# US 2005/0233483 A1 · Method of manufacturing semiconductor device, acid etching resistance material and copolymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0233483 A1
- Document ID: US20050233483A1
- Status: Published application
- Kind: A1
- Application number: 11/056,094
- Filed: 2005-02-14
- Published: 2005-10-20
- Earliest claimed: 2004-03-31
- Assignees: Kabushiki Kaisha Toshiba
- Inventors: Koji Asakawa; Kenichi Ohashi; Akira Fujimoto; Takashi Sasaki
- Web page: https://patentgrep.com/patent/US20050233483A1

## CPC

- H10P 54/00: Cutting or separating of wafers, substrates or parts of devices
- C08F 220/281: {and containing only one oxygen, e.g. furfuryl (meth)acrylate or 2-methoxyethyl (meth)acrylate}
- H10P 50/644: {Anisotropic liquid etching (H10P50/61 takes precedence)}
- H10P 50/692: {characterised by their composition, e.g. multilayer masks or materials}
- H10H 20/82: Roughened surfaces, e.g. at the interface between epitaxial layers
- H10P 72/0426: {with the semiconductor substrates being dipped in baths or vessels}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

Disclosed is an acid etching resistance material comprising a compound having a repeating unit represented by the following general formula (1): (in the general formula (1), R1 is a hydrogen atom or methyl group; R3 is a cyclic group selected from an alicyclic group and an aromatic group; R4 is a polar group; R2 is a group represented by the following general formula (2); and j is 0 or 1): (in the general formula (2), R5 is a hydrogen atom or methyl group).

## Claims

### Claim 1

A method of manufacturing a semiconductor device comprising a semiconductor substrate having a first electrode provided above the rear surface thereof and roughened side surfaces; a light emitting layer formed above the semiconductor substrate; and a second electrode provided above the light emitting layer or above the rear surface; said method comprising:
forming a protective film above an entire surfaces of the semiconductor substrate including the first electrode, the light emitting layer and the second electrode, excluding the side surfaces, the protective film comprising an acid etching resistance material having a repeating unit represented by the following general formula (1):
(in the general formula (1), R1 is a hydrogen atom or methyl group; R3 is a cyclic group selected from an alicyclic group and an aromatic group; R4 is a polar group; R2 is a group represented by the following general formula (2); and j is 0 or 1:
(in the general formula (2), R5 is a hydrogen atom or methyl group);
treating the semiconductor substrate having the protective film formed thereof with an acidic etching solution; and
removing the protective film with an alkaline solution.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the acidic etching solution is a mixed solution comprising hydrochloric acid and aqueous hydrogen peroxide, and the method further comprising dicing the semiconductor substrate provided with the protecting film prior to treating the semiconductor substrate with the mixed solution.

### Claim 3 (depends on 2)

The method according to claim 2, further comprising immersing the semiconductor substrate into concentrated hydrofluoric acid after treating the semiconductor substrate with the mixed solution comprising hydrochloric acid and aqueous hydrogen peroxide, thereby etching sidewalls of the semiconductor substrate to form a rugged surface.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising immersing the semiconductor substrate into concentrated hydrofluoric acid, thereby etching sidewalls of the semiconductor substrate to form a rugged surface.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the concentrated hydrofluoric acid contains hydrofluoric acid at a concentration of 25% or more.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the protecting film comprising a lower protecting film, and further comprising an upper protecting film on the lower protecting film.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the upper protecting film is formed of a novolac resin.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the semiconductor device is a light emitting element.

### Claim 9

An acid etching resistance material comprising a compound having a repeating unit represented by the following general formula (1):
(in the general formula (1), R1 is a hydrogen atom or methyl group; R3 is a cyclic group selected from an alicyclic group and an aromatic group; R4 is a polar group; R2 is a group represented by the following general formula (2); and j is 0 or 1):
(in the general formula (2), R5 is a hydrogen atom or methyl group).

### Claim 10 (depends on 9)

The acid etching resistance material according to claim 9, wherein the cyclic group to be introduced as R3 into the general formula (1) is selected from the group consisting of adamantane, norbornane, cyclohexane and benzene ring.

### Claim 11 (depends on 9)

The acid etching resistance material according to claim 9, wherein the polar group to be introduced as R4 into the general formula (1) is selected from the group consisting of carboxyl group, hydroxyl group and ketone.

### Claim 12 (depends on 9)

The acid etching resistance material according to claim 9, further comprising not more than 50% by weight of hydrophobic low molecular compound.

### Claim 13 (depends on 12)

The acid etching resistance material according to claim 12, wherein the hydrophobic low molecular compound is naphthoquinone diazide.

