# US 2005/0238306 A1 · Method for manufacturing an optical fibre having variations in the refractive index

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0238306 A1
- Document ID: US20050238306A1
- Status: Published application
- Kind: A1
- Application number: 10/751,932
- Filed: 2004-01-07
- Published: 2005-10-27
- Earliest claimed: 2003-01-07
- Assignees: Draka Fibre Technology B.V.
- Inventors: Antonius Elisabeth Breuls; Peter Theodorus Pleunis
- Web page: https://patentgrep.com/patent/US20050238306A1

## CPC

- G02B 6/0288: {Multimode fibre, e.g. graded index core for compensating modal dispersion}
- C03B 37/02718: {Thermal treatment of the fibre during the drawing process, e.g. cooling (coating C03C25/10)}
- G02B 6/02285: {Characterised by the polarisation mode dispersion [PMD] properties, e.g. for minimising PMD (fabrication methods for minimising PMD C03B37/02745)}
- C03B 2203/18: Axial perturbations, e.g. in refractive index or composition
- C03B 2205/56: Annealing or re-heating the drawn fibre prior to coating
- G02B 6/02052: {comprising optical elements other than gratings, e.g. filters (comprising gratings G02B6/02057)}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A method of manufacturing an optical fibre, which method comprises the steps of: i) providing an optical preform, ii) heating one end of said optical preform, iii) drawing an optical fibre from the heated end of the optical preform, iv) cooling the optical fibre, and v) winding the cooled optical fibre onto a reel, with a change in the tension buildup being introduced into the optical fibre in step iv), resulting in variations in the refractive index of the optical fibre as a function of the longitudinal position.

## Claims

### Claim 1

A method of manufacturing an optical fibre, which method comprises the steps of:
i) providing an optical preform,
ii) heating one end of said optical preform,
iii) drawing an optical fibre from the heated end of the optical preform,
iv) cooling the optical fibre, and
v) winding the cooled optical fibre onto a reel, characterized in that a change in the tension buildup is introduced into the optical fibre in step iv), resulting in variations in the refractive index of the optical fibre as a function of the longitudinal position.

### Claim 2 (depends on 1)

A method according to claim 1, characterized in that said change in the tension buildup is effected by locally heating the optical fibre to a temperature ranging between the annealing temperature and the softening temperature.

### Claim 3

A method according to any one of the preceding claims, characterized in that said local heating of the optical fibre takes place at a position along the cooling path where the temperature of the optical fibre is at least 150° C.

### Claim 4

A method according to any one of the preceding claims, characterized in that said local heating is carried out by irradiating the optical fibre with laser light.

### Claim 5 (depends on 4)

A method according to claim 4, characterized in that laser light having a wavelength in the infrared range is used.

### Claim 6 (depends on 4, 5)

A method according to any one or more of the claims 4-5, characterized in that said irradiation is carried out with pulsating laser light.

### Claim 7 (depends on 4, 5, 6)

A method according to any one or more of the claims 4-6, characterized in that said local heating takes place by irradiating the optical fibre with laser light on one side thereof.

### Claim 8 (depends on 4, 5, 6, 7)

A method according to any one or more of the claims 4-7, characterized in that said local heating takes place by irradiating the optical fibre with laser light from different radial positions.

### Claim 9 (depends on 8)

A method according to claim 8, characterized in that said local heating takes place by changing the position of the incident laser light on the optical fibre with respect to the optical fibre.

### Claim 10 (depends on 8)

A method according to claim 8, characterized in that said local heating takes place by changing the position of the surface of the optical fibre to be irradiated with respect to the incident laser light.

### Claim 11

An optical fibre for propagating a signal in different modes, characterized in that the longitudinal length “a” of a change in the tension buildup in the optical fibre and the longitudinal distance “L” between two such changes are in accordance with the following equation:
a<=0.5 L
for at least part of the optical fibre.

### Claim 12

An optical fibre for propagating a signal in different modes, characterized in that the longitudinal length “a” of a change in the tension buildup in the optical fibre and the longitudinal distance “L” between two such changes are in accordance with the following equation:
a≦=0.2 L
for at least part of the optical fibre.

### Claim 13 (depends on 11, 12)

An optical fibre according to any one or more of the claims 11-12, characterized in that the maximum DMD-value for a multimode fibre, optimised in the 850 nm wavelength range, is 0.35 at most.

### Claim 14 (depends on 11, 12)

An optical fibre according to any one or more of the claims 11-12, characterized in that the maximum DMD-value for a multimode fibre, optimised in the 1100 nm wavelength range, is 0.8 at most.

### Claim 15 (depends on 11, 12)

An optical fibre according to any one or more of the claims 11-12, characterized in that the DMD-value for a single mode fibre is 0.06 ps/{square root}km at most.