# US 2006/0032328 A1 · Sintered valve guide and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0032328 A1
- Document ID: US20060032328A1
- Status: Published application
- Kind: A1
- Application number: 11/182,638
- Filed: 2005-07-14
- Published: 2006-02-16
- Earliest claimed: 2004-07-15
- Inventors: Katsunao Chikahata; Koichiro Hayashi; Hiroki Fujitsuka; Toru Tsuboi
- Web page: https://patentgrep.com/patent/US20060032328A1

## CPC

- C22C 38/16: containing copper
- C22C 9/02: with tin as the next major constituent
- C22C 33/0214: {comprising P or a phosphorus compound}
- C22C 33/0228: {comprising other non-metallic compounds or more than 5% of graphite}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/008: {containing tin}
- F01L 3/02: Selecting particular materials for valve-members or valve-seats; Valve-members or valve-seats composed of two or more materials
- F01L 3/08: Valves guides; Sealing of valve stem, e.g. sealing by lubricant
- B22F 2998/00: Supplementary information concerning processes or compositions relating to powder metallurgy
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- F01L 2301/00: Using particular materials
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F01L: CYCLICALLY OPERATING VALVES FOR MACHINES OR ENGINES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

Disclosed is a sintered valve guide guide formed of a sintered alloy consisting essentially of 3.5 to 5% copper, 0.3 to 0.6% tin, 0.04 to 0.15% phosphorus, 1.5 to 2.5% carbon and the balance iron, by mass, and as occasion needs, further containing 0.46 to 1.41% metal oxide, and MnS and/or magnesium silicate. The metallographic structure has: a matrix containing a pearlite phase, a Fe—P—C compound phase and a Cu—Sn alloy phase; pores; and a graphite of 1.2 to 1.7% by mass of the sintered alloy. In the cross section, the ratio of the pearlite phase to the matrix is 90 area % or more, the ratio of the Fe—P—C compound phase is 0.1 to 3 area % of the cross section, the ratio of the Cu—Sn alloy phase to the cross section is 1 to 3% by area, and the ratio of a portion of the Fe—P—C compound phase having a thickness of 15 microns or more is 10 area % or less of the whole Fe—P—C compound phase.

## Claims

### Claim 1

A sintered valve guide formed of a sintered alloy consisting essentially of 3.5 to 5% copper, 0.3 to 0.6% tin, 0.04 to 0.15% phosphorus, 1.5 to 2.5% carbon and the balance iron, by mass,
wherein the sintered alloy has a metallographic structure comprising: a matrix having a pearlite phase, a Fe—P—C compound phase and a Cu—Sn alloy phase; pores; and a graphite phase being dispersed at a ratio of 1.2 to 1.7% by mass of the sintered alloy, and
wherein, in a cross section of the metallographic structure of the sintered alloy, the ratio of the pearlite phase to the matrix is 90% by area or more, the ratio of the Fe—P—C compound phase to the cross section of the metallographic structure is 0.1 to 3% by area, the ratio of the Cu—Sn alloy phase to the cross section of the metallographic structure is 1 to 3% by area, and the ratio of a portion of the Fe—P—C compound phase having a thickness of 15 microns or more to whole of the Fe—P—C compound phase is 10% by area or less.

### Claim 2

A sintered valve guide formed of a sintered alloy consisting essentially of 3.5 to 5% copper, 0.3 to 0.6% tin, 0.04 to 0.15% phosphorus, 1.5 to 2.5% carbon, 0.46 to 1.41% metal oxide and the balance iron, by mass,
wherein the sintered alloy has a metallographic structure comprising: a matrix having a pearlite phase, a Fe—P—C compound phase, a Cu—Sn alloy phase and a metal oxide phase; pores; and a graphite phase being dispersed at a ratio of 1.2 to 1.7% by mass of the sintered alloy, and
wherein, in a cross section of the metallographic structure of the sintered alloy, the ratio of the pearlite phase to the matrix is 90% by area or more, the ratio of the Fe—P—C compound phase to the cross section of the metallographic structure is 0.1 to 3% by area, the ratio of the Cu—Sn alloy phase to the cross section of the metallographic structure is 1 to 3% by area, and a portion of the Fe—P—C compound phase having a thickness of 15 microns or more to whole of the Fe—P—C compound phase is 10% by area or less.

### Claim 3

A sintered valve guide formed of a sintered alloy consisting essentially of 3.5 to 5% copper, 0.3 to 0.6% tin, 0.04 to 0.15% phosphorus, 1.5 to 2.5% carbon, 1% or less of at least one solid lubricant selected from the group consisting of manganese sulfide and magnesium silicate minerals, and the balance iron, by mass,
wherein the sintered alloy has a metallographic structure comprising: a matrix having a pearlite phase, a Fe—P—C compound phase and a Cu—Sn alloy phase; pores; a graphite phase; and said at least one solid lubricant being dispersed in the pores or intergranularly dispersed in the metallographic structure, and
wherein, in a cross section of the metallographic structure of the sintered alloy, the ratio of the pearlite phase to the cross sectioin of the metallographic structure is 80% by area or more, the ratio of the Fe—P—C compound phase to cross section of the metallographic structure is 0.1 to 3% by area, the ratio of the Cu—Sn alloy phase to the cross section of the metallographic structure is 1 to 3% by area, the graphite phase is dispersed in the pores at a ratio of 0.8 to 3.2% by area of the cross section of the metallographic structure, and the ratio of a portion of the Fe—P—C compound phase having a thickness of 15 microns or more to whole of the Fe—P—C compound phase is 10% by area or less.

