# US 2006/0021907 A1 · Inhibitor enhanced thermal upgrading of heavy oils

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2006/0021907 A1
- Document ID: US20060021907A1
- Status: Published application
- Kind: A1
- Application number: 11/127,731
- Filed: 2005-05-12
- Published: 2006-02-02
- Earliest claimed: 2004-05-14
- Assignees: ExxonMobil Research and Engineering Company
- Inventors: Ramesh Varadaraj; Christopher Eppig; Douglas Hissong; Robert Welch
- Web page: https://patentgrep.com/patent/US20060021907A1

## CPC

- C10G 9/007: {Visbreaking}
- C10G 9/16: Preventing or removing incrustation
- C10G 11/00: Catalytic cracking, in the absence of hydrogen, of hydrocarbon oils (cracking in direct contact with molten metals or salts C10G9/34)
- C10G 29/06: Metal salts, or metal salts deposited on a carrier
- C10G 45/00: Refining of hydrocarbon oils using hydrogen or hydrogen-generating compounds
- C10G 47/00: Cracking of hydrocarbon oils, in the presence of hydrogen or hydrogen- generating compounds, to obtain lower boiling fractions (C10G15/00 takes precedence; destructive hydrogenation of non-melting solid carbonaceous or similar materials C10G1/06)
- C10G 47/22: Non-catalytic cracking in the presence of hydrogen
- C10G 49/00: Treatment of hydrocarbon oils, in the presence of hydrogen or hydrogen-generating compounds, not provided for in a single one of groups C10G45/02, C10G45/32, C10G45/44, C10G45/58 or C10G47/00
- C10G 75/04: by addition of antifouling agents
- C10M 135/10: Sulfonic acids or derivatives thereof
- C10M 169/04: Mixtures of base-materials and additives
- C10M 175/0016: {with the use of chemical agents}
- C10M 177/00: Special methods of preparation of lubricating compositions; Chemical modification by after-treatment of components or of the whole of a lubricating composition, not covered by other classes
- C10M 2203/1085: used as base material
- C10M 2219/044: Sulfonic acids, Derivatives thereof, e.g. neutral salts
- C10N 2060/10: by sulfur or a compound containing sulfur
- Y10S 516/909: The agent contains organic compound containing sulfoxy*
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES
- C10M: LUBRICATING COMPOSITIONS (well drilling compositions C09K8/02); USE OF CHEMICAL SUBSTANCES EITHER ALONE OR AS LUBRICATING INGREDIENTS IN A LUBRICATING COMPOSITION (mould release, i.e. separating, agents for metals B22C3/00, for plastics or substances in a plastic state, in general B29C33/56, for glass C03B40/02; textile lubricating compositions D06M11/00, D06M13/00, D06M15/00; immersion oils for microscopy G02B21/33)
- C10N: INDEXING SCHEME ASSOCIATED WITH SUBCLASS C10M RELATING TO LUBRICATING COMPOSITIONS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for upgrading heavy oils by contacting the heavy oil with an inhibitor additive and then thermally treating the inhibitor additized heavy oil. The invention also relates to the upgraded product from the inhibitor enhanced thermal treatment process.

## Claims

### Claim 1

A method for upgrading a heavy oil comprising the steps of:
a) contacting the heavy oil with an effective amount of an inhibitor additive to provide an inhibitor additized heavy oil, which inhibitor additive is represented by the chemical structure:
R-PNA-(X)n
wherein R is an alkyl group containing from 0 to 40 carbon atoms; PNA is a polynuclear aromatic hydrocarbon containing 2 to 15 aromatic rings; X is an acid functionality selected from the group consisting of SO3H, COOH, and PO3H; and n is an integer from 1 to 15; and
b) thermally treating said inhibitor additized heavy oil at a temperature in the range of about 250° C. to 500° C. in the presence of hydrogen at hydrogen partial pressure of between 500 to 2500 psig for a time between 0.1 to 10 hours.

