# US 2006/0040052 A1 · Methods for depositing tungsten layers employing atomic layer deposition techniques

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0040052 A1
- Document ID: US20060040052A1
- Status: Published application
- Kind: A1
- Application number: 10/418,728
- Filed: 2003-04-18
- Published: 2006-02-23
- Earliest claimed: 2001-10-10
- Inventors: Hongbin Fang; Hyungsuk Yoon; Ken Lai; Chi Young; Chao-Ming Huang; Ming Xi; Michael Yang; Hua Chung
- Web page: https://patentgrep.com/patent/US20060040052A1

## CPC

- C23C 16/06: characterised by the deposition of metallic material
- C23C 16/02: Pretreatment of the material to be coated (C23C16/04 takes precedence)
- C23C 16/0218: {in a reactive atmosphere (C23C16/0227 takes precedence)}
- C23C 16/0281: {of metallic sub-layers (C23C16/029 takes precedence)}
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/08: from metal halides
- C23C 16/16: from metal carbonyl compounds
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method for forming a tungsten layer on a substrate surface is provided. In one aspect, the method includes positioning the substrate surface in a processing chamber and exposing the substrate surface to a soak. A nucleation layer is then deposited on the substrate surface in the same processing chamber by alternately pulsing a tungsten-containing compound and a reducing gas selected from a group consisting of silane, disilane, dichlorosilane and derivatives thereof. A tungsten bulk layer may then be deposited on the nucleation layer using cyclical deposition, chemical vapor deposition, or physical vapor deposition techniques.

## Claims

### Claim 1

A method for forming a tungsten layer on a substrate surface, comprising:
positioning the substrate surface in a processing chamber;
exposing the substrate surface to a soak for a predetermined time, wherein the soak comprises a soak compound; and
depositing a nucleation layer in the same processing chamber by alternately pulsing a tungsten-containing compound and a reducing gas,-wherein the reducing gas comprises a reductant different than the soak compound.

### Claim 2 (depends on 1)

The method of claim 1, wherein the reductant is selected from the group consisting of hydrogen, silane, disilane, trisilane, dichlorosilane, borane, diborane, derivatives thereof, and combinations thereof.

### Claim 3 (depends on 2)

The method of claim 2, wherein the nucleation layer is deposited by alternately pulsing tungsten hexafluoride and silane.

### Claim 4 (depends on 2)

The method of claim 2, wherein the nucleation layer is deposited by alternately pulsing tungsten hexafluoride and diborane.

### Claim 5 (depends on 4)

The method of claim 4, wherein the nucleation layer has a thickness in a range from about 10 Å to about 200 Å.

### Claim 6 (depends on 2)

The method of claim 2, wherein the tungsten-containing compound is selected from the group consisting of tungsten hexafluoride and tungsten carbonyl.

### Claim 7 (depends on 6)

The method of claim 6, wherein the soak compound is selected from the group consisting of hydrogen, borane, diborane, hydrogen, silane, disilane, trisilane, dichlorosilane, derivatives thereof and combinations thereof.

### Claim 8 (depends on 7)

The method of claim 7, wherein exposing the substrate surface to the soak for the predetermined time is in a range from about 5 seconds to about 90 seconds.

### Claim 9 (depends on 1)

The method of claim 1, further comprising forming a bulk tungsten deposition film on the nucleation layer using atomic layer deposition, chemical vapor deposition or physical vapor deposition techniques.

### Claim 10 (depends on 7)

The method of claim 7, wherein exposing the substrate surface to the soak is at a temperature in a range from about 100° C. to about 400° C.

### Claim 11 (depends on 7)

The method of claim 7, wherein the substrate surface comprises titanium nitride.

### Claim 12

A method for forming a tungsten layer on a substrate surface, comprising:
exposing a substrate surface to diborane at a pressure range from about 1 Torr to about 50 Torr and at a temperature range from about 100° C. to about 400° C.;
depositing a nucleation layer by alternately pulsing a tungsten-containing compound and silane gas; and
forming a bulk tungsten deposition film on the nucleation layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein exposing the substrate surface to diborane and depositing the nucleation layer occurs in the same chamber.

### Claim 14 (depends on 13)

The method of claim 13, wherein the nucleation layer has a thickness in a range from about 10 Å to about 200 Å.

