# US 2006/0068126 A1 · Method for making an aligned carbon nanotube

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0068126 A1
- Document ID: US20060068126A1
- Status: Published application
- Kind: A1
- Application number: 11/030,364
- Filed: 2005-01-05
- Published: 2006-03-30
- Earliest claimed: 2004-09-30
- Assignees: National Cheng Kung University
- Inventors: Jyh-Ming Ting; Kun-Hou Liao
- Web page: https://patentgrep.com/patent/US20060068126A1

## CPC

- C01B 32/162: characterised by catalysts
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/274: {using seed materials}
- H10P 14/3406: {Carbon, e.g. diamond-like carbon}
- H10P 14/3464: {Nanotubes}
- C01B 2202/08: Aligned nanotubes
- C01B 2202/36: Diameter
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for making an aligned carbon nanotube includes the steps of a) applying a layer of a ferrosilicon alloy film onto a substrate, b) etching the layer of the ferrosilicon film to form a plurality of fine ferrosilicon alloy particles that are distributed properly on the substrate, and c) placing the substrate of step (b) into a microwave plasma enhanced chemical vapor deposition system, and supplying a mixture of a carbon-containing reaction gas and a balance gas at a predetermined flow ratio so as to grow carbon nanotubes on the fine ferrosilicon alloy particles.

## Claims

### Claim 1

A method for making an aligned carbon nanotube, comprising the steps of:
(a) applying a layer of a ferrosilicon alloy film onto a substrate;
(b) etching the layer of the ferrosilicon film to form a plurality of fine ferrosilicon alloy particles that are distributed properly on the substrate; and
(c) placing the substrate of step (b) into a microwave plasma enhanced chemical vapor deposition system, and supplying a mixture of a carbon-containing reaction gas and a balance gas at a predetermined flow ratio so as to grow carbon nanotubes on the fine ferrosilicon alloy particles.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein step (c) is conducted at a temperature ranging from 300 to 380° C.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein step (c) is conducted at a microwave power ranging from 250 to 1500 W and at a working pressure ranging from 20 to 40 Torr.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the substrate is selected from the group consisting of silicon substrates and polymer substrates.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein step (a) is conducted by a process selected from the group consisting of sputtering, chemical vapor deposition, physical vapor deposition, electroplating, and printing.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein step (b) is conducted by placing the substrate coated with the layer of the ferrosilicon alloy film in the microwave plasma enhanced chemical vapor deposition system and supplying an etching gas into the microwave plasma enhanced chemical vapor deposition system.

### Claim 7 (depends on 6)

The method as claimed in claim 6, wherein the etching gas includes at least one gas selected from the group consisting of hydrogen, oxygen, nitrogen, and ammonia.

### Claim 8 (depends on 6)

The method as claimed in claim 6, wherein each of the fine ferrosilicon alloy particles has a particle size ranging from 5 to 25 nm.

### Claim 9 (depends on 6)

The method as claimed in claim 6, wherein the fine ferrosilicon alloy particles have a distribution density ranging from 3×1010 to 4×1010 cm−2.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the predetermined flow ratio of the carbon-containing reaction gas to the balance gas is 2:9.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein the carbon-containing reaction gas includes at least one gas selected from the group consisting of methane, ethane, propane, ethyne, and benzene.

### Claim 12 (depends on 10)

The method as claimed in claim 10, wherein the balance gas includes at least one gas selected from the group consisting of hydrogen, oxygen, nitrogen, and ammonia.