### Claim 2 (depends on 1)

The method of claim 1 wherein the amount of inhibitor additive used is from about 10 to about 50,000 ppm based on the weight of the heavy oil.

### Claim 3 (depends on 1)

The method of claim 1 which is conducted in an inert environment.

### Claim 4 (depends on 1)

The method of claim 1 wherein said contacting is conducted at a temperature from about 25° C. to about 90° C. for a time ranging from about 1 minute to about 24 hours.

### Claim 5 (depends on 1)

The method of claim 1 wherein the heavy oil is selected from the group consisting of crude oil, vacuum resids and atmospheric resids.

### Claim 6 (depends on 1)

The method of claim 1 which further comprises the step of first providing the inhibitor additive with a carrier solvent and then contacting the heavy oil with a mixture of inhibitor additive and carrier solvent.

### Claim 7 (depends on 6)

The method of claim 6 wherein the carrier solvent is selected from the group consisting of water, aromatic hydrocarbon, alcohols and mixtures thereof.

### Claim 8 (depends on 6)

The method of claim 6 wherein the carrier solvent is from about 10 to 80 wt. % of the mixture of inhibitor additive and carrier solvent.

### Claim 9 (depends on 1)

The upgraded oil of claim 1 having at least about 20 wt. % decreased toluene insolubles compared to the untreated heavy oil feedstock obtained by thermal treatment under identical process conditions in the absence of inhibitor.

### Claim 10

A method for upgrading a heavy oil comprising the steps of:
a) contacting the heavy oil with an effective amount of an inhibitor additive to provide an inhibitor additized heavy oil, which inhibitor additive is represented by the chemical structure:
[R-PNA-(SO3−)n]aMb
wherein PNA is a polynuclear aromatic hydrocarbon containing 2 to 15 aromatic rings; X is a sulfonic acid functionality, n is an integer from 1 to 15 representing the number of sulfonic acid functionality on the PNA hydrocarbon; R is an alkyl group containing from 0 to 40 carbon atoms; M is an element selected from the group consisting of Group IV-B, V-B, VI-B, VII-B and VIII of the Long Form of The Periodic Table of Elements; and a and b are integers each ranging from 1 to 4; and
b) thermally treating said inhibitor additized heavy oil at a temperature in the range of about 250° C. to 500° C. in the presence of hydrogen at hydrogen partial pressure of between 500 to 2500 psig for a time between 0.1 to 10 hours.

### Claim 11 (depends on 10)

The method of claim 10 wherein the amount of inhibitor additive used is from about 10 to about 50,000 ppm based on the weight of the heavy oil.

### Claim 12 (depends on 10)

The method of claim 10 which is conducted in an inert environment.

### Claim 13 (depends on 10)

The method of claim 10 wherein said contacting is conducted at a temperature from about 25° C. to about 90° C. for a time ranging from about 1 minute to about 24 hours.

### Claim 14 (depends on 10)

The method of claim 10 wherein the heavy oil is selected from the group consisting of crude oil, vacuum resids and atmospheric resids.

### Claim 15 (depends on 1)

The method of claim 1 which further comprises the step of first providing the inhibitor additive with a carrier solvent and then contacting the heavy oil with a mixture of inhibitor additive and carrier solvent.

### Claim 16 (depends on 15)

The method of claim 15 wherein the carrier solvent is selected from the group consisting of water, aromatic hydrocarbon, alcohols and mixtures thereof.

### Claim 17 (depends on 15)

The method of claim 15 wherein the carrier solvent is from about 10 to 80 wt. % of the mixture of inhibitor additive and carrier solvent.

### Claim 18 (depends on 15)

The method of claim 15 wherein M is selected from Groups VIII and VI-B.

### Claim 19 (depends on 18)

The method of claim 18 wherein M is Mo.

### Claim 20 (depends on 10)

The upgraded oil of claim 10 having at least about 20 wt. % decreased toluene insolubles compared to the untreated heavy oil feedstock obtained by thermal treatment under identical process conditions in the absence of inhibitor.