# US 2005/0259303 A1 · Long-term high temperature and humidity stable holographic optical data storage media compositions with exceptional high dynamic range

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0259303 A1
- Document ID: US20050259303A1
- Status: Published application
- Kind: A1
- Application number: 10/446,771
- Filed: 2003-05-29
- Published: 2005-11-24
- Earliest claimed: 2002-05-29
- Inventors: Songvit Setthachayanon; Xuan Phan; Mark Michaels; Benjamin Ihas
- Web page: https://patentgrep.com/patent/US20050259303A1

## CPC

- G02B 5/32: Holograms used as optical elements
- G03F 7/001: {Phase modulating patterns, e.g. refractive index patterns}
- G03F 7/027: Non-macromolecular photopolymerisable compounds having carbon-to-carbon double bonds, e.g. ethylenic compounds (G03F7/075 takes precedence)
- G11C 13/046: {using other storage elements storing information in the form of an interference pattern}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- G11C: STATIC STORES (semiconductor memory devices H10B)

## Abstract

A novel photoimageable system for a two-chemistry system containing liquid photoreactive asymmetric acrylate compound containing sulfur, aromatic moieties, and optionally bromine, and an aluminum salt compound is disclosed. The photoimageable system has high dynamic range (M/#) and sensitivity and unexpectedly high temperature and high humidity resistance. The photoimageable system retains its dynamic range when exposed to 60° C. for 4 weeks while a composition without the aluminum salt compound lost 75% of its dynamic range under similar exposure conditions. In one embodiment, 2-10 weight % of a thio-butylacrylate dissolved in a two-component urethane matrix containing 0.002 to 1 weight % of the aluminum salt compound showed a dynamic range of greater than 5 for a 200 microns thick sample and retained more than 80% of the dynamic range after 4 weeks exposure at 60° C.

## Claims

### Claim 1

A photoimageable system comprising an aluminum salt compound and an asymmetric acrylate compound comprising sulfur and aromatic moieties, said asymmetric acrylate compound is liquid at room temperature and said photoimageable system retains at least about 40% of a dynamic range when exposed to 60° C./85%RH for 4 weeks.

### Claim 2 (depends on 1)

The photoimageable system of claim 1, wherein said aluminum salt compound comprises a following formula:
[X−R−N(NO)O]nM2
wherein, X═H, CH3, OCH3, F, Cl, CF3 or SOCH3; R is an aliphatic group, an alicyclic group or an aromatic group having 1-18 carbon atoms; n=0-5; M2 is hydrogen, a group I to III metal, a group VIIIB metal, a substituted NH4 group or an unsubstituted NH4 group.

### Claim 3 (depends on 2)

The photoimageable system of claim 2, wherein M2 is Al3+ with n=3 or M2is NH4+with n=0.

### Claim 4 (depends on 2)

The photoimageable system of claim 2, wherein the photoimageable system is a two-chemistry system.

### Claim 5 (depends on 2)

The photoimageable system of claim 2, wherein the photoimageable system forms an optical article.

### Claim 6 (depends on 1)

The photoimageable system of claim 1, wherein the photoimageable system forms a holographic recording medium having a dynamic range of greater than 3 and a shrinkage of less than 0. 1%.

### Claim 7 (depends on 1)

The photoimageable system of claim 1, wherein the photoimageable system is a two-chemistry system.

### Claim 8 (depends on 1)

The photoimageable system of claim 1, further comprising a matrix precursor.

### Claim 9 (depends on 8)

The photoimageable system of claim 8, wherein said matrix precursor comprises a substance selected from the group consisting of a polyol, an aromatic isocyanate, an aliphatic isocyanate, an aromatic diisocyanate, a hexamethylene diisocyanate, a derivative of hexamethylene diisocyanate and combinations thereof.

### Claim 10 (depends on 8)

The photoimageable system of claim 8, wherein said matrix precursor forms a urethane.

### Claim 11

A photoimageable system comprising an aluminum salt compound and a photoactive compound comprising a chemical structure represented by
wherein R is a phenyl group, a mono- or multi-substituted phenyl group, a bromophenyl group or a naphthalene group; R1 and R3 are a methylene group, an ethylene group, a propylene group, or a butylene group; R2 is H or an alkyl group; and R3 is COCH═CH2, COCCH3═CH2, or CH═CH2.

### Claim 12 (depends on 11)

The photoimageable system of claim 11, wherein said aluminum salt compound comprises a following formula:
[X−R−N(NO)O]nM2
wherein, X═H, CH3, OCH3, F, Cl, CF3 or SOCH3; R is an aliphatic group, an alicyclic group or an aromatic group having 1-18 carbon atoms; n=0-5; M2is hydrogen, a group I to III metal, a group VIIIB metal, a substituted NH4 group or an unsubstituted NH4 group.

### Claim 13 (depends on 12)

The photoimageable system of claim 12, wherein M2 is Al3+ with n=3 or M2is NH4+with n=0.

### Claim 14 (depends on 11)

The photoimageable system of claim 11, wherein the photoimageable system forms an optical article.

### Claim 15 (depends on 11)

The photoimageable system of claim 11, wherein the photoimageable system forms a holographic recording medium having a dynamic range of greater than 3 and a shrinkage of less than 0. 1%.

