# US 2005/0233579 A1 · Method for forming metal wires in semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0233579 A1
- Document ID: US20050233579A1
- Status: Published application
- Kind: A1
- Application number: 10/878,360
- Filed: 2004-06-29
- Published: 2005-10-20
- Earliest claimed: 2004-04-20
- Assignees: Hynix Semiconductor Inc.
- Inventors: Ihl Cho
- Web page: https://patentgrep.com/patent/US20050233579A1

## CPC

- H10W 20/081: {by forming openings in the dielectric parts}
- Y10S 438/96: Porous semiconductor
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

The present invention provides a method that can prevent an anti-diffusion film from being formed defectively on a porous dielectric film due to pores in method for forming metal wires in a semiconductor device in which the porous dielectric film is used as an insulating film between metal wires. The method includes forming a porous dielectric film on a semiconductor substrate as an insulating film between metal wires, selectively etching the porous dielectric film to form an aperture defining a metal wire region, infiltrating sealing particles into pores of the porous dielectric film exposed on the sidewall of the aperture, implementing an annealing process for agglomerating the sealing particles to seal the entrances of the pores of the porous dielectric film exposed on the sidewall of the aperture, forming an anti-diffusion film at the bottom and on the sidewall of the aperture, forming a metal film on the anti-diffusion film, and polishing the metal film and the anti-diffusion film until the top of the porous dielectric film is formed to metal wires within the aperture.

## Claims

### Claim 1

A method for forming metal wires in a semiconductor device, comprising the steps of:
forming a porous dielectric film on a semiconductor substrate as an insulating film between metal wires;
selectively etching the porous dielectric film to form an aperture defining a metal wire region;
infiltrating sealing particles into pores of the porous dielectric film exposed on the sidewall of the aperture;
implementing an annealing process for agglomerating the sealing particles to seal the entrances of the pores of the porous dielectric film exposed on the sidewall of the aperture;
forming an anti-diffusion film at the bottom and on the sidewall of the aperture;
forming a metal film on the anti-diffusion film; and
polishing the metal film and the anti-diffusion film until the top of the porous dielectric film is formed to metal wires within the aperture.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the step of infiltrating the sealing particles into the pores of the porous dielectric film exposed on the sidewall of the aperture comprises the steps of:
impregnating a solution containing the sealing particles into the porous dielectric film; and
annealing the porous dielectric film into which the solution is impregnated.

### Claim 3 (depends on 2)

The method as claimed in claim 2, wherein the dielectric constant of the porous dielectric film is no more than 2.5.

### Claim 4 (depends on 3)

The method as claimed in claim 3, wherein the porous dielectric film into which the solution is impregnated is annealed at a temperature of 100° C. to 300° C.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the sealing particles are metallic particles of at least one kind.

### Claim 6 (depends on 5)

The method as claimed in claim 5, wherein the sealing particles are metallic particles of at least one kind selected from Pt, Ru and Pd.

### Claim 7 (depends on 5)

The method as claimed in claim 5, wherein at least one of H2PtCl6, RuCl3 and PdCl2 is dissolved into the solution containing the sealing particles.

### Claim 8 (depends on 5)

The method as claimed in claim 5, wherein the annealing process for agglomerating the sealing particles is performed at a temperature of 200° C. to 600° C.

### Claim 9 (depends on 8)

The method as claimed in claim 8, wherein the annealing process for agglomerating the sealing particles is performed under a N2, Ar, H2 or He gas atmosphere.

### Claim 10 (depends on 5)

The method as claimed in claim 5, wherein the metal film is formed using a Cu film.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein the anti-diffusion film is formed using Ta or TaN.

### Claim 12 (depends on 5)

The method as claimed in claim 5, wherein the aperture includes a trench and a via connected to the trench.