# US 2005/0278939 A1 · Bismuth oxide superconducting wire rod and process for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0278939 A1
- Document ID: US20050278939A1
- Status: Published application
- Kind: A1
- Application number: 10/531,703
- Filed: 2004-06-14
- Published: 2005-12-22
- Earliest claimed: 2003-06-26
- Assignees: Sumitomo Electric Industries, Ltd.
- Inventors: Naoki Ayai
- Web page: https://patentgrep.com/patent/US20050278939A1

## CPC

- C04B 35/453: based on zinc, tin, or bismuth oxides or solid solutions thereof with other oxides, e.g. zincates, stannates or bismuthates
- C04B 35/4525: {also containing lead oxide}
- H10N 60/0801: {Manufacture or treatment of filaments or composite wires}
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3213: Strontium oxides or oxide-forming salts thereof
- C04B 2235/3281: Copper oxides, cuprates or oxide-forming salts thereof, e.g. CuO or Cu2O
- C04B 2235/3296: Lead oxides, plumbates or oxide forming salts thereof, e.g. silver plumbate
- C04B 2235/3298: Bismuth oxides, bismuthates or oxide forming salts thereof, e.g. zinc bismuthate
- Y10T 29/49014: Superconductor
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention provides a method of manufacturing a bismuth based oxide superconducting wire, comprising steps of preparing a raw material powder, and subjecting the raw material powder to plastic working and heat treatment; wherein the raw material powder contains the superconducting phases containing Bi, Pb, Sr, Ca, Cu, and O in a composition ratio of approximately 2:2:1:2 (Bi+Pb):Sr:Ca:Cu, and the non-superconducting phases containing Pb; wherein the composition ratio (Bi+Pb):Sr:Ca:Cu of the raw material powder is approximately 2:2:2:3; and wherein the ratio of the non-superconducting phases to the superconducting phases is 5 wt % or less; or wherein the raw material powder contains orthorhombic superconducting phases containing Bi, Pb, Sr, Ca, Cu, and 0 in a composition ratio of approximately 2:2:1:2 (Bi+Pb):Sr:Ca:Cu; and wherein the composition ratio (Bi+Pb):Sr:Ca:Cu of the raw material powder is approximately 2:2:2:3.

## Claims

### Claim 1

A method of manufacturing a bismuth based oxide superconducting wire, characterized by the steps of preparing a raw material powder and subjecting the raw material powder to plastic working and heat treatment;
wherein the raw material powder contains superconducting phases comprising Bi, Pb, Sr, Ca, Cu, and O in a composition ration of approximately 2:2:1:2 (Bi+Pb):Sr:Ca:Cu and non-superconducting phases containing Pb;
wherein the composition ratio (Bi+Pb):Sr:Ca:Cu of the raw material powder is approximately 2:2:2:3; and
wherein the ratio of the non-superconducting phases to the superconducting phases is 5 wt % or less.

### Claim 2

A method of manufacturing a bismuth based oxide superconducting wire, characterized by the steps of preparing a raw material powder and subjecting the raw material powder to plastic working and heat treatment;
where the raw material powder contains orthorhombic superconducting phases comprising Bi, Pb, Sr, Ca, Cu, and O in a composition ratio of approximately 2:2:1:2 (Bi+Pb):Sr:Ca:Cu; and
wherein the composition ratio (Bi+Pb):Sr:Ca:Cu of the raw material powder is approximately 2:2:2:3.

### Claim 3

A method of manufacturing a bismuth based oxide superconducting wire, characterized by the steps of:
preparing a raw material powder;
subjecting the raw material powder to heat treatment of 600° C. to 750° C. and at oxygen partial pressure of 0.02 atm or less; and
further performing plastic working and heat treatment on the raw material powder after the heat treatment;
wherein the raw material powder contains Bi, Pb, Sr, Ca, Cu, and O in a composition ratio of approximately 2:2:2:3 (Bi+Pb):Sr:Ca:Cu.

### Claim 4 (depends on 1)

A bismuth based oxide superconducting wire obtained by the manufacturing method according to claim 1.

### Claim 5 (depends on 2)

A bismuth based oxide superconducting wire obtained by the manufacturing method according to claim 2.

### Claim 6 (depends on 3)