### Claim 4

A sintered valve guide formed of a sintered alloy consisting essentially of 3.5 to 5% copper, 0.3 to 0.6% tin, 0.04 to 0.15% phosphorus, 1.5 to 2.5% carbon, 0.46 to 1.41% metal oxide, 1.6% or less of at least one solid lubricant selected from the group consisting of manganese sulfide and magnesium silicate minerals, and the balance iron, by mass,
wherein the sintered alloy has a metallographic structure comprising: a matrix having a pearlite phase, a Fe—P—C compound phase, a Cu—Sn alloy phase and a metal oxide phase; pores; a graphite phase; and said at least one solid lubricant being dispersed in the pores or intergranularly dispersed in the metallographic structure, and
wherein, in a cross section of the metallographic structure of the sintered alloy, the ratio of the pearlite phase to the cross sectioin of the metallographic structure is 90% by area or more, the ratio of the Fe—P—C compound phase to cross section of the metallographic structure is 0.1 to 3% by area, the ratio of the Cu—Sn alloy phase to the cross section of the metallographic structure is 1 to 3% by area, the graphite phase is dispersed in the pores at a ratio of 0.8 to 3.2% by area of the cross section of the metallographic structure, and the ratio of a portion of the Fe—P—C compound phase having a thickness of 15 microns or more to whole of the Fe—P—C compound phase is 10% by area or less.

### Claim 5 (depends on 2)

The sintered valve guide as set forth in claim 2, wherein the metal oxide includes at least one oxide of a metal selected from the group consisting of aluminum, silicon, magnesium, iron, calcium and tin.

### Claim 6 (depends on 1)

The sintered valve guide as set forth in claim 1, wherein, in the cross section of the metallographic structure, the ratio of another portion of the Fe—P—C compound phase having a thickness of 5 microns or more and less than 15 microns to whole of the Fe—P—C compound phase is 10 to 40% by area, and the balance Fe—P—C compound phase has a thickness of less than 5 microns.

### Claim 7

A method of manufacturing a sintered valve guide, comprising:
preparing a powder mixture comprising, by mass: 0.27 to 0.7% of a Fe—P alloy powder; 3.93 to 5.44% of a Cu—Sn alloy powder; 1.7 to 2.7% of a graphite powder and the balance iron powder, wherein the Fe—P alloy powder consists essentially of 15 to 21% phosphorus, an inevitable amount of impurities and the balance iron, the Cu—Sn alloy powder consists essentially of 8 to 11% tin, an inevitable amount of impurities and the balance copper;
forming the powder mixture into a tubular compact by pressing the powder mixture in a tubular cavity; and
sintering the tubular compact in a non-oxidizing atmosphere at a sintering temperature of 950 to 1,050 degrees C.

### Claim 8 (depends on 7)

The manufacturing method as set forth in claim 7, wherein the iron powder includes an ore reduced iron powder containing 0.5 to 1.5% by mass of metal oxide.

### Claim 9 (depends on 7)

The manufacturing method as set forth in claim 7, wherein the iron powder is a mixture of an ore reduced iron powder and an atomized iron powder, wherein the content of the atomized iron powder in the mixture is 10 to 30% by mass.

### Claim 10 (depends on 7)

The manufacturing method as set forth in claim 7, wherein the iron powder has a maximum particle size of 104 to 200 microns.

### Claim 11 (depends on 7)

The manufacturing method as set forth in claim 7, wherein the Fe—P alloy powder has a maximum particle size of 61 to 104 microns, and the Cu—Sn alloy powder has a maximum particle size of 35 to 61 microns.

### Claim 12 (depends on 7)

The manufacturing method as set forth in claim 7, wherein the sintering time is 15 to 90 minutes.

### Claim 13 (depends on 7)

The manufacturing method as set forth in claim 7, wherein the preparing of the powder mixture further comprises:
mixing at least one powder of a manganese sulfide and magnesium silicate minerals into the powder mixture to adjust the ratio of said at least one powder in the powder mixture to 1.6% by mass or less.

### Claim 14 (depends on 7)

The manufacturing method as set forth in claim 7, wherein the tubular cavity is tapered at a ratio of 1/5000 to 1/1000 by inclining at least one of an inner bore surface of a die and a circumferential surface of a punch which define the tubular cavity.

### Claim 15 (depends on 7)

The manufacturing method as set forth in claim 7, further comprising:
dipping in an oil the sintered compact obtained by the sintering.

### Claim 16 (depends on 7)

The manufacturing method as set forth in claim 7, further comprising:
cooling the sintered compact obtained by the sintering at a cooling rate of 8 degrees C./min.