# US 2006/0051542 A1 · Polyester polymer and copolymer compositions containing metallic molybdenum particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0051542 A1
- Document ID: US20060051542A1
- Status: Published application
- Kind: A1
- Application number: 10/996,944
- Filed: 2004-11-24
- Published: 2006-03-09
- Earliest claimed: 2004-09-03
- Inventors: Zhiyong Xia; Donna Quillen
- Web page: https://patentgrep.com/patent/US20060051542A1

## CPC

- C08K 3/08: Metals
- Y10T 428/1352: Polymer or resin containing [i.e., natural or synthetic]
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Polyester compositions are disclosed that include polyester polymers or copolymers having incorporated therein metallic molybdenum particles that improve the reheat properties of the compositions. Processes for making such compositions are also disclosed. The molybdenum particles may be incorporated in the polyester by melt compounding, or may be added at any stage of the polymerization, such as during the melt-phase of the polymerization. A range of particle sizes may be used, as well as a range of particle size distributions. The polyester compositions are suitable for use in packaging made from processes in which a reheat step is desirable.

## Claims

### Claim 1

A polyester composition having improved reheat, comprising:
a polyester polymer; and
metallic molybdenum particles, having a median particle size from about 0.005 μm to about 10 μm, dispersed in the polyester polymer.

### Claim 2

A polyester composition having improved reheat, comprising:
a polyester polymer; and
metallic molybdenum particles, having a median particle size from about 0.05 μm to about 5 μm, dispersed in the polyester polymer.

### Claim 3

A polyester composition having improved reheat, comprising:
a polyester polymer; and
metallic molybdenum particles, having a median particle size from about 0.05 μm to about 2 μm, dispersed in the polyester polymer.

### Claim 4 (depends on 1)

The polyester composition of claim 1, wherein the metallic molybdenum particles are present in an amount from about 0.5 ppm to about 500 ppm, with respect to the total weight of the polyester composition.

### Claim 5 (depends on 1)

The polyester composition of claim 1, wherein the metallic molybdenum particles are present in an amount of from 1 ppm to 100 ppm, with respect to the total weight of the polyester composition.

### Claim 6 (depends on 1)

The polyester composition of claim 1, wherein the metallic molybdenum particles are present in an amount of from 5 ppm to 50 ppm with respect to the weight of the polyester composition.

### Claim 7 (depends on 1)

The polyester composition of claim 1, wherein the polyester polymer comprises polyethylene terephthalate.

### Claim 8 (depends on 1)

The polyester composition of claim 1, wherein the polyester composition is in the form of a beverage bottle preform.

### Claim 9 (depends on 1)

The polyester composition of claim 1, wherein the polyester composition is in the form of a beverage bottle.

### Claim 10 (depends on 1)

The polyester of claim 1, wherein the polyester composition is in the form of a molded article.

### Claim 11 (depends on 1)

The polyester composition of claim 1, wherein the polyester polymer comprises a continuous phase, and wherein the metallic molybdenum particles are dispersed within the continuous phase.

### Claim 12 (depends on 1)

The polyester composition of claim 1, wherein the metallic molybdenum particles have a median particle size from 0.08 μm to 1.1 μm, and provide the polyester composition with a reheat rate index of at least 1.05 while maintaining the polyester composition at an L* brightness of 70 or more at a reheat rate index of 1.05.

### Claim 13 (depends on 1)

The polyester composition of claim 1, wherein the metallic molybdenum particles comprise molybdenum-coated particles.

### Claim 14 (depends on 1)

The polyester composition of claim 1, wherein the metallic molybdenum particles comprise hollow spheres comprised of molybdenum.

### Claim 15 (depends on 1)

The polyester composition of claim 1, wherein the metallic molybdenum particles comprise a molybdenum alloy, wherein molybdenum is present in an amount of at least 30 wt. %, with respect to the total weight of the molybdenum alloy.

### Claim 16 (depends on 1)

The polyester composition of claim 1, wherein the metallic molybdenum particles comprise a molybdenum alloy, wherein molybdenum is present in an amount of at least 60 wt. %, with respect to the total weight of the molybdenum alloy.

### Claim 17 (depends on 1)

The polyester composition of claim 1, wherein the metallic molybdenum particles comprise a molybdenum alloy that includes molybdenum and one or more of: germanium, iron, chromium, tungsten, titanium, vanadium, carbon, or tantalum.

### Claim 18 (depends on 17)

The polyester composition of claim 17, wherein the alloy further comprises, in an amount of no more than about 10 wt. %, one or more of: gold, silver, copper, aluminum, manganese, or silicon.

### Claim 19 (depends on 1)

The polyester composition of claim 1, wherein the metallic molybdenum particles have a particle size distribution in which the span (S) is from 0 to about 10.

### Claim 20 (depends on 1)

The polyester composition of claim 1, wherein the metallic molybdenum particles have a particle size distribution in which the span (S) is from 0.01 to 2.

### Claim 21

A polyester composition having improved reheat, comprising:
a polyester polymer in which poly(ethylene terephthalate) residues comprise at least 90 wt. % of the polyester polymer; and
metallic molybdenum particles, having a median particle size from about 0.05 μm to about 2 μm, randomly dispersed in the polyester polymer in an amount from about 5 to about 50 ppm, wherein the polyester composition has a reheat index of 1.05 or more and an L* brightness level of 70 or more at the reheat rate index of 1.05.