### Claim 14

A copolymer comprising:
40 to 70 mol % of 3-hydroxy-1-methacryloyloxy-adamantane represented by the following chemical formula (A2); and
the balance of 2-acryloyloxypropyl phthalate represented by the following chemical formula (A4):

### Claim 15

An acid etching resistance material comprising:
a resin having at least two kinds of repeating units represented by the following general formula (PS1); and
a photo acid generator which is capable of generating an acid as it is irradiated with light:
(in the general formula (PS1), R11 and R13 are individually a hydrogen atom or methyl group; R12 is selected from the group consisting of adamantane, tricyclodecane, norbornane, isobornane, cyclohexane and cyclooctane, each having one or two hydroxyl groups; R14 is selected from the group consisting of adamantane, tricyclodecane, norbornane, isobornane, cyclohexane and cyclooctane, each having one ketone groups; and m and n represent individually a natural number).

### Claim 16 (depends on 15)

The acid etching resistance material according to claim 15, wherein R11 and R13 are individually a hydrogen atom, and R12 is selected from the group consisting of adamantane, tricyclodecane, norbornane, isobornane, cyclohexane and cyclooctane, each having a single hydroxyl group.

### Claim 17 (depends on 16)

The acid etching resistance material according to claim 16, wherein R12 is adamantane having a single hydroxyl group, and R14 is adamantane having a single ketone group.

### Claim 18 (depends on 15)

The acid etching resistance material according to claim 15, wherein the ratio of m:n is confined within the range of 30:70 to 70:30.

### Claim 19

A method of manufacturing a semiconductor device comprising:
forming a layer of a photosensitive etching resistance material on a substrate made of semiconductor or quartz glass, the photosensitive etching resistance material comprising an acid etching resistance material composed of a resin having at least two kinds of repeating units represented by the following general formula (PS1); and a photo acid generator which is capable of generating an acid as it is irradiated with light:
(in the general formula (PS1), R11 and R13 are individually a hydrogen atom or methyl group; R12 is selected from the group consisting of adamantane, tricyclodecane, norbornane, isobornane, cyclohexane and cyclooctane, each having one or two hydroxyl groups; R14 is selected from the group consisting of adamantane, tricyclodecane, norbornane, isobornane, cyclohexane and cyclooctane, each having one ketone groups; and m and n represent individually a natural number):
subjecting the substrate to patterning exposure;
heating the substrate;
subjecting the substrate to a developing treatment using an alkaline developing solution; and
subjecting the substrate to a fluoric acid etching treatment using a solution containing fluoric acid at a concentration ranging from 30% to 50%.

### Claim 20

A method of manufacturing a semiconductor device comprising:
forming a sacrificial layer composed of quartz glass on a semiconductor substrate;
forming an element structure composed of semiconductor on the sacrificial layer;
forming a region composed of a material which is poor in hydrofluoric acid resistance on the semiconductor substrate;
covering the region composed of a material which is poor in hydrofluoric acid resistance with a photosensitive etching resistance material comprising an acid etching resistance material composed of a resin having at least two kinds of repeating units represented by the following general formula (PS1); and a photo acid generator which is capable of generating an acid as it is irradiated with light:
(in the general formula (PS1), R11 and R13 are individually a hydrogen atom or methyl group; R12 is selected from the group consisting of adamantane, tricyclodecane, norbornane, isobornane, cyclohexane and cyclooctane, each having one or two hydroxyl groups; R14 is selected from the group consisting of adamantane, tricyclodecane, norbornane, isobornane, cyclohexane and cyclooctane, each having one ketone groups; and m and n represent individually a natural number); and
removing the sacrificial layer by applying a hydrofluoric acid solution to the semiconductor substrate.

### Claim 21

A method of manufacturing a semiconductor device comprising:
forming a region of a material which is excellent in hydrofluoric acid resistance on a semiconductor substrate;
forming a region of a material which is poor in hydrofluoric acid resistance over the region which is composed of a material which is excellent in hydrofluoric acid resistance;
covering the region which is poor in hydrofluoric acid resistance with a photosensitive etching resistance material comprising an acid etching resistance material composed of a resin having at least two kinds of repeating units represented by the following general formula (PS1); and a photo acid generator which is capable of generating an acid as it is irradiated with light:
(in the general formula (PS1), R11 and R13 are individually a hydrogen atom or methyl group; R12 is selected from the group consisting of adamantane, tricyclodecane, norbornane, isobornane, cyclohexane and cyclooctane, each having one or two hydroxyl groups; R14 is selected from the group consisting of adamantane, tricyclodecane, norbornane, isobornane, cyclohexane and cyclooctane, each having one ketone groups; and m and n represent individually a natural number); and
subjecting the region which is composed of a material which is excellent in hydrofluoric acid resistance to an etching treatment using a solution of hydrofluoric acid.