# US 2006/0075626 A1 · Single-atom tip and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0075626 A1
- Document ID: US20060075626A1
- Status: Published application
- Kind: A1
- Application number: 10/985,717
- Filed: 2004-10-09
- Published: 2006-04-13
- Earliest claimed: 2004-10-09
- Assignees: Academia Sinica
- Inventors: Ing-Shouh Hwang; Hong-Shi Kuo; Tien Tsong; Tsu-Yi Fu
- Web page: https://patentgrep.com/patent/US20060075626A1

## CPC

- C25F 1/00: Electrolytic cleaning, degreasing, pickling or descaling
- C25D 5/003: {Electroplating using gases, e.g. pressure influence}
- C25D 5/022: {using masking means}
- C25D 5/38: of refractory metals or nickel
- C25D 5/48: After-treatment of electroplated surfaces
- C25D 5/50: by heat-treatment
- G01Q 70/16: Probe manufacture
- H01J 9/025: {of field emission cathodes}
- H01J 37/073: Electron guns using field emission, photo emission, or secondary emission electron sources
- H01J 37/08: Ion sources; Ion guns
- C25D 3/48: of gold
- C25D 3/50: of platinum group metals
- H01J 2237/06341: Field emission
- H01J 2237/0807: Gas field ion sources [GFIS]
- Y10T 29/49002: Electrical device making
- C25F: PROCESSES FOR THE ELECTROLYTIC REMOVAL OF MATERIALS FROM OBJECTS; APPARATUS THEREFOR
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- G01Q: SCANNING-PROBE TECHNIQUES OR APPARATUS; APPLICATIONS OF SCANNING-PROBE TECHNIQUES, e.g. SCANNING PROBE MICROSCOPY [SPM]
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

This invention discloses an electrochemical method for the preparation of single atom tips to replace the traditional vacuum evaporation method. The invented method for preparation of single atom tips includes the following steps: A substrate single crystal metal wire etched electrochemically to form a tip. The surface of the metal tip is cleaned. A small quantity of noble metal is plated on the apex of the tip in low concentration noble metal electrolyte. Annealing in vacuum or in inert gas ambient to diffuse the additional electroplated noble metal atoms and thus a single atom tip is formed on the surface of the substrate. The present invention also discloses the single atom tip so prepared. The single atom tip of this invention has only a very small number of atoms, usually only one atom, at its apex.

## Claims

### Claim 1

Method for preparation of a metal tip terminated by a small number of atoms, comprising the following steps:
preparing a metal tip;
cleaning said metal tip;
electroplating on said metal tip a tiny quantity of noble metal; and
thermal processing said plated metal tip to form a pyramid structure terminated by a small number of atoms on apex of said metal tip.

### Claim 2 (depends on 1)

The method according to claim 1, wherein material of said metal tip is selected from the group consisted of tungsten, molybdenum or their alloy.

### Claim 3 (depends on 2)

The method according to claim 2, wherein material of said metal tip is single-crystal <111> wire.

### Claim 4 (depends on 1)

The method according to claim 1, wherein preparing of said metal tip comprises etching a metal wire in an etchant liquid to form a tip shape in said metal wire.

### Claim 5 (depends on 4)

The method according to claim 4, wherein said etchant liquid comprises NaOH, KOH or NH4OH aqueous solution, with a concentration from 0.1 M to saturation.

### Claim 6 (depends on 5)

The method according to claim 5, further comprising a step of applying a voltage or a current to said etchant liquid during etching, wherein said voltage or current is supplied by a DC power supply or an AC power supply.

### Claim 7 (depends on 1)

The method according to claim 1, wherein cleaning of said metal tip comprises cathodic polarization said metal tip in a base aqueous solution.

### Claim 8 (depends on 7)

The method according to claim 7, wherein said base aqueous solution is an acid aqueous solution comprising one or more selected from the group of hydrochloric acid, sulfuric acid, nitric acid, phosphoric acid and chloric acid.

### Claim 9 (depends on 7)

The method according to claim 7, wherein said base aqueous solution is a basic aqueous solution comprising one or more selected from the group of NaOH, KOH and NH4OH.

### Claim 10 (depends on 7)

The method according to claim 7, wherein said base aqueous solution is a salt aqueous solution comprising one or more selected from the group of chlorides such as NaCl and KCl; brominides such as NaBr and KBr; iodides such as NaI and KI; sulfates such as Na2SO4 and K2SO4; phosphates such as Na2HPO3; Nitrate such (NH4)3NO3; cyanates such as NaOCN and KOCN.

