# US 2006/0032334 A1 · Method for manufacturing extrusion die tools

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0032334 A1
- Document ID: US20060032334A1
- Status: Published application
- Kind: A1
- Application number: 10/918,596
- Filed: 2004-08-13
- Published: 2006-02-16
- Earliest claimed: 2004-08-13
- Assignees: VIP Tooling, Inc., (an Indiana corporation)
- Inventors: Paul Nolting
- Web page: https://patentgrep.com/patent/US20060032334A1

## CPC

- B21C 25/025: {Selection of materials therefor}
- B21C 25/00: Profiling tools for metal extruding
- B21C 25/10: Making tools by operations not covered by a single other subclass
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL

## Abstract

The subject invention relates to a new method for manufacturing extrusion die tools that eliminates the step of hardening the steel after cutting the steel to form the desired extrusion die tool design. The new method involves the steps of cutting and finishing steel to form the desired extrusion die tool design, coating the die tool, or parts thereof, and hardening the coated die tool. The new method for manufacturing extrusion die tools reduces the time and the cost involved in their manufacture.

## Claims

### Claim 1

A method for manufacturing an extrusion die tool, the method comprising the steps of:
(a) cutting and finishing steel to form a finished state of an at least one-piece extrusion die tool;
(b) coating at least one portion of the at least one-piece extrusion die tool with a wear resistant coating at a high temperature; and
(c) hardening the at least one-piece extrusion die tool and the at least one coated portion.

### Claim 2 (depends on 1)

The method of claim 1, wherein the at least one portion coated in the coating step comprises a mandrel.

### Claim 3 (depends on 1)

The method of claim 1, wherein the cutting and finishing step forms the finished state of an open extrusion die tool comprising a mandrel insert, a sizing plate insert, and an annular base.

### Claim 4 (depends on 3)

The method of claim 3, wherein the cutting and finishing step comprises cutting and finishing an annealed high-speed steel to form the mandrel insert and the sizing plate insert and hot-working steel to form the annular base.

### Claim 5 (depends on 1)

The method of claim 1, wherein the cutting and finishing step comprises cutting and finishing an annealed high-speed steel to form a mandrel insert and a sizing plate insert.

### Claim 6 (depends on 4)

The method of claim 4, wherein the chemical composition of the annealed high-speed steel comprises one or more of: Carbon, Manganese, Silicon, Chromium, Vanadium, Tungsten, Molybdenum, Cobalt, Sulfur, and Iron.

### Claim 7 (depends on 4)

The method of claim 4, wherein the chemical composition of the hot-working steel comprises one or more of: Carbon, Manganese, Silicon, Chromium, Molybdenum, Vanadium and Iron.

### Claim 8 (depends on 5)

The method of claim 5, wherein the chemical composition of the annealed high-speed steel comprises one or more of: Carbon, Manganese, Silicon, Chromium, Vanadium, Tungsten, Molybdenum, Cobalt, Sulfur, and Iron.

### Claim 9 (depends on 1)

The method of claim 1, wherein the coating step comprises coating the at least one portion of the extrusion die tool at a temperature between about 1200° F.-1300° F.

### Claim 10 (depends on 9)

The method of claim 9, wherein the coating step comprises a CVD coating process.

### Claim 11 (depends on 3)

The method of claim 3, wherein the coating step coats the mandrel insert of the open extrusion die tool with a CVD coating process.

### Claim 12 (depends on 11)

The method of claim 11, further comprising the step of inserting the mandrel insert and sizing plate into the annular base.

### Claim 13 (depends on 5)

The method of claim 5, wherein the coating step coats the mandrel insert with a CVD coating process.

### Claim 14 (depends on 1)

The method of claim 1, wherein the cutting and finishing step forms the finished state of a closed extrusion die tool comprising a mandrel insert, a sizing plate insert, a male body, and a female body.

### Claim 15 (depends on 14)

The method of claim 14, wherein the cutting and finishing step comprises cutting and finishing an annealed high-speed steel to form the mandrel insert and the sizing plate insert and cutting and finishing hot-working steel to form the male and female bodies of the closed extrusion die tool.

### Claim 16 (depends on 15)

The method of claim 15, wherein the chemical composition of the annealed high-speed steel comprises one or more of: Carbon, Manganese, Silicon, Chromium, Vanadium, Tungsten, Molybdenum, Cobalt, Sulfur, and Iron.

### Claim 17 (depends on 16)

The method of claim 16, wherein the chemical composition of the annealed hot-working steel comprises one or more of: Carbon, Manganese, Silicon, Chromium, Molybdenum, Vanadium, and Iron.

### Claim 18 (depends on 14)

The method of claim 14, wherein the coating step coats the mandrel insert of the closed extrusion die tool with the CVD coating process.

### Claim 19 (depends on 18)

The method of claim 18, further comprising the step of inserting the mandrel into the female body and the sizing plate into the male body.

### Claim 20 (depends on 19)

The method of claim 19, further comprising the step of connecting the male body to the female body.

### Claim 21

A method of creating a mandrel insert for an extrusion die tool, the method comprising the steps of:
(a) cutting and finishing annealed steel to form a finished state of the mandrel insert;
(b) coating the mandrel insert with a wear resistant coating at a high temperature; and
(c) hardening the coated mandrel insert.

### Claim 22 (depends on 21)

The method of claim 21, wherein the coating step comprises coating the mandrel insert with a CVD coating process.

### Claim 23 (depends on 22)

The method of claim 22, wherein the cutting and finishing step cuts and finishes an annealed high-speed steel to form said mandrel insert.

### Claim 24 (depends on 23)

The method of claim 23, wherein the chemical composition of the annealed steel comprises one or more of: Carbon, Manganese, Silicon, Chromium, Vanadium, Tungsten, Molybdenum, Cobalt, Sulfur, and Iron.