# US 2006/0032843 A1 · Cutting of cementitious materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0032843 A1
- Document ID: US20060032843A1
- Status: Published application
- Kind: A1
- Application number: 10/528,822
- Filed: 2003-08-29
- Published: 2006-02-16
- Earliest claimed: 2002-09-28
- Inventors: Philippus Crouse; Lin Li; Julian Spencer
- Web page: https://patentgrep.com/patent/US20060032843A1

## CPC

- E04G 23/08: Wrecking of buildings (of fences E04H17/26; {Demolition agents based on cementitious or like materials C04B41/0009})
- E04G 23/00: Working measures on existing buildings, ({domestic cleaning of walls or floors A47L11/00; grinding floors or walls B24B7/18; removing of wall coverings B44C7/00; removing of paint from surfaces B44D3/16; electrochemical desalination or re-alkalisation C04B41/00}; on foundations E02D35/00, E02D37/00; in connection with insulations E04B; subsequent or finishing work E04F)
- E04G: SCAFFOLDING; FORMS; SHUTTERING; BUILDING IMPLEMENTS OR AIDS, OR THEIR USE; HANDLING BUILDING MATERIALS ON THE SITE; REPAIRING, BREAKING-UP OR OTHER WORK ON EXISTING BUILDINGS

## Abstract

A method and apparatus for cutting thick sections of cement-based materials, the method comprising mutually traversing a surface to be cut with a laser beam at a power density sufficient to produce a depth of molten material having a maximum depth of 10 mm at each traverse; allowing the molten material to solidify; breaking the solidified material into particles; and removing the particles by suction means.

## Claims

### Claim at position 1

1-28. (canceled)

### Claim 29

A method for cutting thick sections of cement-based materials, the method comprising:
mutually traversing a surface to be cut with a laser beam at a power density sufficient to produce a depth of molten material having a maximum depth of 10 mm at each traverse;
allowing said molten material to solidify; breaking said solidified material into particles; and
removing said particles by suction means.

### Claim 30 (depends on 29)

A method according to claim 29 wherein a plurality-of traverses are made along substantially the same cutting path.

### Claim 31 (depends on 29)

A method according to either claim 29 wherein the laser beam is unfocused.

### Claim 32 (depends on 29)

A method according to claim 29 wherein the laser beam is a parallel beam.

### Claim 33 (depends on 29)

A method according to claim 29 wherein the laser beam has a rectangular cross section.

### Claim 34 (depends on 29)

A method according to claim 29 wherein the material is removed directly after solidification after each pass.

### Claim 35 (depends on 29)

A method according to claim 29 wherein the solidified material is broken up by a hollow crushing tube which also serves as a material extractor conduit.

### Claim 36 (depends on 29)

A method according to claim 29 wherein the depth of the molten material at each pass lies in the range from 0.5 to 5 mm.

### Claim 37 (depends on 29)

A method according to claim 29 wherein the pressure required for crushing the solidified material is less than 100 MPa.

### Claim 38 (depends on 29)

A method according to claim 29 wherein the laser power density lies in the range 300 W·cm−2 to 3000 W·cm−2.

### Claim 39 (depends on 29)

A method according to claim 29 wherein the beam traverse speed lies between 3 cm·min−1 and 30 cm·min−1.

### Claim 40 (depends on 29)

A method according to claim 29 wherein an oxygen jet is applied directly at the beam spot when reinforcing steel bars are being cut.

### Claim 41 (depends on 29)

A method according to claim 29 wherein the surface temperature of the material being treated lies in the range 700° C. to 2400° C.

### Claim 42 (depends on 29)

A method according to claim 29 wherein the vapor-to-melt ratio lies in the range between 0.05 and 3.

### Claim 43 (depends on 29)

A method according to claim 29 wherein the material removal rate lies in the region of 150 cm−3·kWh−1 for a diode laser and 100 cm−3·kWh−1 for a CO2 laser.

### Claim 44 (depends on 29)

A method according to claim 29 wherein the laser is selected from the group consisting of a COIL, Nd:YAG, CO2 and diode laser.

### Claim 45 (depends on 29)

A method according to claim 29 wherein the laser beam is delivered by a fiber optic cable.

### Claim 46 (depends on 29)

A method according to claim 29 wherein the laser beam is delivered by a mobile beam delivery system comprising a system of reflecting mirrors.

### Claim 47

An apparatus for cutting thick sections of cement-based materials in which material is made molten and allowed to solidify, the apparatus comprising
a means for mutually traversing a surface to be cut with an unfocused laser beam at a power density sufficient to produce a depth of molten material having a maximum depth of 10 mm at each traverse;
a means for breaking the solidified material into particles; and
a suction means for removing the particles.

### Claim 48 (depends on 47)

An apparatus according to claim 47 wherein the means for breaking re-solidified material comprises a percussive member for crushing the material.

### Claim 49 (depends on 48)

An apparatus according to claim 48 wherein the percussive member is hollow and crushed material is removed through the member by suction means.

### Claim 50 (depends on 47)

An apparatus according to claim 47 wherein the laser beam is substantially parallel.

### Claim 51 (depends on 47)

An apparatus according to claim 47 wherein the laser beam has a circular or rectangular cross section.