# US 2006/0052531 A1 · Modified polymer particle, packing material and column for chromatography

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0052531 A1
- Document ID: US20060052531A1
- Status: Published application
- Kind: A1
- Application number: 10/527,096
- Filed: 2003-09-11
- Published: 2006-03-09
- Earliest claimed: 2002-09-17
- Assignees: Showa Denko K.K.
- Inventors: Takashi Kotsuka; Kuniaki Shimbo
- Web page: https://patentgrep.com/patent/US20060052531A1

## CPC

- C08G 63/91: Polymers modified by chemical after-treatment
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

An object of the present invention is to prevent an isolation of carboxyl group caused by hydrolysis of ester bond, which occurs when a polymer particle containing an ester bond is used in the presence of a strongly acidic or strongly alkaline solution to thereby improve the acid Ealkali durability of the polymer particle. When a polymer particle containing an ester bond is treated with an acid or alkali hydrous solution and thereby an ester bond which is located and exposed on the surface of the particle and is readily hydrolyzed is previously hydrolyzed to isolate a carboxyl group and then the free carboxyl group is capped by amidation, to thereby dissolve the above problem.

## Claims

### Claim 1

A modified polymer particle improved in the acid.alkali durability, obtained by treating a polymer particle containing an ester bond with an acid or alkali hydrous solution to partially hydrolyze the ester bond and isolate a carboxyl group and capping the free carboxyl group through amidation.

### Claim 2 (depends on 1)

The modified polymer particle improved in the acid.alkali durability as claimed in claim 1, wherein the ester bond having been hydrolyzed is an ester bond readily coming into contact with liquid.

### Claim 3 (depends on 1)

The modified polymer particle improved in the acid.alkali durability as claimed in claim 1, wherein the amine used for the amidation is an amine represented by formula (1):
NHR1R2 (1)
(wherein R1 and R2 each independently represents a hydrogen atom, an alkyl group having a carbon number of 18 or less, which may be branched or may be substituted by a halogen, or a phenyl group).

### Claim 4 (depends on 3)

The modified polymer particle improved in the acid.alkali durability as claimed in claim 3, wherein the amine used for the amidation is an amine represented by formula (2):
NH2R3 (2)
(wherein R3 represents a hydrogen atom, an alkyl group having a carbon number of 18 or less, which may be branched or may be substituted by a halogen, or a phenyl group).

### Claim 5

A modified polymer particle improved in the acid.alkali durability, wherein when the polymer particle is packed in a column having an inner diameter of 4.6 mm and a length of 150 mm and the alkali durability is evaluated using the column by the following method, the increase percentage of the pyridine retentivity after passing an alkali eluent is 50% or less:
Evaluation Method:
(1) an eluent of acetonitrile/aqueous 0.1% phosphoric acid solution=30/70 is passed at a flow rate of 0.3 ml/min for 30 minutes, the column temperature is set to 40° C., and the pyridine retentivity is measured by using an eluent of acetonitrile/water=30/70 at a flow rate of 0.5 ml/min,
(2) an alkali eluent of acetonitrile/aqueous 0.01 mol sodium hydroxide solution=50/50 is passed through the same column at a flow rate of 0.5 ml/min for 4 hours at a column temperature of 40° C., then an eluent of acetonitrile/aqueous 0.1% phosphoric acid solution=30/70 is passed at a flow rate of 0.3 ml/min for 30 minutes, the column temperature is set to 40° C., and the pyridine retentivity is measured by using an eluent of acetonitrile/water=30/70 at a flow rate of 0.5 ml/min, and
(3) the pyridine retentivity of (2) is compared with the pyridine retentivity of (1).

### Claim 6 (depends on 1, 2, 3, 4, 5)

The modified polymer particle improved in the acid-alkali durability as claimed in any one of claims 1 to 5, wherein the average particle size of the polymer particle is from 1 to 50 μm.

### Claim 7

A polymer-base packing material for chromatography, using a modified polymer particle improved in the acid.alkali durability, the polymer particle being obtained by treating a polymer particle containing an ester bond with an acid or alkali hydrous solution to partially hydrolyze the ester bond and isolate a carboxyl group and then capping the free carboxyl group through amidation.

### Claim 8 (depends on 7)

The polymer-base packing material for chromatography as claimed in claim 7, wherein the ester bond having been hydrolyzed is an ester bond readily coming into contact with liquid.

### Claim 9 (depends on 7)

The polymer-base packing material for chromatography as claimed in claim 7, wherein the amine used for the amidation is an amine represented by formula (1):
NHR1R2 (1)
(wherein R1 and R each independently represents a hydrogen atom, an alkyl group having a carbon number of 18 or less, which may be branched or may be substituted by a halogen, or a phenyl group).

### Claim 10 (depends on 9)

The polymer-base packing material for chromatography as claimed in claim 9, wherein the amine used for the amidation is an amine represented by formula (2):
NH2R3 (2)
(wherein R3 represents a hydrogen atom, an alkyl group having a carbon number of 18 or less, which may be branched or may be substituted by a halogen, or a phenyl group).