### Claim 11 (depends on 7)

The method according to claim 7, wherein said base aqueous solution further comprises an acid buffer agent or a basic buffer agent.

### Claim 12 (depends on 7)

The method according to claim 7, wherein said cathodic polarization comprises applying a cathodic potential on said metal tip in said base aqueous solution using a potentiostat.

### Claim 13 (depends on 7)

The method according to claim 7, wherein said cathodic polarization comprises applying a negative voltage or negative current to said metal tip in said base aqueous solution using a power supply.

### Claim 14 (depends on 1)

The method according to claim 1, wherein said noble metal is selected from palladium, platinum, iridium, rhodium, gold or their alloy.

### Claim 15 (depends on 1)

The method according to claim 1, wherein said electroplating comprises plating said metal tip by dropping plating electrolyte into said base aqueous solution directly during said cleaning.

### Claim 16 (depends on 15)

The method according to claim 15, wherein said plating electrolyte is an aqueous electrolytic liquid containing soluble noble metal salt.

### Claim 17 (depends on 16)

The method according to claim 16, wherein concentration of said noble metal salt is above 10−7 M.

### Claim 18 (depends on 16)

The method according to claim 16, wherein said noble metal salt comprises a soluble palladium compound selected from the group of palladium chloride, palladium sulfate, palladium nitrate, sodium palladium nitrate and palladium diamminonitrate.

### Claim 19 (depends on 16)

The method according to claim 16, wherein said noble metal salt comprises a soluble platinum compound selected from the group of platinum chloride, platinum sulfate, chloroplatinic acid, sodium chloroplatinate and sodium platinate.

### Claim 20 (depends on 16)

The method according to claim 16, wherein said noble metal salt comprises a soluble iridium compound selected from the group of iridium chloride and (NH4)IrCl6.

### Claim 21 (depends on 16)

The method according to claim 16, wherein said noble metal salt comprises a soluble rhodium compound selected from the group of rhodium chloride, rhodium nitrate and rhodium sulfate.

### Claim 22 (depends on 16)

The method according to claim 16, wherein said noble metal salt comprises a soluble gold compound selected from the group of potassium gold cyanide (PGC), gold cyanide and gold chloride.

### Claim 23 (depends on 15)

The method according to claim 15, wherein concentration of said noble metal ions in said base aqueous solution is maintained in the range from 10−12M to 10−5M, obtained by dropping said plating electrolyte in said base aqueous solution.

### Claim 24 (depends on 1)

The method according to claim 1, wherein said plated metal tip comprises metal tip electroplated with said noble metal on its surface.

### Claim 25 (depends on 1)

The method according to claim 1, wherein said thermal processing comprises annealing said plated metal tip.

### Claim 26 (depends on 25)

The method according to claim 25, wherein said annealing is conducted under 500 to 1,200□ for 30 seconds to 30 hours.

### Claim 27 (depends on 25)

The method according to claim 25, wherein said annealing is conducted in vacuum or in inert gas.

### Claim 28 (depends on 1)

The method according to claim 1, wherein said metal tip is coated with a shielding layer at areas other than its apex region before said electroplating.

### Claim 29 (depends on 28)

The method according to claim 28, wherein said shielding layer comprises a material selected from resin, such as nail polish, ethyl acetate, butyl acetate, paints, hot melt adhesives, ethylene resin, polyurethane, epoxy resin or silicone; oils or wax, such as insulation oil, paraffin wax or Apiezon; or inorganic chemicals, such as silicon oxide, aluminum oxide, silicon nitride or boron nitride.

### Claim 30 (depends on 1)

The method according to claim 1, further comprising a step of applying anodic potentials on said plated metal tip in said base aqueous solution using a potentiostat.

### Claim 31 (depends on 12)

The method according to claim 12, wherein said applied cathodic potential is below −0.4 V (SCE).

### Claim 32 (depends on 13)

The method according to claim 13, wherein said negative voltage is below −0.4 V.

### Claim 33 (depends on 13)

The method according to claim 13, wherein said negative current is greater than 1 nA.

### Claim 34 (depends on 30)

The method according to claim 30, wherein said anodic potentials are above 0.2 V (SCE).

### Claim 35 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26, 27, 28, 29, 30, 31, 32, 33, 34)

A metal tip terminated by a small number of atoms prepared according to the method of anyone of claims 1-34.

### Claim 36 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26, 27, 28, 29, 30, 31, 32, 33, 34)

A single atom metal tip prepared according to the method of anyone of claims 1-34.