# US 2006/0037699 A1 · Polishing pad and method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0037699 A1
- Document ID: US20060037699A1
- Status: Published application
- Kind: A1
- Application number: 10/536,621
- Filed: 2003-11-27
- Published: 2006-02-23
- Earliest claimed: 2002-11-27
- Assignees: Toyo Tire & Rubber Co., Ltd.
- Inventors: Masahiko Nakamori; Tetsuo Shimomura; Takatoshi Yamada; Kazuyuki Ogawa; Atsushi Kazuno; Kimihiro Watanabe
- Web page: https://patentgrep.com/patent/US20060037699A1

## CPC

- B24B 37/205: {provided with a window for inspecting the surface of the work being lapped}
- B24B 37/013: Devices or means for detecting lapping completion
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS

## Abstract

A polishing pad enabling a highly precise optical endpoint sensing during the polishing process and thus having excellent polishing characteristics (such as surface uniformity and in-plane uniformity) is disclosed. A polishing pad enabling to obtain the polishing profile of a large area of a wafer is also disclosed. A polishing pad of a first invention comprises a light-transmitting region having a transmittance of not less than 50% over the wavelength range of 400 to 700 nm. A polishing pad of a second invention comprises a light-transmitting region having a thickness of 0.5 to 4 mm and a transmittance of not less than 80% over the wavelength range of 600 to 700 nm. A polishing pad of a third invention comprises a light-transmitting region arranged between the central portion and the peripheral portion of the polishing pad and having a length (D) in the diametrical direction which is three times or more longer than the length (L) in the circumferential direction.

## Claims

### Claim 1

A polishing pad used in chemical mechanical polishing and having a polishing region and a light-transmitting region, said polishing pad having at least one of the following characteristics: i) light transmittance in the light-transmitting region throughout the wavelength range of 400 to 700 nm is 50% or more: ii) a thickness of the light-transmitting region is 0.5 to 4 mm. and light transmittance in the light-transmitting region throughout the wavelength range of 600 to 700 nm is 80% or more; or iii) the light-transmitting region is arranged between a central portion and a peripheral portion of the polishing pad, and a length (D) in a diametrical direction is 3 times or more longer than a length (L) in a circumferential direction.

### Claim 2 (depends on 1)

The polishing pad according to claim 1, wherein a rate of change of the light transmittance in the light-transmitting region in wavelengths of 400 to 700 nm represented by the following equation is 50% or less:
the rate of change (%)={(maximum transmittance in 400 to 700 nm−minimum transmittance in 400 to 700 nm)/maximum transmittance in 400 to 700 nm}×100.

### Claim 3 (depends on 1)

The polishing pad according to claim 1, wherein the light transmittance in the light-transmitting region at a wavelength of 400 nm is 50% or more, and the transmittance in the light-transmitting region throughout the wavelength range of 500 to 700 nm is 90% or more.

### Claim 4 (depends on 1)

The polishing pad according to any one of claims 1, wherein a difference among respective light transmittances in the light-transmitting region in 500 to 700 nm is 5% or less.

### Claim at position 5

5-6. (canceled)

### Claim 7 (depends on 1)

The polishing pad according to claim 1, wherein a shape of the light-transmitting region is rectangular.

### Claim 8 (depends on 1)

The polishing pad according to claim 1, wherein a length (D) in a diametrical direction is ¼ to ½ relative to a diameter of a material to be polished.

### Claim 9 (depends on 1)

The polishing pad according to claims 1, wherein a scatter of the thickness of the light-transmitting region is 100 μm or less.

### Claim 10 (depends on 1)

The polishing pad according to claims 1, wherein materials for forming the polishing region and the light-transmitting region are polyurethane resin.

### Claim 11 (depends on 10)

The polishing pad according to claim 10, wherein the polyurethane resin as the material for forming the polishing region and the polyurethane resin as the material for forming the light-transmitting region comprise the same kinds of organic isocyanate, polyol and chain extender.

### Claim 12 (depends on 1)

The polishing pad according to of claims 1, wherein a material for forming the light-transmitting region is non-foam.

### Claim 13 (depends on 1)

The polishing pad according to claim 1, which does not have an uneven structure for retaining and renewing an abrasive liquid on a surface of the light-transmitting region on a polishing side.

### Claim 14 (depends on 1)

The polishing pad according to claims 1, wherein a material for forming the polishing region is fine-cell foam.

### Claim 15 (depends on 1)

The polishing pad according to of claims 1, wherein a surface of the polishing region on a polishing side is provided with grooves.

### Claim 16 (depends on 14)

The polishing pad according to claim 14, wherein an average cell diameter of the fine-cell foam is 70 μm or less.

### Claim 17 (depends on 1)

The polishing pad according to claims 1, wherein a specific gravity of the fine-cell foam is 0.5 to 1.0 g/cm3.

### Claim 18 (depends on 1)

The polishing pad according to claims 1, wherein a hardness of the fine-cell foam is 45 to 65° in terms of Asker D hardness.

### Claim 19 (depends on 1)

The polishing pad according to claim 1, wherein a compressibility of the fine-cell foam is 0.5 to 5.0%.

### Claim 20 (depends on 1)

The polishing pad according to claims 1, wherein a compression recovery of the fine-cell foam is 50 to 100%.

### Claim 21 (depends on 1)

The polishing pad according to claims 1, wherein a storage elastic modulus of the fine-cell foam at 40° C. at 1 Hz is 200 MPa or more.

### Claim 22 (depends on 1)

A method of producing a semiconductor device, which comprises a step of polishing a surface of a semiconductor wafer with the polishing pad recited in claims 1.