# US 2006/0032739 A1 · Method for producing silicon oxide film and method for producing optical multilayer film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0032739 A1
- Document ID: US20060032739A1
- Status: Published application
- Kind: A1
- Application number: 11/256,941
- Filed: 2005-10-25
- Published: 2006-02-16
- Earliest claimed: 2003-04-25
- Assignees: Asahi Glass Company, Limited
- Inventors: Toru Ikeda; Takahiro Mashimo; Eiji Shidoji; Toshihisa Kamiyama; Yoshihito Katayama
- Web page: https://patentgrep.com/patent/US20060032739A1

## CPC

- G02B 1/10: Optical coatings produced by application to, or surface treatment of, optical elements (G02B1/08 takes precedence)
- C23C 14/0042: {Controlling partial pressure or flow rate of reactive or inert gases with feedback of measurements}
- C23C 14/0094: {in transition mode}
- C23C 14/083: {of refractory metals or yttrium}
- C23C 14/10: Glass or silica
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

The invention provides a method for producing a silicon oxide film, whereby a film having uniform optical constants such as refractive index, absorption coefficient, etc. can be formed continuously at a high deposition rate. A method for producing a silicon oxide film, which comprises depositing a silicon oxide film on a substrate by carrying out AC sputtering by using a sputtering target comprising silicon carbide and silicon with a ratio in number of atoms of C to Si being from 0.5 to 0.95, in an atmosphere containing an oxidizing gas, with an alternating current having a frequency of from 1 to 1,000 kHz.

## Claims

### Claim 1

A method for producing a silicon oxide film, which comprises depositing a silicon oxide film on a substrate by carrying out AC sputtering by using a sputtering target comprising silicon carbide and silicon with a ratio in number of atoms of C to Si being from 0.5 to 0.95, in an atmosphere containing an oxidizing gas, with an alternating current having a frequency of from 1 to 1,000 kHz.

### Claim 2 (depends on 1)

The method for producing a silicon oxide film according to claim 1, wherein the sputtering is carried out in a transition region.

### Claim 3 (depends on 1)

The method for producing a silicon oxide film according to claim 1, wherein the area of the sputtering target is from 300 to 100,000 cm2.

### Claim 4 (depends on 1)

The method for producing a silicon oxide film according to claim 1, wherein the area of the substrate is from 0.1 to 20.0 m2.

### Claim 5 (depends on 1)

The method for producing a silicon oxide film according to claim 1, wherein the shape of the sputtering target is columnar.

### Claim 6 (depends on 1)

The method for producing a silicon oxide film according to claim 1, wherein the oxidizing gas is oxygen, and oxygen is contained in an amount of from 35 to 60 vol % in the atmosphere.

### Claim 7 (depends on 1)

The method for producing a silicon oxide film according to claim 1, wherein the power density against the sputtering target in the sputtering is at least 5 W/cm2.

### Claim 8 (depends on 1)

The method for producing a silicon oxide film according to claim 1, wherein the deposition rate in the sputtering is at least 20 nm·m/min.

### Claim 9 (depends on 1)

The method for producing a silicon oxide film according to claim 1, wherein in the silicon oxide film, the SiO2 component is at least 99 mass % based on the entire film.

### Claim 10 (depends on 1)

The method for producing a silicon oxide film according to claim 1, wherein the silicon oxide film has an absorption coefficient of at most 1×10−3.

### Claim 11 (depends on 1)

The method for producing a silicon oxide film according to claim 1, wherein the silicon oxide film has is a film thickness of from 5 nm to 1 μm.

### Claim 12 (depends on 1)

A method for producing an optical multilayer film, which comprises forming, on a substrate, an optical multilayer film comprising plural layers of films including at least a silicon oxide film, wherein the silicon oxide film is formed by the method for producing a silicon oxide film as defined in claim 1.

### Claim 13 (depends on 12)

The method for producing an optical multilayer film according to claim 12, wherein the optical multilayer film comprises at least 20 layers of films.

### Claim 14 (depends on 12)

The method for producing an optical multilayer film according to claim 12, wherein any film other than the silicon oxide film contained in the optical multilayer film, is a Nb2O5 film, a TiO2 film or a Ta2O5 film.

### Claim 15 (depends on 12)

The method for producing an optical multilayer film according to claim 12, wherein the optical multilayer film has an absorbance of at most 5% in the entire visible light region.

### Claim 16 (depends on 12)

The method for producing an optical multilayer film according to claim 12, wherein the application of the optical multilayer film is an anti-reflection film, a dichroic mirror, a ultraviolet/infrared filter or a bandpass filter.