### Claim 16 (depends on 11)

The photoimageable system of claim 11, wherein the photoimageable system forms a holographic recording medium having a dynamic range of greater than 4 and a shrinkage of less than 0.08%.

### Claim 17 (depends on 11)

The photoimageable system of claim 11, wherein the photoimageable system is a two-chemistry system.

### Claim 18 (depends on 11)

The photoimageable system of claim 11, further comprising a matrix precursor.

### Claim 19 (depends on 18)

The photoimageable system of claim 18, wherein said matrix precursor comprises a substance selected from the group consisting of a polyol, an aromatic isocyanate, an aliphatic isocyanate, an aromatic diisocyanate, a hexamethylene diisocyanate, a derivative of hexamethylene diisocyanate and combinations thereof.

### Claim 20 (depends on 18)

The photoimageable system of claim 18, wherein said matrix precursor forms a urethane.

### Claim 21 (depends on 1)

A method of manufacturing an optical article, comprising:
obtaining the photoimageable system of claim 1 and
reacting at least some ingredients of the photoimageable system to form said optical article.

### Claim 22 (depends on 21)

The method of claim 21, wherein said reacting comprises a polymerization reaction selected from a group consisting of a urethane formation reaction, an urea formation reaction, cationic epoxy polymerization, cationic vinyl ether polymerization, cationic alkenyl ether polymerization, cationic allyl ether polymerization, cationic ketene acetal polymerization, epoxy-amine step polymerization, epoxy-mercaptan step polymerization, unsaturated ester-amine step polymerization, unsaturated ester-mercaptan step polymerization, a hydrosilylation reaction and combinations thereof.

### Claim 23 (depends on 21)

The method of claim 21, wherein the photoimageable system comprises a matrix precursor, said matrix precursor comprising a substance selected from the group consisting of a polyol, an aromatic isocyanate, an aliphatic isocyanate, an aromatic diisocyanate, a hexamethylene diisocyanate, a derivative of hexamethylene diisocyanate and combinations thereof.

### Claim 24 (depends on 21)

The method of claim 21, wherein the photoimageable system comprises a polyol, said polyol comprising a polyol of a material selected from the group consisting of polypropylene oxide, polytetramethylene ether diol and combinations thereof.

### Claim 25 (depends on 21)

The method of claim 21, wherein the optical article is a holographic recording medium.

### Claim 26 (depends on 11)

A method of manufacturing an optical article, comprising:
obtaining the photoimageable system of claim 11 and reacting at least some ingredients of the photoimageable system to form said optical article.

### Claim 27 (depends on 26)

The method of claim 26, wherein said reacting comprises a polymerization reaction selected from a group consisting of a urethane formation reaction, an urea formation reaction, cationic epoxy polymerization, cationic vinyl ether polymerization, cationic alkenyl ether polymerization, cationic allyl ether polymerization, cationic ketene acetal polymerization, epoxy-amine step polymerization, epoxy-mercaptan step polymerization, unsaturated ester-amine step polymerization, unsaturated ester-mercaptan step polymerization, a hydrosilylation reaction and combinations thereof.

### Claim 28 (depends on 26)

The method of claim 26, wherein the photoimageable system comprises a matrix precursor, said matrix precursor comprising a substance selected from the group consisting of a polyol, an aromatic isocyanate, an aliphatic isocyanate, an aromatic diisocyanate, a hexamethylene diisocyanate, a derivative of hexamethylene diisocyanate and combinations thereof.

### Claim 29 (depends on 26)

The method of claim 26, wherein the photoimageable system comprises a polyol, said polyol comprising a polyol of a material selected from the group consisting of polypropylene oxide, polytetramethylene ether diol and combinations thereof.

### Claim 30 (depends on 26)

The method of claim 26, wherein the optical article is a holographic recording medium.

### Claim 31 (depends on 26)

The method of claim 26, wherein said photoimageable system retains at least about 40% of a dynamic range when exposed to 60° C./85% RH for 4 weeks.

### Claim 32 (depends on 26)

The method of claim 26, wherein said photoimageable system retains at least about 60% of a dynamic range when exposed to 60° C./85% RH for 4 weeks.

### Claim 33 (depends on 26)

The method of claim 26, wherein said photoimageable system retains at least about 80% of a dynamic range when exposed to 60° C./85% RH for 4 weeks.

### Claim 34 (depends on 1)

A method recording an interference pattern, comprising:
exposing a holographic recording medium comprising the photoimageable system of claim 1 to an interference pattern;
recording the interference pattern to the holographic recording medium.

### Claim 35 (depends on 34)

The method of claim 34, wherein the holographic recording medium has a dynamic range of greater than 3 and a shrinkage of less than 0. 1%.

### Claim 36 (depends on 34)

The method of claim 34, further comprising exposing the recorded interference pattern to a reference beam to produce a signal beam.

### Claim 37 (depends on 11)

A method recording an interference pattern, comprising:
exposing a holographic recording medium comprising the photoimageable system of claim 11 to an interference pattern;
recording the interference pattern to the holographic recording medium.

### Claim 38 (depends on 37)

The method of claim 37, wherein the holographic recording medium has a dynamic range of greater than 3 and a shrinkage of less than 0. 1%.

### Claim 39 (depends on 37)

The method of claim 37, further comprising exposing the recorded interference pattern to a reference beam to produce a signal beam.