A method of repairing failure spots using a first metal alloy charge and a metal precipitate from a second metal alloy charge, along a section of a first tubular conduit within a subterranean well, comprising the steps of:
- (1) introducing into the well a well tool, comprising:
- (a) an elongated housing having a cylindrical interior chamber and a lower end, said chamber being formed by first and second sections thereof, said housing having proximate its lower end a circumferentially extending dissolvable sacrificial wall means for initially isolating the chambers from the exterior of the housing and, upon melting of the metal alloy charges, providing a passageway through said housing to permit the first metal alloy charge and the precipitate of the second metal alloy charge to flow out of the housing and into the well;
- (c) a first, lower temperature melting eutectic metal alloy charge deposited within one of the first and second sections of the chamber;
- (d) a second, higher temperature melting metal alloy charge deposited within the other of the first and second sections of the chamber;
- (e) means at one end of said housing for introducing, positioning and retrieving said tool within said well;
- (f) an ignitable fuel system within said chamber;
- (g) means for igniting the fuel system, whereby, upon activation of the igniting means, the fuel system is ignited sufficient to heat and melt the first lower temperature melting eutectic metal alloy charge and thereafter sufficient to heat and melt the second higher temperature melting metal alloy charge, whereby, upon said melting of said alloy charges, a metal precipitate is formed from the second metal alloy charge and the sacrificial wall is dissolved to provide said passageway for the flow of the first metal alloycharge and the precipitate through the housing and into the well;
- (h) plug means initially carried on said housing and selectively detachable therefrom for defining an annular area between the exterior of said plug means and the interior of said first tubular conduit when said tool is straddleingly positioned immediate said failure spots;
- (2) straddleingly positioning the tool immediate the area of the section of the first tubular conduit including the failure spots;
- (3) igniting the fuel charge to generate sufficient heat to sequentially melt the low temperature alloy and the high temperature alloy and form a metal precipitate from the high temperature metal alloy, whereby the passageway in the housing is opened to permit the metal precipitate formed from the high temperature alloy to first flow out of the housing and form a bridge into the well immediate the failure spots, and to secondly permit the low temperature alloy to flow out of the housing upon the bridge and into the well immediate the failure spot, to plug and cover the failure spots:
- (4) applying an upward force upon the well tool to detach the plug means from the housing;
- and
- (5) retrieving the housing to the top of the well.