# US 2006/0051900 A1 · Method of manufacturing a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0051900 A1
- Document ID: US20060051900A1
- Status: Published application
- Kind: A1
- Application number: 11/153,824
- Filed: 2005-06-16
- Published: 2006-03-09
- Earliest claimed: 2004-09-09
- Assignees: Oki Electric Industry Co., Ltd.
- Inventors: Yoshinori Shizuno
- Web page: https://patentgrep.com/patent/US20060051900A1

## CPC

- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/019: {of bond pads}
- H10W 74/129: {forming a chip-scale package [CSP]}
- H10W 70/656: Fan-in layouts
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/07251: {characterised by changes in properties of the bump connectors during connecting}
- H10W 72/221: {Structures or relative sizes}
- H10W 72/222: {Multilayered bumps, e.g. a coating on top and side surfaces of a bump core}
- H10W 72/223: {characterised by the structure of the outermost layers, e.g. multilayered coatings}
- H10W 72/242: {relative to the surface, e.g. recessed, protruding}
- H10W 72/244: {relative to underlying supporting features, e.g. bond pads, RDLs or vias}
- H10W 72/247: {Dispositions of multiple bumps}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/255: {of outermost layers of multilayered bumps, e.g. material of a coating}
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/934: {Cross-sectional shape, i.e. in side view}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a semiconductor device has: preparing a semiconductor wafer having electrode pads formed on the main surface; forming contact portions, which connect to the electrode pads, on the main surface; forming a sealing resin over the main surface; grinding the top face of the sealing resin for exposing the top faces of the contact portions; polishing the top face of the sealing resin by blast processing for exposing the side of the contact portions; and forming external terminals connected with the contact portions exposing from the sealing resin.

## Claims

### Claim 1

A method of manufacturing a semiconductor device comprising:
preparing a semiconductor wafer having electrode pads formed on a main surface;
forming contact portions connecting to said electrode pads on said main surface;
forming a sealing resin over said main surface;
grinding a top face of said sealing resin to expose top faces of said contact portions;
polishing said top face of said sealing resin by blast processing to expose a side of said contact portions; and
forming external terminals being connected to said contact portions exposed from said sealing resin.

### Claim 2 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein
a liquid honing method is used for the blast processing.

### Claim 3 (depends on 2)

The method of manufacturing a semiconductor device according to claim 2, wherein
said liquid honing method includes ejecting a liquid mixture of abrasive grains and water from a nozzle together with compressed air, said abrasive grains include polygonal particles of alumina.

### Claim 4 (depends on 3)

The method of manufacturing a semiconductor device according to claim 3, wherein ejecting a liquid mixture of abrasive grains and water is performed twice with an air pressure of 0.25 MPa at a processing speed of 10 mm/sec.

### Claim 5 (depends on 2)

The method of manufacturing a semiconductor device according to claim 2, wherein
polygon particles of alumina (Al2O3) are used as abrasive grains in said liquid honing process.

### Claim 6 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein
said external terminals are spherical electrodes whose material includes solders.

### Claim 7 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, further comprising,
forming conductive layers on said contact portions after exposing said top faces of said contact portions.

### Claim 8 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7, further comprising:
a liquid honing method is used for said blast processing.

### Claim 9 (depends on 8)

The method of manufacturing a semiconductor device according to claim 8, wherein
polygon particles of alumina (Al2O3) are used as abrasive grains in the liquid honing process.

### Claim 10 (depends on 8)

The method of manufacturing a semiconductor device according to claim 8, wherein
said liquid honing method includes ejecting a liquid mixture of abrasive grains and water from a nozzle together with compressed air, said abrasive grains include polygonal particles of alumina.

### Claim 11 (depends on 10)

The method of manufacturing a semiconductor device according to claim 10, wherein ejecting a liquid mixture of abrasive grains and water is performed twice with an air pressure of 0.25 MPa at a processing speed of 10 mm/sec.

### Claim 12 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7, wherein
said conductive layers includes nickel.

### Claim 13 (depends on 12)

The method of manufacturing a semiconductor device according to claim 12, wherein
the external terminals are spherical electrodes of which material includes solders.

### Claim 14 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein
a difference between a height of said top surface of said sealing resin and said top faces of said contact portions is 10 μm.

### Claim 15 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein
a height of said contact portion is between 80 to 90 μm with a diameter of 250 μm.

### Claim 16 (depends on 15)

The method of manufacturing a semiconductor device according to claim 15, wherein
a difference between a height of said top surface of said sealing resin and said top faces of said contact portions is 10 μm.

### Claim 17 (depends on 16)

The method of manufacturing a semiconductor device according to claim 16, further comprising,
forming conductive layers on said contact portions after exposing said top faces of said contact portions.

### Claim 18 (depends on 17)

The method of manufacturing a semiconductor device according to claim 17, wherein
said conductive layers includes nickel.

### Claim 19 (depends on 18)

The method of manufacturing a semiconductor device according to claim 18, wherein
a thickness of said conductive layers is 3 μm.