# US 2006/0076106 A1 · Method of making high loft nonwoven

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0076106 A1
- Document ID: US20060076106A1
- Status: Published application
- Kind: A1
- Application number: 11/274,982
- Filed: 2005-11-15
- Published: 2006-04-13
- Earliest claimed: 2003-05-30
- Assignees: Western Nonwovens, Inc.
- Inventors: Sheri McGuire
- Web page: https://patentgrep.com/patent/US20060076106A1

## CPC

- D04H 1/60: the bonding agent being applied in dry state, e.g. thermo-activatable agents in solid or molten state, and heat being applied subsequently
- D04H 1/54: by welding together the fibres, e.g. by partially melting or dissolving (in combination with needling D04H1/485)
- D04H 1/70: characterised by the method of forming fleeces or layers, e.g. reorientation of fibres
- Y10T 442/60: Nonwoven fabric [i.e., nonwoven strand or fiber material]
- Y10T 442/637: Including strand or fiber material which is a monofilament composed of two or more polymeric materials in physically distinct relationship [e.g., sheath-core, side-by-side, islands-in-sea, fibrils-in-matrix, etc.] or composed of physical blend of chemically different polymeric materials or a physical blend of a polymeric material and a filler material
- Y10T 442/69: Autogenously bonded nonwoven fabric
- Y10T 442/692: Containing at least two chemically different strand or fiber materials
- Y10T 442/696: Including strand or fiber material which is stated to have specific attributes [e.g., heat or fire resistance, chemical or solvent resistance, high absorption for aqueous compositions, water solubility, heat shrinkability, etc.]
- Y10T 442/697: Containing at least two chemically different strand or fiber materials
- Y10T 442/698: Containing polymeric and natural strand or fiber materials
- D04H: MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARY MATERIAL (weaving D03; knitting D04B; braiding D04C; net-making D04G; sewing D05B; tufting D05C; finishing non-woven fabrics D06); FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS, NON-WOVEN FABRICS; COTTON-WOOL; WADDING {; NON-WOVEN FABRICS FROM STAPLE FIBRES, FILAMENTS OR YARNS, BONDED WITH AT LEAST ONE WEB-LIKE MATERIAL DURING THEIR CONSOLIDATION}(non-woven fabrics having an intermediate or external layer of a different kind, e.g. of woven fabric, B32B)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention relates to a process for making high loft, nonwoven material by providing either natural and/or synthetic fibers, providing a low melt binder fiber, mixing the low melt binder fiber and the natural and/or synthetic fibers to form a web, cross-lapping the web, drafting the web with a drafter, heating the drafted web to a temperature sufficient to melt the low melt binder fibers, and cooling the web thereby forming a structural nonwoven material. The nonwoven batt can be cross-lapped between 2 and 10 layers and when the batt is cooled and has structural rigidity, the tensile strength in the machine direction is at least 50% of the tensile strength in the cross-direction. The batt weight is in a range of 0.25 oz/ft2 to 2.0 oz/ft2. The low melt binder fibers comprise 10 to 30 wt. % of the nonwoven batt and the synthetic and/or natural fibers comprise about 70 to 90 wt. %. This product is useful for nonwoven applications in indoor and outdoor furniture, quilting, bed covers and mattresses specifically.

## Claims

### Claim 1

A process of making high loft, nonwoven material, comprising the steps of:
providing natural and/or synthetic fibers;
providing low melt binder fibers, wherein the binder fibers comprises low melt fibers or bicomponent fibers;
mixing said low melt fibers and said natural and/or synthetic fibers to form a web;
cross lapping the web;
drafting the web with a drafter;
heating the drafted web to a temperature sufficient to melt the low melt binder fibers; and cooling the web, whereby the nonwoven material is formed.

### Claim 2 (depends on 1)

The process of claim 1, further including the step of attenuating the web with the drafter.

### Claim 3 (depends on 1)

The process of claim 1, wherein the drafter comprising a plurality of zones, wherein each zone includes rollers, and wherein said rollers in each subsequent zone rotate at the same or greater rpm than the rollers in a previous zone.

### Claim 4 (depends on 1)

The process of claim 1, wherein the nonwoven material has a weight that is no more than 2.0 oz/ft2 and has a tensile strength in a machine direction that is at least 50 percent of the tensile strength in a cross direction.

### Claim 5

A process of making high loft, nonwoven batt, comprising the steps of:
providing natural and/or synthetic fibers;
providing low melt binder fibers, wherein said binder fibers comprises low melt fibers or bicomponent fibers;
mixing said low melt fibers and said natural and/or synthetic fibers to form a web;
cross lapping the web, wherein said cross lapping provides between 2 to 10 layers, thus forming a batt;
drafting said batt with a drafter;
heating said drafted batt to a temperature sufficient to melt the low melt binder fibers; and
cooling said batt, said batt having a tensile strength in a machine direction that is at least 50 percent of the tensile strength in a cross direction.

### Claim 6 (depends on 5)

The process of claim 5, wherein said synthetic fiber is selected from the class of polyester, polyamide, polyolefin, polyacrylic, cellulose acetate, melamine, rayon, mixtures of these, or copolymers of these.

### Claim 7 (depends on 5)

The process of claim 5, wherein said natural fiber is selected from the class of cotton, wool, flax, kenaf, hemp, silk, jute, asbestos, ramie, or mixtures of these.

### Claim 8 (depends on 7)

The process of claim 7, wherein said natural fiber is selected from the class of cotton, wool, flax, kenaf, hemp, silk, jute, asbestos, ramie, or mixtures of these

### Claim 9 (depends on 5)

The process of claim 5, wherein the weight of said batt is in the range of 0.25 oz/ft2 to 2.0 oz/ft2.

### Claim 10 (depends on 9)

The process of claim 9, having a loft recovery of at least 90% under a load of 10 lbs per sq. ft, for a duration of 2 minutes.

### Claim 11 (depends on 5)

The process of claim 5, wherein said low melt binder comprises no more than about 30 percent by weight, of the batt.

### Claim 12 (depends on 5)

The process of claim 5, wherein said batt comprises from about 10 to about 20 wt. % low melt binder fibers and wherein said synthetic fiber comprises from about 80 to about 90 wt. % polyester fiber.

### Claim 13 (depends on 12)

The process of claim 12, wherein said polyester comprises fibers of different denier.

### Claim 14 (depends on 13)

The process of claim 13, wherein said denier is from about 15 to about 25.

### Claim 15 (depends on 5)

The process of claim 5, wherein said low melt binder fibers comprises from about 5 to about 25 wt % of said batt.

### Claim 16

A process of making high loft, nonwoven batt, comprising the steps of:
providing polyester fibers;
providing low melt binder fibers, wherein said binder fibers comprises low melt fibers or bicomponent fibers, said low melt binder fibers comprises no more than about 30 percent by weight, of the batt;
mixing said low melt fibers and said polyester fibers to form a web;
cross lapping the web, wherein said cross lapping provides between 2 to 10 layers, thus forming a batt, wherein the weight of said batt is in the range of 0.25 oz/ft2 to 2.0 oz/ft2;
drafting said batt with a drafter;
heating said drafted batt to a temperature sufficient to melt at least a portion of said low melt binder fibers; and
cooling said batt, said batt having a tensile strength in a machine direction that is at least 50 percent of the tensile strength in a cross direction.

### Claim 17 (depends on 16)

The process of claim 16, wherein said tensile strength in the machine direction is greater than the tensile strength in the cross direction.