### Claim 11

A polymer-base packing material for chromatography, using a modified polymer particle improved in the acid-alkali durability such that when the polymer particle is packed in a column having an inner diameter of 4.6 mm and a length of 150 mm and the alkali durability is evaluated using the column by the following method, the increase percentage of the pyridine retentivity after passing an alkali eluent is 50% or less:
Evaluation Method:
(1) an eluent of acetonitrile/aqueous 0.1% phosphoric acid solution=30/70 is passed at a flow rate of 0.3 ml/min for 30 minutes, the column temperature is set to 40° C., and the pyridine retentivity is measured by using an eluent of acetonitrile/water=30/70 at a flow rate of 0.5 ml/min,
(2) an alkali eluent of acetonitrile/aqueous 0.01 mol sodium hydroxide solution=50/50 is passed through the same column at a flow rate of 0.5 ml/min for 4 hours at a column temperature of 40° C., then an eluent of acetonitrile/aqueous 0.1 % phosphoric acid solution=30/70 is passed at a flow rate of 0.3 ml/min for 30 minutes, the column temperature is set to 40° C., and the pyridine retentivity is measured by using an eluent of acetonitrile/water=30/70 at a flow rate of 0.5 ml/min, and
(3) the pyridine retentivity of (2) is compared with the pyridine retentivity of (1).

### Claim 12 (depends on 7, 8, 9, 10, 11)

The polymer-base packing material for chromatography as claimed in any one of claims 7 to 11, wherein the average particle size of the polymer particle is from 1 to 50 μm.

### Claim 13

A method for producing a modified polymer particle improved in the acid.alkali durability, comprising treating a polymer particle containing an ester bond with an acid or alkali hydrous solution to partially hydrolyze the ester bond and isolate a carboxyl group and then capping the free carboxyl group through amidation.

### Claim 14 (depends on 13)

The method for producing a modified polymer particle improved in the acid.alkali durability as claimed in claim 13, wherein the ester bond having been hydrolyzed is an ester bond readily coming into contact with liquid.

### Claim 15 (depends on 13)

The method for producing a modified polymer particle improved in the acid-alkali durability as claimed in claim 13, wherein the amine used for the amidation is an amine represented by formula (1):
NHR1R2 (1)
(wherein R1 and R2 each independently represents a hydrogen atom, an alkyl group having a carbon number of 18 or less, which may be branched or may be substituted by a halogen, or a phenyl group).

### Claim 16 (depends on 15)

The method for producing a modified polymer particle improved in the acid.alkali durability as claimed in claim 15, wherein the amine used for the amidation is an amine represented by formula (2):
NH2R3 (2)
(wherein R3 represents a hydrogen atom, an alkyl group having a carbon number of 18 or less, which may be branched or may be substituted by a halogen, or a phenyl group).

### Claim 17 (depends on 13, 14, 15, 16)

The method for producing a modified polymer particle improved in the acid-alkali durability as claimed in any one of claims 13 to 16, wherein when the polymer particle is packed in a column having an inner diameter of 4.6 mm and a length of 150 mm and the alkali durability is evaluated using the column by the following method, the increase percentage of the pyridine retentivity after passing an alkali eluent is 50% or less:
Evaluation Method:
(1) an eluent of acetonitrile/aqueous 0.1% phosphoric acid solution=30/70 is passed at a flow rate of 0.3 ml/min for 30 minutes, the column temperature is set to 40° C., and the pyridine retentivity is measured by using an eluent of acetonitrile/water=30/70 at a flow rate of 0.5 ml/min,
(2) an alkali eluent of acetonitrile/aqueous 0.01 mol sodium hydroxide solution=50/50 is passed through the same column at a flow rate of 0.5 ml/min for 4 hours at a column temperature of 40° C., then an eluent of acetonitrile/aqueous 0.1% phosphoric acid solution=30/70 is passed at a flow rate of 0.3 ml/min for 30 minutes, the column temperature is set to 40° C., and the pyridine retentivity is measured by using an eluent of acetonitrile/water=30/70 at a flow rate of 0.5 ml/min, and
(3) the pyridine retentivity of (2) is compared with the pyridine retentivity of (1).

### Claim 18 (depends on 13, 14, 15, 16)

The method for producing a modified polymer particle improved in the acid-alkali durability as claimed in any one of claims 13 to 16, wherein the average particle size of the polymer particle is from 1 to 50 μm.

### Claim 19 (depends on 6)

A method for producing a polymer-base packing material for chromatography, comprising producing the polymer-base packing material for chromatography described in claim 6 by performing one or both of the hydrolysis treatment with an acid or alkali hydrous solution and the capping treatment through amidation, in the state of the polymer-base packing material being packed in the column.

### Claim 20 (depends on 6)

A chromatography column using the polymer-base packing material for chromatography improved in the acid-alkali durability described in claim 6.