# US 2006/0051504 A1 · Process for manufacturing thermoplastic materials containing inorganic particulates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0051504 A1
- Document ID: US20060051504A1
- Status: Published application
- Kind: A1
- Application number: 10/934,991
- Filed: 2004-09-07
- Published: 2006-03-09
- Earliest claimed: 2004-09-07
- Inventors: Daniel Craig; Jeffrey Elliott; George Perakis
- Web page: https://patentgrep.com/patent/US20060051504A1

## CPC

- C08K 9/04: Ingredients treated with organic substances {(treated with macromolecular compounds C08K9/08)}
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

Processes are disclosed for treating an inorganic particulate to provide improved dispersibility in a thermoplastic, for example, titanium dioxide as an opacifier or colorant in a polyolefin concentrate, and for producing said pigmented thermoplastic, wherein a surface coating is deposited on the particulate which comprises at least one amide of a fatty acid and an aliphatic amine.

## Claims

### Claim 1

A process for improving the dispersibility of an inorganic particulate in a thermoplastic, comprising depositing a surface coating on the particulate including at least one amide of a fatty acid and an aliphatic amine.

### Claim 2 (depends on 1)

A process as defined in claim 1, wherein the surface coating is accomplished by supplying one or more of the amides into a fluid energy mill wherein the inorganic particulate is being milled.

### Claim 3 (depends on 1)

A process as defined in claim 1, wherein the surface coating is accomplished by spraying one or more of the amides onto, or mixing one or more of the amides into, the dry inorganic particulate.

### Claim 4 (depends on 1)

A process as defined in claim 1, wherein the surface coating is accomplished by adding one or more of the amides to a slurry of the inorganic particulate and then recovering the inorganic particulate from the slurry.

### Claim 5 (depends on 1)

A process as defined in claim 1, wherein the inorganic particulate comprises titanium dioxide, basic carbonate white lead, basic sulfate white lead, basic silicate white lead, zinc sulfide, zinc oxide, a composite pigment of zinc sulfide and barium sulfate, antimony oxide, calcium carbonate, calcium sulfate, a china or kaolin clay, mica, diatomaceous earth; iron oxide, lead oxide, cadmium sulfide, cadmium selenide, lead chromate, zinc chromate, nickel titanate or chromium oxide.

### Claim 6 (depends on 5)

A process as defined in claim 5, wherein a surface coating is deposited on the inorganic particulate comprised of one or more of lauric acid amide, palmitic acid amide, stearic acid amide, erucic acid amide, ethylenebisstearamide and stearic acid N,N-dimethylamide.

### Claim 7 (depends on 6)

A process as defined in claim 6, wherein a surface coating is deposited on the inorganic particulate such that the amide materials comprise from about 0.25 to about 2.5 percent by weight of the inorganic particulate.

### Claim 8 (depends on 7)

A process as defined in claim 7, wherein the inorganic particulate is titanium dioxide.

### Claim 9 (depends on 1)

A process as defined in claim 1, comprising depositing an inorganic metal oxide or an inorganic metal hydroxide on the inorganic particulate, before the amide-containing surface coating is deposited.

### Claim 10

A process for manufacturing an inorganic particulate-containing thermoplastic, comprising a) depositing a surface coating on an inorganic particulate which comprises at least one amide of a fatty acid and an aliphatic amine, and b) intimately mixing said treated inorganic particulate with a thermoplastic material under temperature conditions wherein the thermoplastic is at least partially melted for the duration of the mixing step.