### Claim 15 (depends on 14)

The method of claim 14, wherein the bulk tungsten deposition film has a thickness in a range from about 100 Å to about 5,000 Å.

### Claim 16 (depends on 13)

The method of claim 13, wherein exposing the substrate surface to diborane for a predetermined time is in a range from about 5 seconds to about 90 seconds.

### Claim 17 (depends on 12)

The method of claim 12, wherein the substrate surface comprise a barrier layer selected from the group consisting of titanium, titanium nitride, tungsten nitride, tantalum and tantalum nitride.

### Claim 18

A method for forming a tungsten layer on a substrate surface, comprising:
positioning the substrate surface in a processing chamber;
exposing the substrate surface to a diborane soak for a predetermined time;
depositing a nucleation layer in the same processing chamber by alternately pulsing a tungsten-containing compound and a reducing gas, wherein the reducing gas comprises a reductant; and
forming a bulk tungsten deposition film on the nucleation layer.

### Claim 19 (depends on 18)

The method of claim 18, wherein the nucleation layer has a thickness in a range from about 10 Å to about 200 Å.

### Claim 20 (depends on 19)

The method of claim 19, wherein the bulk tungsten deposition film has a thickness in a range from about 100 Å to about 5,000 Å.

### Claim 21 (depends on 19)

The method of claim 19, wherein the tungsten-containing compound is selected from the group consisting of tungsten hexafluoride and tungsten carbonyl.

### Claim 22 (depends on 21)

The method of claim 21, wherein exposing the substrate surface to the diborane soak for the predetermined time is in a range from about 5 seconds to about 90 seconds.

### Claim 23 (depends on 22)

The method of claim 22, wherein exposing the substrate surface to the diborane soak is at a temperature in a range from about 100° C. to about 400° C.

### Claim 24 (depends on 18)

The method of claim 18, wherein the reductant is selected from the group consisting of hydrogen, silane, disilane, trisilane, dichlorosilane, borane, diborane, derivatives thereof, and combinations thereof.

### Claim 25 (depends on 24)

The method of claim 24, wherein the tungsten-containing compound is tungsten hexafluoride and the reductant is silane.

### Claim 26 (depends on 24)

The method of claim 24, wherein the tungsten-containing compound is tungsten hexafluoride and the reductant is diborane.

### Claim 27

A method for forming a tungsten layer on a substrate surface, comprising:
positioning the substrate surface in a processing chamber;
exposing the substrate surface to a soak for a predetermined time, wherein the soak comprises a soak compound selected from the group consisting of hydrogen, borane, diborane, hydrogen, silane, disilane, trisilane, dichlorosilane, derivatives thereof and combinations thereof; and
depositing a nucleation layer in the same processing chamber by alternately pulsing a tungsten-containing compound and a reducing gas, wherein the reducing gas comprises a reductant different than the soak compound.

### Claim 28 (depends on 27)

The method of claim 27, wherein the reductant is selected from the group consisting of hydrogen, silane, disilane, trisilane, dichlorosilane, borane, diborane, derivatives thereof, and combinations thereof.

### Claim 29 (depends on 28)

The method of claim 28, wherein the nucleation layer is deposited by alternately pulsing tungsten hexafluoride and silane.

### Claim 30 (depends on 28)

The method of claim 28, wherein the nucleation layer is deposited by alternately pulsing tungsten hexafluoride and diborane.

### Claim 31 (depends on 30)

The method of claim 30, wherein the nucleation layer has a thickness in a range from about 10 Å to about 200 Å.

### Claim 32 (depends on 28)

The method of claim 28, wherein the tungsten-containing compound is selected from the group consisting of tungsten hexafluoride and tungsten carbonyl.

### Claim 33 (depends on 32)

The method of claim 32, wherein exposing the substrate surface to the soak for the predetermined time is in a range from about 5 seconds to about 90 seconds.

### Claim 34 (depends on 28)

The method of claim 28, further comprising forming a bulk tungsten deposition film on the nucleation layer using atomic layer deposition, chemical vapor deposition or physical vapor deposition techniques.

### Claim 35 (depends on 32)

The method of claim 32, wherein exposing the substrate surface to the soak is at a temperature in a range from about 100° C. to about 400° C.

### Claim 36 (depends on 32)

The method of claim 32, wherein the substrate surface comprises titanium nitride.