# US 2006/0065934 A1 · Semiconductor device and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0065934 A1
- Document ID: US20060065934A1
- Status: Published application
- Kind: A1
- Application number: 10/998,193
- Filed: 2004-11-29
- Published: 2006-03-30
- Earliest claimed: 2004-09-29
- Assignees: Kabushiki Kaisha Toshiba
- Inventors: Yasunori Okayama; Kiyotaka Miyano; Kazunari Ishimaru
- Web page: https://patentgrep.com/patent/US20060065934A1

## CPC

- H10D 64/511: {for IGFETs}
- H10D 84/0174: {the gate conductors being silicided}
- H10D 84/0177: {the gate conductors having different materials or different implants}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 30/0212: {using self-aligned silicidation}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A semiconductor device suitable for the miniaturization and comprising properly controlled Si/SiGe gate electrode comprises an insulator formed on a semiconductor substrate, a first gate electrode formed on the insulator and including silicon-germanium, wherein a germanium concentration is higher near an interface to the insulator and lower in a surface side opposite to the insulator, and a second gate electrode formed on the insulator and including silicon-germanium, wherein a germanium concentration is substantially uniform and an n-type dopant of a concentration of above 6×1020 atoms/cm3 is contained.

## Claims

### Claim 1

A semiconductor device comprising:
an insulator formed on a semiconductor substrate;
a first gate electrode formed on the insulator and including silicon-germanium, wherein a germanium concentration is higher near an interface to the insulator and lower in a surface side opposite to the insulator; and
a second gate electrode formed on the insulator and including silicon-germanium, wherein a germanium concentration is substantially uniform and an n-type dopant of a concentration of above 6×1020 atoms/cm3 is contained.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1,
wherein the first gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is above 15% but below 50%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the first gate electrode is above 10%,
and wherein the second gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is below 10%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the second gate electrode is below 5%.

### Claim 3 (depends on 1)

The semiconductor device according to claim 1, wherein a crystal grain size in the second gate electrode is greater than that in the first gate electrode.

### Claim 4 (depends on 1)

The semiconductor device according to claim 1, wherein a width of the first gate electrode in a channel direction at the interface to the insulator is narrower than that at the surface side and a difference between the width at the interface to the insulator and at the surface side in the first gate electrode is greater than that in the second gate electrode.

### Claim 5

A semiconductor device comprising:
an insulator formed on a semiconductor substrate;
a first gate electrode formed on a semiconductor substrate and including silicon-germanium, wherein a germanium concentration is higher near an interface to the insulator and lower in a surface side opposite to the insulator, and at least one of carbon, nitrogen or oxygen of a concentration of above 1×1015 atoms/cm2 but below 1×1016 atoms/cm2 is contained; and
a second gate electrode formed on the insulator and including silicon-germanium, wherein a germanium concentration is substantially uniform and an n-type dopant of a concentration of above 6×1020 atoms/cm3 is contained.

### Claim 6 (depends on 5)

The semiconductor device according to claim 5, wherein the second gate electrode is crystallized after being made into amorphous by implantation.

### Claim 7 (depends on 5)

The semiconductor device according to claim 5,
wherein the first gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is above 15% but below 50%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the first gate electrode is above 10%,
and wherein the second gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is below 10%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the second gate electrode is below 5%.

### Claim 8 (depends on 5)

The semiconductor device according to claim 5, wherein a crystal grain size in the second gate electrode is greater than that in the first gate electrode.

### Claim 9 (depends on 5)

The semiconductor device according to claim 5, wherein a width of the first gate electrode in a channel direction at the interface to the insulator is narrower than that at the surface side and a difference between the width at the interface to the insulator and at the surface side in the first gate electrode is greater than that in the second gate electrode.

### Claim 10

A method for manufacturing a semiconductor device comprising:
forming an insulator on a semiconductor substrate;
forming a first silicon film on the insulator;
forming a semiconductor film containing silicon and germanium on the first silicon film;
forming a second silicon film on the semiconductor film;
introducing an n-type dopant of a concentration of above 6×1020 atoms/cm3 into at least the second silicon film in a second gate electrode forming area;
forming first and second gate electrodes by processing the first silicon film, semiconductor film and second silicon film; and
heat treating the semiconductor substrate with the first and second gate electrodes formed thereon to allow the germanium in the first and second gate electrodes to be redistributed within each gate electrode to a distribution different each other.

### Claim 11 (depends on 10)

The method for manufacturing a semiconductor device according to claim 10,
wherein the first gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is above 15% but below 50%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the first gate electrode is above 10%,
and wherein the second gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is below 10%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the second gate electrode is below 5%.

### Claim 12 (depends on 10)

The method for manufacturing a semiconductor device according to claim 10, wherein a thickness of the second silicon film is three times or more thicker than that of the semiconductor film.

### Claim 13 (depends on 12)

The method for manufacturing a semiconductor device according to claim 12,
wherein the first gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is above 15% but below 50%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the first gate electrode is above 10%,
and wherein the second gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is below 10%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the second gate electrode is below 5%.

### Claim 14 (depends on 12)

The method for manufacturing a semiconductor device according to claim 12, further comprising:
introducing at least one of carbon, nitrogen or oxygen of a concentration of above 1×1015 atoms/cm2 but below 1×1016 atoms/cm2 into at least the second silicon film in the first gate electrode forming area.

### Claim 15 (depends on 10)

The method for manufacturing a semiconductor device according to claim 10, further comprising:
introducing at least one of carbon, nitrogen or oxygen of a concentration of above 1×1015 atoms/cm2 but below 1×1016 atoms/cm2 into at least the second silicon film in the first gate electrode forming area.

### Claim 16 (depends on 15)

The method for manufacturing a semiconductor device according to claim 15,
wherein the first gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is above 15% but below 50%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the first gate electrode is above 10%,
and wherein the second gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is below 10%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the second gate electrode is below 5%.

### Claim 17 (depends on 10)

The method for manufacturing a semiconductor device according to claim 10, further comprising:
implanting ions into at least the second silicon film in the second gate electrode forming area to make the second silicon film into amorphous.

### Claim 18

A method for manufacturing a semiconductor device comprising:
forming an insulator on a semiconductor substrate;
forming a first silicon film on the insulator;
forming a semiconductor film containing silicon and germanium on the first silicon film;
forming a second silicon film on the semiconductor film;
introducing an n-type dopant of a concentration of above 6×1020 atoms/cm3 into at least the second silicon film in a second gate electrode forming area;
heat treating the semiconductor substrate to allow the germanium in the first and second gate electrodes to be redistributed within each gate electrode to a distribution different each other;
forming first and second electrodes by processing the first silicon film, semiconductor film and second silicon film; and
laterally etching the first gate electrode to make a width in a channel direction near an interface of the gate electrode to the insulator narrower than that at a surface side thereof.

### Claim 19 (depends on 18)

The method for manufacturing a semiconductor device according to claim 18,
wherein the first gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is above 15% but below 50%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the first gate electrode is above 10%,
and wherein the second gate electrode including the silicon-germanium has a germanium atomic concentration near the interface to the insulator is below 10%, a germanium atomic concentration in the surface side is below 5%, and a germanium concentration variation in the second gate electrode is below 5%.

### Claim 20 (depends on 18)

The method for manufacturing a semiconductor device according to claim 18, wherein a thickness of the second silicon film is three times or more thicker than that of the semiconductor film.