# US 2006/0065829 A1 · Method for electron beam-initiated coating for application of transmission electron microscopy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0065829 A1
- Document ID: US20060065829A1
- Status: Published application
- Kind: A1
- Application number: 10/711,644
- Filed: 2004-09-29
- Published: 2006-03-30
- Earliest claimed: 2004-09-29
- Assignees: International Business Machines Corporation
- Inventors: Wei Lu
- Web page: https://patentgrep.com/patent/US20060065829A1

## CPC

- G01N 1/32: Polishing; Etching
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A method for preparing a specimen for application of microanalysis thereto includes forming an initial conductive layer over a defined area of interest on a semiconductor substrate, the initial conductive layer formed through an electron beam deposition process. A volume of substrate material surrounding the area of interest is removed, thereby forming the specimen, including said area of interest and said initial conductive layer over the area of interest. The specimen is then removed from the bulk substrate material.

## Claims

### Claim 1

A method for preparing a specimen for application of microanalysis thereto, the method comprising:
forming an initial conductive layer over an area of interest, said initial conductive layer formed through a low-energy beam deposition process;
removing a volume of material surrounding said area of interest by forming a pair of trenches in a bulk material having said area of interest formed thereon, thereby forming a membrane including said area of interest and said initial conductive layer over said area of interest; and
removing said membrane from said bulk material.

### Claim 2 (depends on 1)

The method of claim 1, wherein said low-energy beam deposition process comprises electron beam deposition.

### Claim 3 (depends on 2)

The method of claim 2, wherein said initial conductive layer further comprises at least one of: platinum, tungsten, gold, aluminum, titanium, and combinations thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein said initial conductive layer is formed at a thickness of about 10 nanometers (nm) to about 100 nm.

### Claim 5 (depends on 4)

The method of claim 4, wherein said initial conductive layer is formed over an area of about 1 micron by about 10 microns.

### Claim 6 (depends on 4)

The method of claim 4, further comprising implementing a high-energy beam deposition process for increasing the thickness of said initial conductive layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein said high-energy beam deposition process comprises ion beam deposition.

### Claim 8 (depends on 1)

The method of claim 1, wherein said removing a volume of material surrounding said area of interest is implemented by focused ion beam milling.

### Claim 9

A method for preparing a specimen for application of microanalysis thereto, the method comprising:
forming an initial conductive layer over a defined area of interest on a semiconductor substrate, said initial conductive layer formed through an electron beam deposition process;
removing a volume of substrate material surrounding said area of interest, thereby forming the specimen, including said area of interest and said initial conductive layer over said area of interest; and
removing the specimen from said bulk substrate material.

### Claim 10 (depends on 9)

The method of claim 9, wherein the microanalysis comprises tunneling electron microscopy (TEM).

### Claim 11 (depends on 10)

The method of claim 10, wherein said initial conductive layer further comprises at least one of: platinum, tungsten, gold, aluminum, titanium, and combinations thereof.

### Claim 12 (depends on 9)

The method of claim 9, wherein said initial conductive layer is formed at a thickness of about 10 nanometers (nm) to about 100 nm.

### Claim 13 (depends on 12)

The method of claim 12, wherein said initial conductive layer is formed over an area of about 1 micron by about 10 microns.

### Claim 14 (depends on 12)

The method of claim 12, further comprising implementing a high-energy beam deposition process for increasing the thickness of said initial conductive layer.

### Claim 15 (depends on 14)

The method of claim 14, wherein said high-energy beam deposition process comprises ion beam deposition.

### Claim 16 (depends on 9)

The method of claim 9, wherein said removing a volume of substrate material surrounding said area of interest is implemented by focused ion beam milling.