# US 2006/0076087 A1 · Modified sintered RE-Fe-B-type, rare earth permanent magnets with improved toughness

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0076087 A1
- Document ID: US20060076087A1
- Status: Published application
- Kind: A1
- Application number: 11/284,275
- Filed: 2005-11-21
- Published: 2006-04-13
- Earliest claimed: 2002-04-29
- Inventors: Shiqiang Liu; Jinfang Liu
- Web page: https://patentgrep.com/patent/US20060076087A1

## CPC

- H01F 1/0577: {sintered}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

Compositionally modified, sintered RE-Fe-B-based rare earth permanent magnets demonstrate the optimum combination of mechanical and magnetic properties, thereby maximizing fracture toughness with corresponding improved machinability, while maintaining the maximum energy product (BH)max.

## Claims

### Claim 1

A class of sintered rare earth permanent magnets having improved fracture toughness, suitable for conventional machining and drilling, having a general formula selected from the group consisting of:
(a) NdwFe94-wB6,
wherein: w has a value between about 16 and about 22;
(b) Nd16Fe78-xTixB6, wherein:
x has a value between about 0.78 and about 2.34;
(c) Nd16Fe78-yNbyB6, wherein:
y has a value between about 1.56 and about 2.34; and
(d) Nd16Fe78-zCuzB6, wherein:
z has a value between about 0.78 and about 1.56;
and wherein said rare earth permanent magnet maintains high maximum energy product of at least about 30 MGOe, while showing an improved fracture toughness over conventional sintered Nd—Fe—B rare earth permanent magnets from between about 6% and about 74%.

### Claim 2

In sintered rare earth permanent magnets having the formula, RE-Fe—B, the improvement comprising: modifying said formula according to one of the formulas selected from the group consisting of:
(a) NdwFe94-wB6, wherein:
w has a value between about 14 and about 25;
(b) Nd16Fe78-xTixB6 wherein:
x has a value between about 0.02 and about 2.34;
(c) Nd16Fe78-yNbyB6, wherein:
y has a value between about 0.02 and about 2.34; and
(d) Nd16Fe78-zCuzB6, wherein:
z has a value between about 0.02 and about 1.56;
and wherein said rare earth permanent magnet maintains high energy product, while showing an improved fracture toughness over conventional sintered Nd—Fe—B rare earth permanent magnets from between about 6% and about 74%.

### Claim 3 (depends on 1)

Rare earth permanent magnets according to claim 1, wherein said magnets represented by NdwFe94-wB6 are selected from the group consisting of:
Nd16Fe78B6,
Nd17Fe77B6,
Nd18Fe76B6,
Nd19Fe75B6,
Nd20Fe74B6,
Nd21Fe73B6,
Nd22Fe72B6, and
Nd23Fe71B6.

### Claim 4 (depends on 1)

Rare earth-permanent magnets according to claim 1, wherein said magnets represented by Nd16Fe78-xTixB6 are selected from the group consisting of:
Nd16Fe77.22Ti0.78B6,
Nd16Fe76.44Ti1.56B6,
Nd16Fe75.66Ti2.34B6, and
Nd16Fe74.88Ti3.12B6.

### Claim 5 (depends on 1)

Rare earth permanent magnets according to claim 1, wherein said magnets represented by Nd16Fe78-yNbyB6 are selected from the group consisting of:
Nd16Fe77.22Nb0.78B6,
Nd16Fe76.44Nb1.56B6,
Nd16Fe75.66Nb2.34B6, and
Nd16Fe74.88Nb3.12B6.

### Claim 6 (depends on 1)

Rare earth permanent magnets according to claim 1, wherein said magnets represented by Nd16Fe78-zCuzB6 are selected from the group consisting of:
Nd16Fe77.22Cu0.78B6,
Nd16Fe76.44Cu1.56B6,
Nd16Fe75.66Cu2.34B6, and
Nd16Fe74.88Cu3.12B6.

### Claim 7

A class of rare earth permanent magnets having the following general formula:
R100-mTMmAn,
wherein R is one or a mixture of rare earths or yttrium, TM is one or a mixture of transition metals, A is one or a mixture of the following elements: Be, B, C, Mg, Al, Si, P, Ga, Ge, As, Se, In, Sn, Sb, Te, I, Pb, and Bi, and m=80-92, n=0-20; and
wherein the magnets comprise a main phase and one or more minor phases, wherein the composition of the main phase is expressed as:
R100-fTMfAv,
in which R is one or a mixture of rare earths or yttrium, TM is one or a mixture of transition metals, A is one or a mixture of the following elements: Be, B, C, Mg, Al, Si, P, Ga, Ge, As, Se, In, Sn, Sb, Te, I, Pb, and Bi, and f=75-90, v=0-20;
and wherein the minor phase or phases are rich in transition metal(s) and their composition is expressed as:
R100-qTMqAp,
where R is one or a mixture of rare earths or yttrium, TM is one or a mixture of transition metals, A is one or a mixture of the following elements: Be, B, C, Mg, Al, Si, P, Ga, Ge, As, Se, In, Sn, Sb, Te, I, Pb, and Bi, and q=85-100, p=0-20; and wherein the total atomic percentage of transition metals, TM, in the soft minor phases R100-qTMqAp is more than 85%.

### Claim 8 (depends on 7)

The class of rare earth permanent magnets of claim 7, wherein the total atomic percentage of transition metals, TM, in the soft minor phases R100-qTMqAp is more than 90%.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

Rare earth permanent magnets as described in any of claims 1 through 8 that possess fracture toughness equal to or greater than 15 ft-lbs/in2 at 20° C.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

Rare earth permanent magnets as described in any of claims 1 through 8 that possess fracture toughness equal to or greater than 20 ft-lbs/in2 at 20° C.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

Rare earth permanent magnets as described in any of claims 1 through 8 that have an average grain size smaller than 25 microns.

### Claim 12 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

Rare earth permanent magnets as described in any of claims 1 through 8 that have an average grain size smaller than 15 microns.