# US 2005/0238796 A1 · Method of fabricating composite cathodes for solid oxide fuel cells by infiltration

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0238796 A1
- Document ID: US20050238796A1
- Status: Published application
- Kind: A1
- Application number: 10/831,384
- Filed: 2004-04-22
- Published: 2005-10-27
- Earliest claimed: 2004-04-22
- Inventors: Tad Armstong; Anil Virkar
- Web page: https://patentgrep.com/patent/US20050238796A1

## CPC

- H01M 4/9066: {of metal-ceramic composites or mixtures, e.g. cermets}
- H01M 4/8885: {Sintering or firing}
- H01M 4/9033: {Complex oxides, optionally doped, of the type M1MeO3, M1 being an alkaline earth metal or a rare earth, Me being a metal, e.g. perovskites}
- H01M 8/1253: the electrolyte containing zirconium oxide
- H01M 2004/8689: {Positive electrodes}
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

In the manufacture of a composite cathode, a porous structure is made of the electrolyte material by sintering a mixed material of primary material of the electrolyte and a secondary material. The mixture is treated to sinter the primary material. The secondary material is removed. The secondary material during sintering inhibits porosity loss and grain growth in the primary material while enabling formation of good necks for interparticle contact. The porous structure is then infiltrated with a liquid that contains precursors of an electrocatalytically active material. The infiltrated structure is then heated to convert the precursors to an electrocatalytically active material.

## Claims

### Claim 1

A method for forming a composite cathode upon a ceramic electrolyte surface comprising:
depositing a two-phase mixture of an oxygen-ion conducting ceramic primary material, and a fugitive or removable secondary material on the ceramic electrolyte surface,
subjecting the mixture to sintering conditions to sinter to the primary material, and the secondary material having properties such that during sintering the secondary material resists densification and grain growth of the primary material under sintering conditions that permit the growth of interparticle contact,
removing the secondary material to form a porous structure of the primary material to form a porous ceramic structure of the primary material,
infiltrating the porous structure with a liquid containing precursors of an electrocatalytically active material, the precursors containing metal ions in the same proportion as that in the electrocatalytically active material;
heating the infiltrated porous structure to a temperature sufficient to convert the precursors to the electrocatalytically active material.

### Claim 2 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the porous ceramic structure comprises one or more of zirconia, ceria, stabilized hafnia, bismuth oxide, and thoria.

### Claim 3 (depends on 2)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 2 wherein the porous ceramic structure comprises one of more of yttria stabilized zirconia, rare-earth-oxide-stabilized zirconia, scandia-stabilized zirconia, rare-earth doped ceria, alkaline-earth doped ceria, stabilized hafnia, rare-earth oxide stabilized bismuth oxide.

### Claim 4 (depends on 2)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 2 wherein the porous ceramic structure comprises one or more of samaria-stabilized ceria (SDC) or La1-xSrxGa1-yMgyO3-δ, (LSGM).

### Claim 5 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the electrocatalytically active material is any one or a mixture of LSM, LSC, LSF, SrFeCo0.5Ox, SrCo0.8Fe0.2O3-δ, La0.8Sr0.2Co08Ni0.2O3-δ, and La0.7Sr0.3Fe0.8Ni0.2O3-δ, La2NiO4, or noble metals.

### Claim 6 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the secondary material is a metal oxide that is reducible to a metal, and wherein the removing the secondary material comprises reducing the metal oxide to the metal to form a cermet of the oxygen-ion conducting ceramic and the metal, and leaching the metal from the cermet.

### Claim 7 (depends on 2)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 2 wherein the metal oxide is one or more of NiO, CuO, FeO, CoO, and ZnO.

### Claim 8 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the secondary material is a metal oxide that is reducible to a metal, and wherein the removing the secondary material comprises reducing the metal oxide to the metal to form a cermet of the oxygen-ion conducting ceramic and the metal, and heating the cermet to melt or vaporize the metal to form the porous structure of the oxygen ion conducting ceramic.

### Claim 9 (depends on 8)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 8 wherein the metal oxide is ZnO.

### Claim 10 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the secondary material is a metal oxide that is non-reactive with the oxygen conducting ceramic, melts at a temperature higher than processing temperatures, and is soluble in a liquid solvent;
and wherein the removing comprises leaching out the metal oxide with the solvent to form the porous structure of the oxygen ion conducting ceramic.

### Claim 11 (depends on 10)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 10 wherein the solvent is water or dilute acid solution, and wherein the metal oxide is one of more of ZnO, LiBO2, K4P2O4.3H2O, K2WO4, AlNaO2, or Al2CaO4.

### Claim 12 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the secondary material is a material reactive with a reactant to form a liquid or gas, and the removing comprises reacting the secondary material with the reactant.

### Claim 13 (depends on 12)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 12 wherein the secondary material is Ni or a material that can form Ni, the reactant is CO, and the reacting forms gas phase Ni(CO)4.

### Claim 14 (depends on 13)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 13 wherein the secondary material is NiO and the secondary material is reduced to Ni by exposure to a reducing atmosphere before reacting with the reactant CO.

### Claim 15 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the secondary material is a pore former that can be decomposed when heated in an oxidizing atmosphere, and the removing comprises heating in an oxidizing atmosphere to decompose the pore former.

### Claim 16 (depends on 15)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 15 wherein the secondary material is one or more of carbon, starch, cellulose, or a polymer

### Claim 17 (depends on 15)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 15 wherein the sintering is in a reducing atmosphere, and thereafter the atmosphere is switched to an oxidizing atmosphere for the heating in an oxidizing atmosphere.

### Claim 18 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the secondary material is a salt that is nonreactive with the oxygen conducting ceramic, melts at a temperature higher than processing temperatures, has low vapor pressure at high temperatures sufficient to inhibit its loss during sintering, and is soluble in a solvent, and the removing comprises treating the composite of the oxygen conducting ceramic and a secondary phase of the secondary material with the solvent to dissolve the salt in the solvent.

### Claim 19 (depends on 18)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 18 wherein the solvent is one or more of water, dilute acid solution, and alcohol, and the salt is soluble in the solvent.

### Claim 20 (depends on 19)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 19 wherein the salt is one or a more of KCl, LiF, K2S, and NaCl.

### Claim 21 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the secondary material is a salt that is nonreactive with the oxygen conducting ceramic, melts at a lower temperature relative to the processing temperature, has a vapor pressure at high temperatures sufficient to be removed, and the removing comprises heat treating the composite of the oxygen conducting ceramic and a secondary phase of the secondary material to a temperature above the melting or boiling point of the salt to remove the salt by vaporization.

### Claim 22 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the liquid for the infiltrating is a solution containing dissolved precursors of the electrocatalytically active material.

### Claim 23 (depends on 22)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 22 wherein the solution contains precursors for the electrocatalytically active material, the electrocatalytically active materials being one or more of LSM, LSC, LSF, SrFeCo0.5Ox, SrCo0.8Fe0.2O3-δ, La0.8Sr0.2Co0.8Ni0.2O3-δ, and La0.7Sr0.3Fe0.8Ni0.2O3-δ, La2NiO4, silver, platinum, palladium, or rhodium.

### Claim 24 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the liquid for the infiltrating is mixture of liquid salts.

### Claim 25 (depends on 1)

A method for forming a composite cathode upon a ceramic electrolyte surface as in claim 1 wherein the heating is at a temperature between 500° C. and 800° C.