# US 2006/0051696 A1 · Toner for developing electrostatic latent image and image-forming method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0051696 A1
- Document ID: US20060051696A1
- Status: Published application
- Kind: A1
- Application number: 11/247,231
- Filed: 2005-10-12
- Published: 2006-03-09
- Earliest claimed: 2002-11-15
- Assignees: Konica Minolta Business Technologies, Inc.
- Inventors: Chikara Tsutsui; Masahiro Anno; Masahide Inoue; Katsunori Kurose
- Web page: https://patentgrep.com/patent/US20060051696A1

## CPC

- G03G 9/0827: {characterised by their shape, e.g. degree of sphericity}
- G03G 9/0819: {characterised by the dimensions of the particles}
- G03G 9/0821: {characterised by physical parameters (magnetic parameters G03G9/083)}
- G03G 9/08782: {Waxes}
- G03G 9/08795: {characterised by their chemical properties, e.g. acidity, molecular weight, sensitivity to reactants}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- G03G 9/09791: {Metallic soaps of higher carboxylic acids}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

A toner for developing electrostatic latent images, having a specified volume-average particle size, an average degree of roundness, a standard deviation of the degree of roundness and surface properties D/d50 wherein a specified amount of fatty acid metal salt that has a specified volume-average particle size is externally added, and an image-forming method using such a toner.

## Claims

### Claim 1

An image-forming method comprising:
developing an electrostatic latent image formed on a surface of an electrostatic latent image supporting member with a toner to form an image;
transferring the image to a transferring member; and
cleaning the residual toner on the electrostatic latent image supporting member by using a cleaning blade, wherein the cleaning blade is placed with a press-contact angle of 10 to 20° and a press-contact force of 20 to 50 N/m with respect to the electrostatic latent image supporting member,
wherein the toner has a volume-average particle size of 3 to 7 μm, an average degree of roundness of 0.960 to 0.995, a standard deviation of the degree of roundness of not more than 0.04, and surface properties D/d50 that satisfies the following conditional expression, and 0.005 to 0.015% by weight of fatty acid metal salt that has a volume-average particle size of 1.5 to 12 μm and is externally added;
D/d50≧0.40 in which D=6/(ρ·S), (ρ is a true density (g/cm3)) of toner particles, S is a BET specific surface area ((m2/g) of toner particles), and d50 represents a weight-average particle size (μm) of the toner particles.

### Claim 2 (depends on 1)

The method of claim 1, wherein the fatty-acid metal salt is calcium stearate.

### Claim 3 (depends on 1)

The method of claim 1, wherein an amount of the toner that is transported by a toner-supporting member is regulated by a regulating member that is placed in contact with the surface of the toner-supporting member and the regulated toner is transported to a developing area to develop electrostatic latent images.

### Claim 4 (depends on 1)

The method of claim 1, wherein the toner comprises a binder resin having: a glass transition temperature of 50 to 75° C., a softening point of 80 to 160° C., a number-average molecular weight of 1,000 to 30,000 and a ratio of weight-average molecular weight/number-average molecular weight of 2 to 100.

### Claim 5 (depends on 1)

The method of claim 1, wherein the toner comprises a binder resin having: a glass transition temperature of 50 to 75° C., a softening point of 80 to 120° C., a number-average molecular weight of 2,500 to 30,000 and a ratio of weight-average molecular weight/number-average molecular weight of 2 to 20.

### Claim 6 (depends on 1)

The method of claim 1, wherein the toner is prepared by a wet method and subjected to a heat treatment to have a globular shape.

### Claim 7 (depends on 6)

The method of claim 6, wherein the heat treatment is an instantaneous heat treatment by applying heat to toner particles in hot air flow.

### Claim 8 (depends on 6)

The method of claim 6, wherein the toner is a non-magnetic toner.

### Claim 9 (depends on 1)

The method of claim 1, wherein the fatty-acid metal salt has a volume-average-particle size of 2 to 10 μm.

### Claim 10 (depends on 1)

The method of claim 1, wherein the fatty-acid metal salt has a melting point of 100 to 150° C.

### Claim 11 (depends on 1)

The method of claim 1, wherein the average degree of roundness is 0.970 to 0.990.

### Claim 12 (depends on 11)

The method of claim 11, wherein the standard deviation of the degree of roundness is 0.01 to 0.035.

### Claim 13 (depends on 12)

The method of claim 12, wherein the surface properties satisfy the following conditions: 0.7≧D/d50≧0.45.

### Claim 14 (depends on 1)

The method of claim 1, wherein the standard deviation of the degree of roundness is 0.01 to 0.035

### Claim 15 (depends on 1)

The method of claim 1, wherein the surface properties satisfy the following conditions:
0.6≧D/d5≧0.40.

### Claim 16 (depends on 1)

The method of claim 1, comprising a first binder resin and a second binder resin having a different softening point from the first binder resin.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first binder resin has a softening point of 80 to 125° and the second resin has a softening point of 125 to 160° C.

### Claim 18 (depends on 8)

The method of claim 8, wherein the fatty-acid metal salt has a volume-average-particle size of 2 to 10 μm, the average degree of roundness if 0.970 to 0.990, the standard deviation of the degree of roundness is 0.01 to 0.035 and the surface properties satisfy the following conditions: 0.7≧D/d50≧0.45.