Decomposition of Polyester
AssigneeChemical Products Corporation
InventorsLloyd Mauldin, Jerry Cook
Life of this patent
Estimating the term…
Abstract
A process to decompose polyester by heating in the presence of a cyclic ester solvent is disclosed. Physically separated polyester-rich waste can be recycled by forming an admixture with a cyclic ester solvent, preferably propylene carbonate, and heating the admixture to a temperature above about 215 degrees Celsius. The polyester is decomposed into monomers and oligomers which are soluble in ethylene carbonate or propylene carbonate at ambient temperature. The polyester decomposition products are useful as components of an industrial solvent or as inputs to other chemical processes.
Claims18
A method for decomposing the polyester component of a commingled post-consumer or post-industrial waste into monomeric and oligomeric units constituting a portion of an ester solvent composition comprising:
- (a) admixing commingled waste with an initial ester solvent composition containing at least one cyclic ester;
- (b) heating the admixture to a temperature above about 215 degrees Celsius for a period of at least 3 minutes to form a second ester solvent composition;
- (c) cooling the second ester solvent composition to a temperature below about 70 degrees Celsius;
- and (d) separating the second ester solvent composition from solid impurities by sedimentation, flocculation, filtration, centrifugation, or combinations thereof.
A method for decomposing poly(ethylene terephthalate) face fibers from post-consumer carpet into components of a liquid ester solvent composition comprising:
- (a) admixing the poly(ethylene terephthalate) face fibers with an initial ester solvent composition containing principally ethylene carbonate, propylene carbonate, butylene carbonate, or mixtures thereof;
- (b) heating the admixture to a temperature above about 220 degrees Celsius for a period of at least about 5 minutes to form a second ester solvent composition;
- (c) separating the second ester solvent composition from solid polyester and impurities by electrophoresis, sedimentation, flocculation, filtration, centrifugation, or combinations thereof;
- (d) cooling the second ester solvent composition to a temperature below about 30 degrees Celsius;
- and (e) separating the cooled second ester solvent composition from precipitated solids by electrophoresis, sedimentation, flocculation, filtration, centrifugation, or combinations thereof.
A method for decomposing polyester into compounds having an appreciable solubility in cyclic esters at about 30 degrees Celsius and constituting a component of a liquid ester solvent composition comprising:
- (a) admixing polyester with ethylene carbonate, propylene carbonate, butylene carbonate, or mixtures thereof;
- (b) heating the admixture to a temperature above about 220 degrees Celsius for a period of at least about 5 minutes to form an ester solvent composition;
- (c) separating the ester solvent composition from solid polyester and impurities by sedimentation, flocculation, filtration, centrifugation, or combinations thereof;
- (d) cooling the ester solvent composition to a temperature below about 50 degrees Celsius;
- and (e) separating the cooled ester solvent composition from precipitated solids by sedimentation, flocculation, filtration, centrifugation, or combinations thereof.
Chemical compositions employed as solvents containing at least (1) decomposition products of poly(ethylene terephthalate) polyester and (2) one or more cyclic esters.
Chemical compositions employed as solvents containing as one component compounds resulting from the thermal degredation of poly(ethylene terephthalate) dissolved in ethylene carbonate, propylene carbonate, butylene carbonate, or mixtures thereof.