### Claim 22

A process for producing a polyester composition, comprising:
an esterification step comprising transesterifying a dicarboxylic acid diester with a diol, or directly esterifying a dicarboxylic acid with a diol, to obtain one or more of a polyester monomer or a polyester oligomer;
a polycondensation step comprising reacting the one or more of a polyester monomer or a polyester oligomer in a polycondensation reaction in the presence of a polycondensation catalyst to produce a polyester polymer having an It.V. from about 0.50 dL/g to about 1.1 dL/g;
a particulation step in which the polyester polymer is solidified into particles;
an optional solid-stating step in which the solid polymer is polymerized to an It.V. from about 0.70 dL/g to about 1.2 dL/g; and
a particle addition step comprising adding and dispersing metallic molybdenum particles to provide an amount from about 1 ppm to about 100 ppm by weight of the polymer, wherein the particle addition step occurs before, during, or after any of the preceding steps.

### Claim 23 (depends on 22)

The process according to claim 22, wherein the process further comprises a forming step, following the optional solid-stating step, the forming step comprising melting and extruding the resulting solid polymer to obtain a formed item having the metallic molybdenum particles dispersed therein.

### Claim 24 (depends on 23)

The process according to claim 23, wherein the particle addition step occurs during or after the optional solid-stating step and prior to the forming step.

### Claim 25 (depends on 22)

The process according to claim 22, wherein the particle addition step comprises adding the metallic molybdenum particles as a thermoplastic concentrate prior to or during the forming step, the thermoplastic concentrate comprising the metallic molybdenum particles in an amount from about 50 ppm to about 5,000 ppm, with respect to the weight of the thermoplastic concentrate.

### Claim 26 (depends on 22)

The process according to claim 22, wherein the metallic molybdenum particles have a median particle size from about 0.005 μm to about 10 μm.

### Claim 27 (depends on 22)

The process according to claim 22, wherein the particle addition step is carried out prior to or during the polycondensation step.

### Claim 28 (depends on 22)

The process according to claim 22, wherein the particle addition step is carried out prior to or during the particulation step.

### Claim 29 (depends on 22)

The process according to claim 22, wherein the particle addition step is carried out prior to or during the solid-stating step.

### Claim 30 (depends on 23)

The process according to claim 23, wherein the particle addition step is carried out prior to or during the forming step.

### Claim 31 (depends on 22)

The process according to claim 22, wherein the dicarboxylic acid comprises terephthalic acid.

### Claim 32 (depends on 22)

The process according to claim 22, wherein the dicarboxylic acid diester comprises dimethyl terephthalate.

### Claim 33 (depends on 22)

The process according to claim 22, wherein the diol comprises ethylene glycol.

### Claim 34 (depends on 22)

The process according to claim 22, wherein the dicarboxylic acid comprises naphthalene dicarboxylic acid.

### Claim 35 (depends on 22)

The process according to claim 22, wherein the dicarboxylic acid comprises an aromatic dicarboxylic acid.

### Claim 36 (depends on 25)

The process according to claim 25, wherein the thermoplastic concentrate comprises:
metallic molybdenum particles, in an amount ranging from 0.15 wt. % and up to about 35 wt. % based on the weight of the thermoplastic concentrate; and
a thermoplastic polymer, in an amount of at least 65 wt. % based on the weight of the thermoplastic concentrate.

### Claim 37 (depends on 36)

The process according to claim 36, wherein the thermoplastic polymer comprises one or more of: a polyester, a polyolefin, or a polycarbonate.

### Claim 38

A process for making a polyester preform, comprising feeding a molten or solid bulk polyester and a liquid, molten or solid polyester concentrate composition to a machine for manufacturing the preform, the concentrate composition comprising metallic molybdenum particles having a median particle size from about 0.005 μm to about 10 μm, to obtain a preform having from about 1 ppm to about 100 ppm metallic molybdenum particles, based on the weight of the polyester preform.

### Claim 39 (depends on 38)

The process of claim 38, wherein the metallic molybdenum particles are present in the concentrate composition in an amount of at least 0.15 wt. %.

### Claim 40 (depends on 39)

The process of claim 39, wherein the concentrate polyester polymer comprises the same residues as the bulk polyester polymer.

### Claim 41 (depends on 38)

The process of claim 38, wherein the bulk polyester and the polyester concentrate are fed to the machine in separate streams.

### Claim 42 (depends on 38)

The process of claim 38, wherein the concentrate polyester comprises post-consumer-recycle polyester.

### Claim 43

A process for producing a polyester composition, comprising adding a concentrate polyester composition to a melt phase process for the manufacture of virgin polyester polymers, said concentrate comprising metallic molybdenum particles having a median particle size from about 0.005 μm to about 10 μm, to obtain a polyester composition having from about 1 ppm to about 100 ppm metallic molybdenum particles, based on the weight of the polyester composition.

### Claim 44 (depends on 43)

The process of claim 43, wherein the polyester concentrate is added to the melt phase when the melt phase has an It.V. which is within +/−0.2 It.V. units of the It.V. of the polyester concentrate.