensile intrinsic stress is in a range from about 900-1200 MPa.

### Claim 38 (depends on 34)

The semiconductor structure of claim 34, wherein said stressed layer comprises silicon nitride.

### Claim 39 (depends on 34)

The semiconductor structure of claim 34, wherein said stressed layer is formed on a source region and a drain region of said transistor element.

### Claim 40 (depends on 34)

The semiconductor structure of claim 34, further comprising at least one contact via formed through said stressed layer, said at least one contact via being located over said transistor element.

### Claim 41

A semiconductor structure, comprising:
a substrate comprising a first transistor element and a second transistor element;
a first stressed layer formed over said first transistor element; and
a second stressed layer formed over said second transistor element, wherein said second stressed layer does not cover said first transistor element;
wherein at least one of said first stressed layer and said second stressed layer has a predetermined tensile intrinsic stress of at least about 900 MPa.

### Claim 42 (depends on 41)

The semiconductor structure of claim 41, wherein said first stressed layer is formed both over said first transistor element and said second transistor element.

### Claim 43 (depends on 41)

The semiconductor structure of claim 41, wherein said first stressed layer does not cover said second transistor element.

### Claim 44 (depends on 41)

The semiconductor structure of claim 41, wherein a channel region of said first transistor element is stressed and a channel region of said second transistor element is substantially unstressed.

### Claim 45 (depends on 41)

The semiconductor structure of claim 41, wherein at least one of said first stressed layer and said second stressed layer comprises silicon nitride.

### Claim 46 (depends on 41)

The semiconductor structure of claim 41, wherein said predetermined tensile intrinsic stress is about 1000 MPa or more.

### Claim 47 (depends on 41)

The semiconductor structure of claim 41, wherein said predetermined tensile intrinsic stress is about 1100 MPa or more.

### Claim 48 (depends on 41)

The semiconductor structure of claim 41, wherein said predetermined tensile intrinsic stress is in a range from about 900-1200 MPa.

### Claim 49 (depends on 41)

The semiconductor structure of claim 41, wherein said first stressed layer is formed on a source region and a drain region of said first transistor element.

### Claim 50 (depends on 41)

The semiconductor structure of claim 41, further comprising at least one first contact via formed through said first stressed layer and at least one second contact via formed through said second stressed layer, said at least one first contact via being located over said first transistor element, said at least one second contact via being located over said second transistor element.