# US 2006/0040511 A1 · [method of fabricating shallow trench isolation structure for reducing wafer scratch]

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0040511 A1
- Document ID: US20060040511A1
- Status: Published application
- Kind: A1
- Application number: 10/711,003
- Filed: 2004-08-17
- Published: 2006-02-23
- Earliest claimed: 2004-08-17
- Inventors: Jason Lu
- Web page: https://patentgrep.com/patent/US20060040511A1

## CPC

- H10W 46/00: Marks applied to devices, e.g. for alignment or identification
- H10P 95/062: {involving a dielectric removal step}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W 46/603: {Formed on wafers or substrates before dicing and remaining on chips after dicing}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of fabricating a shallow trench isolation structure for reducing wafer scratch reducing scratch on a wafer surface is provided. A parameter of a processing operation is controlled in a manner to reduce an amassment of material over the wafer surface. Thus, a step height from the surface of the substrate, which would otherwise cause micro-scratches on the wafer surface in a subsequent chemical-mechanical polishing operation, can be effectively reduced.

## Claims

### Claim 1

A method of fabricating a shallow trench isolation structure for reducing wafer scratch reducing wafer scratch, comprising the steps of:
providing a substrate; and
performing a processing operation over a surface of the substrate prior to performing a chemical mechanical polishing process, wherein at least a protrusion is formed over the surface of the substrate during the processing operation, and wherein a parameter of the processing operation is adjusted in a manner to reducing a step height of the protrusion compared that without adjusting the parameter of the processing operation.

### Claim 2 (depends on 1)

The method of reducing wafer scratch of claim 1, wherein the processing operation comprises a laser marking process.

### Claim 3 (depends on 2)

The method of reducing wafer scratch of claim 2, wherein the step of adjusting a parameter of a processing operation comprises adjusting an energy of the laser beam used in the laser marking process.

### Claim 4 (depends on 3)

The method of reducing wafer scratch of claim 3, wherein the energy of the laser beam used in the laser marking process is smaller than 1000 micro-joule (μ j).

### Claim 5 (depends on 3)

The method of reducing wafer scratch of claim 3, wherein the step of adjusting parameter of the processing operation comprises reducing the step height to a level below 4 micrometer (μ m).

### Claim 6

A method of fabricating a shallow trench isolation structure for reducing wafer scratch process of fabricating a shallow trench isolation structure, comprising the steps of:
providing a substrate;
performing a laser marking operation to form a laser mark on the substrate, wherein at least a protrusion is formed during the laser marking operation due to an amassment of material, and wherein a parameter of the laser marking operation is adjusted in a manner to reduce a step height of the protrusion compared to that without adjusting the parameter;
forming a patterned mask layer over the substrate;
etching the substrate using the patterned mask layer as an etching mask to form a trench;
forming an insulation layer over the substrate, wherein the insulation layer completely fills the trench;
removing a portion of the insulation layer by performing a chemical-mechanical polishing process; and
removing the patterned mask layer.

### Claim 7 (depends on 6)

The method process of claim 6, wherein step of controlling the parameter of the laser marking operation includes adjusting an energy of the laser beam used in the laser marking operation to a level below 1000 micro-joule (μ j).

### Claim 8 (depends on 6)

The method process of claim 6, wherein the step of controlling the parameter in the laser marking operation comprises reducing the step height to a level below 4 micrometer (μ m).