# US 2005/0237695 A1 · Method for producing dielectric ceramic powder and method for producing composite dielectric material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0237695 A1
- Document ID: US20050237695A1
- Status: Published application
- Kind: A1
- Application number: 11/110,652
- Filed: 2005-04-20
- Published: 2005-10-27
- Earliest claimed: 2004-04-21
- Assignees: TDK Corporation
- Inventors: Isao Kanada; Norimasa Sakamoto
- Web page: https://patentgrep.com/patent/US20050237695A1

## CPC

- H05K 1/0373: {containing additives, e.g. fillers (H05K1/036 takes precedence)}
- C01B 13/145: {After-treatment of oxides or hydroxides, e.g. pulverising, drying, decreasing the acidity}
- C01G 23/006: {Alkaline earth titanates}
- C04B 35/465: based on alkaline earth metal titanates
- C04B 35/4682: {based on BaTiO3 perovskite phase}
- C04B 35/47: based on strontium titanates
- C04B 35/6261: {Milling}
- C04B 35/6262: {of calcined, sintered clinker or ceramics}
- C04B 35/62625: {Wet mixtures}
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C04B 35/80: Fibres, filaments, whiskers, platelets, or the like
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/12: Surface area
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3213: Strontium oxides or oxide-forming salts thereof
- C04B 2235/3215: Barium oxides or oxide-forming salts thereof
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3436: Alkaline earth metal silicates, e.g. barium silicate
- C04B 2235/3454: Calcium silicates, e.g. wollastonite
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/5463: Particle size distributions
- C04B 2235/661: Multi-step sintering
- H05K 3/1291: {Firing or sintering at relative high temperatures for patterns on inorganic boards, e.g. co-firing of circuits on green ceramic sheets}
- H05K 2201/0209: Inorganic, non-metallic particles
- H05K 2203/1126: Firing, i.e. heating a powder or paste above the melting temperature of at least one of its constituents
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A method for producing a dielectric ceramic powder which can secure fluidity of the mixture thereof with a resin, even when produced by milling, is provided. A composite dielectric material which secures, the fluidity of the mixture thereof with a resin and is excellent in dielectric properties can be obtained on the basis of the method for producing a dielectric ceramic powder, comprising a first firing step for firing a starting material at a first temperature to obtain a first fired substance; a first milling step for milling the first fired substance to obtain a first milled substance; a second firing step for firing the first milled substance at a second temperature lower than the first temperature to obtain a second fired substance; and a second milling step for milling the second fired substance to obtain a second milled substance.

## Claims

### Claim 1

A method for producing a dielectric ceramic powder, comprising:
a first firing step for firing a starting material by retaining said starting material at a first temperature to obtain a first fired substance;
a first milling step for milling said first fired substance to obtain a first milled substance;
a second firing step for firing said first milled substance by retaining said first milled substance at a second temperature lower than said first temperature to obtain a second fired substance; and
a second milling step for milling said second fired substance to obtain a second milled substance.

### Claim 2 (depends on 1)

The method for producing a dielectric ceramic powder according to claim 1, wherein:
said first temperature in said first firing step is 1300 to 1650° C., and said second temperature in said second firing step is 1100 to 1300° C.

### Claim 3 (depends on 1)

The method for producing a dielectric ceramic powder according to claim 1, wherein:
the difference between said first temperature and said second temperature is 100° C. or greater.

### Claim 4 (depends on 1)

The method for producing a dielectric ceramic powder according to claim 1, wherein:
the retention time in said second firing step is shorter than that in said first firing step.

### Claim 5 (depends on 1)

The method for producing a dielectric ceramic powder according to claim 1, wherein:
said second milled substance obtained by said second milling step has the largest particle size of 10 μm or less.

### Claim 6 (depends on 5)

The method for producing a dielectric ceramic powder according to claim 5, wherein:
said second milled substance obtained by said second milling step has the largest particle size of 8 μm or less.

### Claim 7 (depends on 1)

The method for producing a dielectric ceramic powder according to claim 1, wherein:
a jet mill is used in said first milling step and said second milling step.

### Claim 8 (depends on 1)

The method for producing a dielectric ceramic powder according to claim 1, wherein:
said dielectric ceramic powder is a composite perovskite ceramic powder.

### Claim 9 (depends on 8)

The method for producing a dielectric ceramic powder according to claim 8, wherein:
said composite perovskite ceramic powder is at least one of (Ba, Sr)-based ceramic, (Ba, Ca)-based ceramic, (Sr, Ca)TiO3-based ceramic and (Ba, Sr, Ca)TiO3-based ceramic.

### Claim 10 (depends on 9)

The method for producing a dielectric ceramic powder according to claim 9, wherein:
said first temperature in said first firing step is 1250 to 1450° C., and said second temperature in said second firing step is 1100 to 1300° C.

### Claim 11 (depends on 1)

The method for producing a dielectric ceramic powder according to claim 1, wherein:
said starting material is a calcined substance obtained by calcining a mixture of raw material powders.

### Claim 12

A method for producing a composite dielectric material comprising a dielectric ceramic powder and an organic resin material for holding said dielectric ceramic powder therein, wherein:
said dielectric ceramic powder is produced through:
a first firing step for firing a starting material by retaining said starting material at a first temperature to obtain a first fired substance;
a first milling step for milling said first fired substance to obtain a first milled substance;
a second firing step for firing said first milled substance by retaining said first milled substance at a second temperature lower than said first temperature to obtain a second fired substance; and
a second milling step for milling said second fired substance to obtain a second milled substance.

### Claim 13 (depends on 12)

The method for producing a composite dielectric material according to claim 12, further comprising:
a mixing step for mixing said dielectric ceramic powder with said organic resin material.

### Claim 14 (depends on 12)

The method for producing a composite dielectric material according to claim 12, wherein:
said first temperature in said first firing step is 1300 to 1650° C., and said second temperature in said second firing step is 1100 to 1300° C.

### Claim 15 (depends on 12)

The method for producing a composite dielectric material according to claim 12, wherein:
a jet mill is used in said first milling step and said second milling step.