# US 2006/0051519 A1 · Multi-stage processes for drying and curing substrates coated with aqueous basecoat and a topcoat

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0051519 A1
- Document ID: US20060051519A1
- Status: Published application
- Kind: A1
- Application number: 10/933,752
- Filed: 2004-09-03
- Published: 2006-03-09
- Earliest claimed: 2004-09-03
- Inventors: Dennis Dixon; Basil Gregorovich; John Moore
- Web page: https://patentgrep.com/patent/US20060051519A1

## CPC

- B05D 7/534: {the first layer being let to dry at least partially before applying the second layer (B05D7/538 takes precedence)}
- B05D 3/0209: {Multistage baking}
- B05D 3/0263: {with IR heaters}
- B05D 3/029: {with microwaves}
- B05D 3/0413: {Heating with air}
- B05D 2201/00: Polymeric substrate or laminate
- B05D 2202/00: Metallic substrate
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

A multi-stage process for drying and curing substrates coated with liquid waterborne basecoat and a topcoat includes: (a) applying a liquid waterbome basecoating composition to the substrate surface; (b) exposing the basecoating composition to air having a temperature ranging from ambient to about 40° C. for a period of about 30 seconds to volatilize at least a portion of volatile material from the liquid basecoating composition, the velocity of the air at the surface of the basecoating composition being about 0.3 to about 1 meter per second; (c) applying heated air to the basecoating composition for a period ranging from about 30 to about 45 seconds, the velocity of the air at the surface of the basecoating composition ranging from about 1.5 to 15 meters per second, the air having a temperature ranging from about 30° C. to about 90° C.; (d) applying infrared radiation and heated air simultaneously to the basecoating composition for a period of ranging from about 30 to 45 seconds, the velocity of the air at the surface of the basecoating ranging from about 1.5 to 5 meters per second, the air having a temperature ranging from about 30° C. to about 60° C., such that a sufficiently dried basecoat is formed upon the surface of the substrate; (e) applying a topcoating composition over the basecoat; and (f) simultaneously curing the basecoating composition and the topcoating composition together.

## Claims

### Claim 1

A process for drying substrates coated with liquid waterborne basecoats, comprising the steps of: (a) applying a waterborne basecoating composition to a surface of the substrate; (b) exposing the basecoating composition to air having a temperature ranging from about 20° C. to about 40° C. for a period of about 30 seconds to volatilize at least a portion of volatile material from the liquid basecoating composition, the velocity of the air at a surface of the basecoating composition being about 0.3 to about 1 meter per second; (c) applying heated air to the basecoating composition for a period of about 30 seconds to 2 minutes, the velocity of the air at the surface of the basecoating composition being about 1.5 to about 15 meters per second, the air having a temperature ranging from about 30° C. to about 90° C.; (d) applying infrared radiation and heated air simultaneously to the basecoating composition for a period from about 30 seconds to 2 minutes, the velocity of the air at the surface of the basecoating composition being about 1.5 to 5 meters per second, the air having temperature of from about 30° C. to about 60° C., such that a sufficiently dried basecoat is formed upon the surface of the substrate; and (e) applying a topcoating composition over the basecoat.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the substrate is metal selected from the group consisting of iron, steel, aluminum, zinc, magnesium, alloys and combinations thereof.

### Claim 3 (depends on 2)

The process according to claim 2, wherein the metal substrate is an automotive body component.

### Claim 4 (depends on 1)

The process according to claim 1, wherein the period ranges from about 30 seconds to about 2 minutes in step (b).

### Claim 5 (depends on 1)

The process according to claim 1, wherein the infrared radiation applied in step (d) is emitted at a wavelength in the near- to intermediate-infrared region ranging from about 0.7 to about 20 micrometers.

### Claim 6 (depends on 5)

The process according to claim 5, wherein the infrared radiation applied in step (d) is emitted at a wavelength in the near-infrared region ranging from about 0.7 to about 4 micrometers.

### Claim 7 (depends on 1)

The process according to claim 1, wherein the period ranges from about 30 seconds to about 45 seconds in step (c).

### Claim 8 (depends on 7)

The process according to claim 7, wherein the period ranges from about 30 seconds to about 45 seconds in step (d).

### Claim 9 (depends on 1)

The process according to claim 1, wherein the topcoat is applied over the basecoat wet on wet.

### Claim 10 (depends on 1)

The process according to claim 1, further comprising an additional step of simultaneously curing the basecoating composition and the topcoating composition after application of the topcoating composition.

### Claim 11 (depends on 1)

The process according to claim 1, wherein the substrate is a polymeric substrate and wherein the peak temperature of the substrate during the process does not exceed the heat distortion temperature of the polymeric material.

### Claim 12 (depends on 1)

The process according to claim 1 wherein the radiation source is microwave energy.