# US 2006/0032811 A1 · Transition radiation apparatus and method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0032811 A1
- Document ID: US20060032811A1
- Status: Published application
- Kind: A1
- Application number: 10/915,809
- Filed: 2004-08-10
- Published: 2006-02-16
- Earliest claimed: 2004-08-10
- Assignees: Intel Corporation
- Inventors: Yashesh Shroff
- Web page: https://patentgrep.com/patent/US20060032811A1

## CPC

- C23F 4/00: Processes for removing metallic material from surfaces, not provided for in group C23F1/00 or C23F3/00
- B23K 26/0661: {disposed on the workpiece}
- B23K 26/18: using absorbing layers on the workpiece, e.g. for marking or protecting purposes
- B23K 26/40: taking account of the properties of the material involved
- C23F 3/04: Heavy metals
- B23K 2101/40: Semiconductor devices
- B23K 2103/50: {Inorganic materials other than metals or composite materials}
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

In one embodiment of the present invention, intervening material layers (208) are recessed (304) relative to membrane layers (208) thereby providing increased surface area contact between the membranes (208) and support posts (408). Increased surface area contact assists in reducing membrane shape changes (122) and defects (124, 126) that can result from thermal and physical stress. In an alternative embodiment, problems related to stiction during release of a stack of membranes (208) is reduced by using different processes to completely remove portions of intervening material layers (206) between membrane layers (208). The first process removes the bulk of the intervening material layer (206). The second process removes the remaining portions of the intervening material layer (602).

## Claims

### Claim 1

A transition radiation emitting structure comprising a plurality of membrane layers, wherein a portion of edge regions of at least one membrane layer is inset with respect to a sidewall of an adjoining support post structure.

### Claim 2 (depends on 1)

The structure of claim 1, wherein the plurality of membrane layers comprises at least fifteen membrane layers.

### Claim 3 (depends on 2)

The structure of claim 2, wherein a thickness of a membrane layer in the plurality of membrane layers is within a range of approximately 27 and 108 nanometers, and a spacing between membrane layers is in a range approximately of 3-7 microns.

### Claim 4 (depends on 1)

The structure of claim 1, wherein a membrane in the plurality of membrane layers comprises molybdenum.

### Claim 5 (depends on 1)

The structure of claim 1, wherein the adjoining support post structure is tapered.

### Claim 6

A method for forming a transition radiation emitting structure comprising:
forming a stack of alternating membrane layers and intervening material layers over a substrate;
forming an opening at least partially through the stack of alternating membrane layers and intervening material layers;
recessing portions of the intervening material layers exposed by the opening relative to an edge region of a membrane layer exposed by the opening; and
filling the opening with material to define a support post structure, wherein the support post structure abuts portions of the edge region of the membrane layer, a lower surface of the membrane layer, and an upper surface of the membrane layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein a number of membrane layers formed in the transition radiation emitting structure is in a range of approximately 15-50.

### Claim 8 (depends on 6)

The method of claim 6, wherein at least one of the membrane layers has a thickness in a range of approximately 27 and 108 nanometers, and at least one of the intervening material layers has a thickness in a range of 3-7 microns.

### Claim 9 (depends on 6)

The method of claim 6, wherein at least one of the membrane layers comprises molybdenum.

### Claim 10 (depends on 6)

The method of claim 6, wherein the opening is further characterized as a tapered opening.

### Claim 11 (depends on 6)

The method of claim 6, further comprising:
partially removing portions of the intervening material layer between the membrane layers using a first process;
completely removing residual portions of the intervening material layer using a second process, wherein the first process is different from the second process.

### Claim 12

A method for forming a transition radiation emitting structure comprising:
forming a stack of alternating membrane layers and intervening material layers;
partially removing portions of the intervening material layer using a first process; and
completely removing residual portions of the intervening material layer using a second process, wherein the first process is different from the second process.

### Claim 13 (depends on 11)

The method of claim 11, wherein the first process is further characterized as a wet process and the second process is further characterized as a dry process.

### Claim 14 (depends on 13)

The method of claim 13, wherein the second process is further characterized as a dry-etch process.

### Claim 15 (depends on 11)

The method of claim 11, wherein the intervening material layer is further characterized as a resist layer.

### Claim 16 (depends on 11)

The method of claim 11, wherein at least one membrane layer has a thickness in a range of approximately 27-108 nanometers, and at least one intervening material layer has a thickness in a range of 3-7 microns.

### Claim 17 (depends on 11)

The method of claim 11, wherein at least one of the membrane layers comprise molybdenum.

### Claim 18

A method for manufacturing a semiconductor structure comprising:
positioning a semiconductor substrate in proximity to a transition radiation emitting structure, the transition radiation emitting structure having a plurality of membrane layers, wherein portions of peripheral edge regions of the membrane layers are inset with respect to sidewalls of an adjoining support post structure;
passing electron beam energy through the plurality of membrane layers to generate extreme ultraviolet radiation; and
using the extreme ultraviolet radiation to define patterned features on the semiconductor substrate.

### Claim 19 (depends on 18)

The method of claim 18, wherein an intervening material layer portion between two adjacent membrane layers has been partially removed using a first process and completely removed using a second process, wherein the first process is different from the second process.

### Claim 20

A method for manufacturing a semiconductor structure comprising:
positioning a semiconductor substrate in proximity to a transition radiation emitting structure, the transition radiation emitting structure having a plurality of membrane layers, wherein intervening material layer portions between the membrane layers have been partially removed using a first process and completely removed using a second process, wherein the first process is different from the second process;
passing electron beam energy through the plurality of membrane layers to generate extreme ultraviolet radiation; and
using the extreme ultraviolet radiation to define patterned features on the semiconductor substrate.

### Claim 21 (depends on 20)

The method of claim 20, wherein the first process is further characterized as a wet-etch process and the second process is further characterized as a dry-etch process.