# US 2006/0052533 A1 · Crosslinked polyvinyl acetals

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0052533 A1
- Document ID: US20060052533A1
- Status: Published application
- Kind: A1
- Application number: 10/542,019
- Filed: 2003-12-12
- Published: 2006-03-09
- Earliest claimed: 2003-01-09
- Assignees: Kuraray Europe GmbH
- Inventors: Bernd Papenfuhs; Martin Steuer; Matthias Gutweiler
- Web page: https://patentgrep.com/patent/US20060052533A1

## CPC

- C08F 8/28: Condensation with aldehydes or ketones
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The invention relates to methods for producing crosslinked polyvinyl acetals, according to which a polyvinyl alcohol (A1) containing carboxyl groups is crosslinked by (i) reacting the polymer (A1) with at least one polyaldehyde of formula R9(CHO)n, and (ii) at least partly esterifying groups of formula (1) and formula (4a) with each other, said steps being performed in any order. The invention further relates to methods for producing crosslinked polyvinyl acetals, according to which a polyvinyl alcohol (A2) is crosslinked by (i) reacting the polymer (A2) with at least one compound of formula (6), (ii) adding at least one compound of formula (4b), (iii) adding a polyaldehyde of formula (5), and (iv) at least partly esterifying groups of formula (1) and structural units derived from the compound of formula (4b) with each other, the radicals R7, R8, R9, R10, and R11, and the index n being defined as indicated in the description. Also disclosed are the crosslinked polyvinyl acetals obtained by means of the inventive method and particularly appropriate areas of application of said polymers.

## Claims

### Claim 1

A method for the manufacture of cross-linked polyvinylacetals, in which a polymer (A1) which contains in relation to its total weight
(a) 1.0 to 99.9 wt % structural units of formula (I)
where R1 represents hydrogen or methyl
(b) 0 to 99.0 wt % structural units of formula (2)
wherein R2 represents hydrogen or an alkyl group with 1 to 6 carbon atoms,
(c) 0 to 70.0 wt % of structural units of formula (3)
wherein R3, R4, R5 and R6, are in each case groups independent of each other with a molecular weight in the range from 1 to 500 g/mol,
(d) 0.00001 to 30.0 wt % structural units of formula (4a)
wherein R7 is a linkage, an alkylene group with 1 to 10 carbon atoms or an if necessary substituted arylene group with 6 to 12 carbon atoms and R8 is hydrogen, COOH, an alkyl group with 1 to 10 carbon atoms or an if necessary substituted aryl group with 6 to 12 carbon atoms, wherein one in any sequence,
(i) reacts polymer (A1) with at least one polyaldehyde of formula (5),
R9(CHO)n (5)
wherein R9 represents a linkage or a group having 1 to 40 carbon atoms and n is a whole number greater than 2
and
(ii) groups of formula (1) and formula (4a) at least partially esterified with each other,

### Claim 2 (depends on 1)

The method according to claim 1, characterized in that at any point in time at least one compound of formula (6) is added,
wherein R10 and R11, are hydrogen, an alkyl group with 1 to 10 carbon atoms or an if necessary substituted aryl group with 6 to 12 carbon atoms, in each case independent of each other.

### Claim 3 (depends on 1)

The method according to claim 1, characterized in that a polymer (A1) with R8=hydrogen is employed.

### Claim 4 (depends on 1)

The method according to claim 1, characterized in that a polymer (A1) is employed, in which R7 is a linkage or an alkylene group with 1 to 4 carbon atoms.

### Claim 5

A method for the manufacture of cross-linked polyvinylacetals, in which a polymer (A2) is cross-linked, which in relation to its total weight contains
(a) 1.0 to 99.9 wt % structural units of formula (1)
wherein R1 represents hydrogen or methyl
(b) 0 to 99.0 wt % structural units of formula (2)
wherein R2 represents hydrogen or an alkyl group with 1 to 6 carbon atoms,
(c) 0 to 70.0 wt % of structural units of formula (3)
wherein R3, R4, R5 and R6, are in each case groups independent of each other with a molecular weight in the range from 1 to 500 g/mol,
characterized in that
(i) the polymer (A2) reacts with at least one compound of formula (6)
wherein R10 and R11, in each case independent of each other, are hydrogen, an alkyl group with 1 to 10 carbon atoms or an if necessary substituted aryl group with 6 to 12 carbon atoms.
(ii) at least one compound of formula (4b) is added
wherein R7 is a linkage, an alkylene group with 1 to 10 carbon atoms or an if necessary substituted arylene group with 6 to 12 carbon atoms and R8 is hydrogen, COOH, an alkyl group with 1 to 10 carbon atoms or an if necessary substituted aryl group with 6 to 12 carbon atoms,
(iii) a polyaldehyde added of formula (5),
R9(CHO)n (5)
wherein R9 is a linkage or a group having 1 to 40 carbon atoms and n is a whole 0n0umber greater than 2
and
(iv) groups of formula (1) and derived from structural units of formula (4b) at least partially esterified with each other.

### Claim 6 (depends on 5)

The method according to claim 5, characterized in that at least one compound of formula (4b) with R8=hydrogen is employed.

### Claim 7 (depends on 5)

The method according to claim 5, characterized in that at least one compound of formula (4b) is employed, in which R7 is a linkage or an alkylene group with 1 to 4 carbon atoms.

### Claim 8 (depends on 1)

The method according to claim 1 characterized in that a compound (5) with n=2 or 3 is employed.

### Claim 9 (depends on 1)

The method according to claim 1 characterized in that a compound (5) is employed in which R9 is an aliphatic, cycloaliphatic and/or aromatic group with 1 to 12 carbon atoms.

### Claim 10 (depends on 9)

The method according to claim 9, characterized in that glutardialdehyde and/or n-nonanedial is utilized as compound (5).

### Claim 11 (depends on 1)

The method according to claim 1, characterized in that n-butyraldehyde is employed as compound (6).

### Claim 12 (depends on 1)

The method according to claim 1, characterized in that
(1) 95.00 to 99.99 parts by weight at least of one compound (6)
(2) 0.01 to 5.00 parts by weight at least of a polyaldehyde (5) is added, wherein the parts by weight given is made up to 100.00 parts by weight.

### Claim 13 (depends on 1)

The method according to claim 1, characterized in that, the esterification (ii) or (iv), is if necessary carried out in presence of at least one softener, at bulk temperatures in the range from 80 to 280° C.

### Claim 14 (depends on 13)

The method according to claim 13, characterized in that the cross-linking is carried out in an extruder, kneading device or another heatable unit.

### Claim 15 (depends on 1)

The cross-linked polyvinylacetal obtainable by means of a method in accordance with claim 1.

### Claim 16 (depends on 15)

The polyvinylacetal in accordance with claim 15, characterized in that less than 10.0 wt % of its total content is esterified and non-esterified in relation to the total weight of polyvinylacetal.

### Claim 17 (depends on 15)

The polyvinylacetal in accordance with claim 15, characterized in that it contains softeners.

### Claim 18 (depends on 15)

Molding material containing a polyvinylacetal in accordance with claim 15.

### Claim 19 (depends on 15)

Film containing a polyvinylacetal in accordance with claim 15.

### Claim 20 (depends on 19)

The use of a film in accordance with claim 19 for the manufacture of laminated safety glasses.

### Claim 21 (depends on 15)

A coating containing a polyvinylacetal in accordance with claim 15.

### Claim 22 (depends on 15)

The use of a polyvinylacetal in accordance with claim 15 for the manufacture of ionically conductive intermediate layers for electrochromic systems.