# US 2005/0238562 A1 · Systems and methods for synthesis of gallium nitride powders

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0238562 A1
- Document ID: US20050238562A1
- Status: Published application
- Kind: A1
- Application number: 10/997,254
- Filed: 2004-11-24
- Published: 2005-10-27
- Earliest claimed: 2003-11-24
- Assignees: Arizona Board of Regents
- Inventors: Fernando Ponce; Rafael Garcia; Abigail Bell; Alan Thomas; Michael Stevens
- Web page: https://patentgrep.com/patent/US20050238562A1

## CPC

- C30B 29/406: {Gallium nitride}
- C01B 21/0632: {with gallium, indium or thallium}
- C01P 2002/30: Three-dimensional structures
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/84: by UV- or VIS- data
- C01P 2002/85: by XPS, EDX or EDAX data
- C01P 2004/03: obtained by SEM
- C01P 2004/04: obtained by TEM, STEM, STM or AFM
- C01P 2004/11: with a prismatic shape
- C01P 2004/22: with a polygonal circumferential shape
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/52: highly monodisperse size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A method of producing high quality GaN powder by combining high purity gallium and high purity ammonia in a tube reactor under controlled conditions. A reaction between the ammonia and gallium under the controlled conditions produces a porous gallium melt and to a full reaction, yielding high purity crystalline GaN powders with a stoichiometric nitrogen concentration and a hexagonal wurtzite structure.

## Claims

### Claim 1

A method for making gallium nitride, said method comprising the steps of:
subjecting gallium to a temperature between 100° C. and 700° C. in an ammonia flow to dissolve ammonia in the gallium; and then
increasing the temperature to between 1000° C. and 1200° C. to react the ammonia with the gallium to produce a porous, crystalline structure characterized by:
hexagonal columnar micro-crystals having a large distribution in size, and
hexagonal platelets having a small distribution in size,
wherein both the micro-crystals and the platelets have a well defined wurtzite crystalline structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein said subjecting step is carried out for approximately 5 minutes to 2 hours.

### Claim 3 (depends on 2)

The method of claim 2, wherein said subjecting step produces a gallium-ammonia solution and wherein said solution is heated at 1000° C. to 1200° C. for approximately one hour.

### Claim 4 (depends on 1)

The method of claim 1, wherein said crystalline structure is characterized by the absence of a broad emission around 2.214 eV (yellow luminescence).

### Claim 5 (depends on 1)

The method of claim 1, wherein the large distribution is approximately 10μ to 30μ and the small distribution is approximately 0.5μ to 2.0μ.

### Claim 6

A method for making gallium nitride powder, said method comprising the steps of:
dissolving ammonia in liquid gallium; and then
reacting ammonia with the gallium to produce a porous, crystalline structure; and
fracturing the structure to produce a powder.

### Claim 7 (depends on 6)

The method of claim 6, wherein the gallium is of high purity greater than about 99 weight % and the ammonia is of high purity greater than about 99 weight %.

### Claim 8 (depends on 6)

The method of claim 6, wherein the amount of gallium provided is between 1 and 10 grams.

### Claim 9 (depends on 6)

The method of claim 6, wherein the gallium nitride has a nitrogen concentration of about 16.89 weight percent.

### Claim 10 (depends on 6)

The method as of claim 6, wherein said reacting step takes place in an ammonia atmosphere to provide an excess of ammonia for reacting with the gallium.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

Gallium nitride powder made by the method of one of claims 1-10.