# US 2005/0233489 A1 · Method for manufacturing electroluminescence display panel and evaporation mask

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0233489 A1
- Document ID: US20050233489A1
- Status: Published application
- Kind: A1
- Application number: 11/142,224
- Filed: 2005-06-01
- Published: 2005-10-20
- Earliest claimed: 2001-08-31
- Inventors: Ryuji Nishikawa; Tsutomu Yamada
- Web page: https://patentgrep.com/patent/US20050233489A1

## CPC

- C23C 14/042: {using masks}
- H10K 71/164: {using vacuum deposition}
- H10K 59/12: Active-matrix OLED [AMOLED] displays
- H10K 59/35: comprising red-green-blue [RGB] subpixels
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

An evaporation mask onto which an opening is formed for selectively allowing passage of an evaporation substance from an evaporation source onto a glass substrate to form an evaporation layer of an electroluminescence element in a predetermined pattern is placed between an evaporation source and a glass substrate and evaporation is performed. As a material for the evaporation mask, a material having a thermal expansion coefficient 160% or smaller of the thermal coefficient of glass is employed so as to minimize the thermal deformation of the evaporation mask which is closer the evaporation source and temperature of which is increased, to thereby improve the evaporation patterning precision.

## Claims

### Claim at position 1

1-8. (canceled)

### Claim 9

A method for manufacturing an electroluminescence display panel in which electroluminescence elements are formed on a glass substrate in a matrix form, wherein
an evaporation mask made of a material having a thermal expansion coefficient of approximately 18.16% of a thermal expansion coefficient of glass is used when a material to be evaporated as an element is vaporized at an evaporation source and is evaporated onto a glass substrate to form an evaporation element layer of an electroluminescence element; and
said evaporation mask is placed between said evaporation source and said glass substrate and said evaporation element layer is patterned simultaneously with evaporation of said material to be evaporated as an element.

### Claim 10 (depends on 9)

A method for manufacturing an electroluminescence display panel according to claim 9, wherein said material for said evaporation mask is an alloy of iron (Fe), nickel (Ni) in an amount of 31% of said iron, and cobalt (Co) in an amount of 5% of said iron.

### Claim 11

A method for manufacturing an electroluminescence display panel in which electroluminescence elements are formed on a glass substrate in a matrix form, wherein
an evaporation mask made of a material having a thermal expansion coefficient of approximately 18.16% of a thermal expansion coefficient of glass is used when a material to be evaporated as an element is vaporized at an evaporation source and is evaporated onto a glass substrate to form an evaporation element layer of an electroluminescence element; and
said evaporation mask is placed between said evaporation source and said glass substrate using a mask supporting mechanism in which a material having a thermal expansion coefficient of approximately 18.16% of said thermal expansion coefficient of glass is used at least for a mask holding section, and said evaporation element layer is patterned simultaneously with evaporation of said material to be evaporated as an element.

### Claim 12 (depends on 11)

A method for manufacturing an electroluminescence display panel according to claim 11, wherein each of said materials for said evaporation mask and for said mask holding section is an alloy of iron (Fe), nickel (Ni) in an amount of 31% of said iron, and cobalt (Co) in an amount of 5% of said iron.

### Claim 13

A method for manufacturing an electroluminescence display panel in which electroluminescence elements are formed on a glass substrate in a matrix form, wherein
when a material to be evaporated as an element is vaporized at an evaporation source and is evaporated onto a glass substrate to form an evaporation element layer of an electroluminescence element, an evaporation mask is placed between said evaporation in which a material having a thermal expansion coefficient of approximately 18.16% of said thermal expansion coefficient of glass is used at least for a mask holding section, and said evaporation element layer is patterned simultaneously with evaporation of said material to be evaporated as an element.

### Claim 14 (depends on 13)

A method for manufacturing an electroluminescence display panel according to claim 13, wherein said material for said mask holding section is an alloy of iron (Fe), nickel (Ni) in an amount of 31% of said iron, and cobalt (Co) in an amount of 5% of said iron.