# US 2006/0066327 A1 · Method and structures for testing a semiconductor wafer prior to performing a flip chip bumping process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0066327 A1
- Document ID: US20060066327A1
- Status: Published application
- Kind: A1
- Application number: 10/953,291
- Filed: 2004-09-29
- Published: 2006-03-30
- Earliest claimed: 2004-09-29
- Assignees: Agere Systems Inc.
- Inventors: Mark Bachman; Daniel Chesire; Taeho Kook; Sailesh Merchant
- Web page: https://patentgrep.com/patent/US20060066327A1

## CPC

- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10P 74/273: {Interconnections for measuring or testing, e.g. probe pads}
- H10W 72/019: {of bond pads}
- H10W 72/251: {Materials}
- H10W 72/90: Bond pads, in general
- H10W 72/922: {Bond pads being integral with underlying chip-level interconnections}
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

An interface assembly (20) and method for testing a semiconductor wafer prior to performing a flip chip bumping process are provided. The interface assembly includes a flip chip bonding pad (24) having a region (28) for performing the bumping process. A test pad (22) is integrally constructed with the bonding pad and includes a probe region (26) for performing wafer-level testing prior to performing the bumping process. The integral construction of the bonding and testing pads avoids, for example, an introduction of propagation delays to test signals passing therethrough, thereby improving the accuracy and reliability of wafer test results.

## Claims

### Claim 1

An interface assembly for a semiconductor wafer, said interface assembly comprising:
a flip chip bonding pad including a region for performing a bumping process; and
a test pad integrally constructed with said bonding pad, said test pad being coplanar relative to said flip chip bonding pad and including a probe region for performing wafer-level testing prior to performing said bumping process.

### Claim 2 (depends on 1)

The interface assembly of claim 1 wherein said test pad may be disposed anywhere along a periphery of said bonding pad.

### Claim 3 (depends on 1)

The interface assembly of claim 1 wherein said bonding pad comprises a shape selected from the group consisting of a polygonal shape, and a circular shape.

### Claim 4 (depends on 1)

The interface assembly of claim 1 wherein said test pad comprises a shape selected from the group consisting of a polygonal shape, and a circular shape.

### Claim 5 (depends on 1)

The interface assembly of claim 1 further comprising a first metal redistribution layer electrically connected to said bonding and test pads, and being co-planar with one another.

### Claim 6 (depends on 5)

The interface assembly of claim 5 wherein said first metal redistribution layer is electrically connected by way of a via to a second redistribution layer being disposed in a different plane than the first redistribution layer.

### Claim 7 (depends on 1)

The interface assembly of claim 1 wherein the region to be bumped is defined by a first opening in a passivation layer.

### Claim 8 (depends on 7)

The interface assembly of claim 7 wherein the probe region is defined by a second opening in said passivation layer, said first and second openings being spaced apart from one another.

### Claim 9

A method for testing a semiconductor wafer prior to performing a flip chip bumping process, said method comprising:
providing a flip chip bonding pad having a region for performing said bumping process;
integrally constructing a test pad with said bonding pad; and
disposing said test pad coplanar with said flip chip bonding pad, said test pad including a probe region for performing a wafer test prior to performing said bumping process.