# US 2005/0239969 A1 · Method for the production of polymeric hydroperoxides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0239969 A1
- Document ID: US20050239969A1
- Status: Published application
- Kind: A1
- Application number: 10/521,900
- Filed: 2003-07-30
- Published: 2005-10-27
- Earliest claimed: 2002-07-19
- Inventors: Maximilian Dorn; Eberhard Hagel
- Web page: https://patentgrep.com/patent/US20050239969A1

## CPC

- C08G 77/38: Polysiloxanes modified by chemical after-treatment
- C08G 63/91: Polymers modified by chemical after-treatment
- C08G 65/324: containing oxygen
- C08G 85/004: {Modification of polymers by chemical after-treatment}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Disclosed is a method for producing a polymeric hydroperoxide which forms a radical polymer but no low-molecular radical under redox influence. According to the inventive method, a synthetic polymer containing at least one tertiary hydroxyl group or olefin function is reacted with concentrated hydrogen peroxide and a concentrated mineral acid.

## Claims

### Claim 1

A process for preparing a polymeric hydroperoxide which in a redox reaction forms free-radical polymer but no low molecular weight free radical, characterized in that a synthetic polymer comprising at least one tertiary hydroxyl group or olefin function is reacted with concentrated hydrogen peroxide and a concentrated mineral acid.

### Claim 2 (depends on 1)

The process as claimed in claim 1, characterized in that H2O2 having a concentration of from 50 to 70% is used.

### Claim 3 (depends on 1, 2)

The process as claimed in claim 1 or 2, characterized in that sulfuric acid having a concentration of from 50 to 80% is used as concentrated mineral acid.

### Claim 4

The process as claimed in any of the preceding claims, characterized in that the polymer is used as a solution in an organic solvent.

### Claim 5

The process as claimed in any of the preceding claims, characterized in that a polysiloxane polyol, polyether polyol or polyester polyol is used as starting material.

### Claim 6

The process as claimed in any of the preceding claims, characterized in that the reaction is carried out at a temperature of from +10 to +60° C.