# US 2005/0231118 A1 · Non-lead glass, glass powder for covering electrodes and plasma display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0231118 A1
- Document ID: US20050231118A1
- Status: Published application
- Kind: A1
- Application number: 11/155,652
- Filed: 2005-06-20
- Published: 2005-10-20
- Earliest claimed: 2003-07-18
- Assignees: Asahi Glass Company, Limited
- Inventors: Satoshi Fujimine; Hiroshi Usui; Masaki Torimoto; Masamichi Tanida
- Web page: https://patentgrep.com/patent/US20050231118A1

## CPC

- C03C 3/068: containing rare earths
- C03C 3/066: containing zinc
- C03C 17/02: with glass (C03C17/34, C03C17/44 take precedence)
- H01J 2211/38: Dielectric or insulating layers
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Non-lead glass consisting essentially of, as represented by mol %, from 20 to 50% of B2O3, from 5 to 35% of SiO2, from 10 to 30% of ZnO, from 0 to 10% of Al2O3, from 0 to 10% of SrO, from 6 to 16% of BaO, from 2 to 16% of Li2O, from 0 to 10% of Na2O+K2O, from 0 to 9% of Bi2O3, and from 0 to 2% of CuO+CeO2, wherein (B2O3+SiO2+Al2O3)/(Bi2O3+BaO) is at least 3.25, and MgO+CaO is at most 8 mol %. Further, a plasma display device wherein transparent electrodes formed on a glass substrate constituting a front substrate, or electrodes formed on a glass substrate constituting a rear substrate, are covered by the non-lead glass.

## Claims

### Claim 1

Non-lead glass consisting essentially of, as represented by mol % based on the following oxides, from 20 to 50% of B2O3, from 5 to 35% of SiO2, from 10 to 30% of ZnO, from 0 to 10% of Al2O3, from 0 to 10% of SrO, from 6 to 16% of BaO, from 2 to 16% of Li2O, from 0 to 10% of Na2O+K2O, from 0 to 9% of Bi2O3, and from 0 to 2% of CuO+CeO2, wherein (B2O3+SiO2+Al2O3)/(Bi2O3+BaO) is at least 3.25, and when MgO and/or CaO is contained, MgO+CaO is at most 8 mol %.

### Claim 2 (depends on 1)

The non-lead glass according to claim 1, wherein B2O3+SiO2+Al2O3 is at least 46 mol %.

### Claim 3 (depends on 1)

The non-lead glass according to claim 1, wherein, as represented by mol %, SiO2 is at least 7%, Al2O3 is from 0 to 8%, SrO is from 0 to 5%, Li2O is at least 2.5%, ZnO+Na2O+K2O is at most 30%, CuO is at least 0.2%, and when MgO and/or CaO is contained, MgO+CaO is at most 3%.

### Claim 4 (depends on 1)

The non-lead glass according to claim 1, wherein Li2O+Na2O+K2O is at most 16%.

### Claim 5 (depends on 1)

The non-lead glass according to claim 1, which contains no Bi2O3 or contains Bi2O3 in a range of less than 1 mol %.

### Claim 6 (depends on 1)

The non-lead glass according to claim 1, wherein Bi2O3 is at least 1 mol %, and CuO+CeO2 is at least 0.2 mol %.

### Claim 7

Non-lead glass consisting essentially of, as represented by mol % based on the following oxides, from 20 to 50% of B2O3, from 5 to 35% of SiO2, from 10 to 30% of ZnO, from 0 to 10% of Al2O3, from 0 to 10% of SrO, from 6 to 16% of BaO, from 2 to 16% of Li2O, from 0 to 10% of Na2O+K2O, and from 0 to 2% of CuO+CeO2, and containing no Bi2O3.

### Claim 8 (depends on 7)

The non-lead glass according to claim 7, wherein CuO+CeO2 is at least 0.2 mol %.

### Claim 9 (depends on 1)

The non-lead glass according to claim 1, wherein, as represented by mol %, B2O3 is from 23 to 38%, SiO2 is from 6 to 23%, ZnO is from 21 to 28%, Al2O3 is from 4 to 6%, BaO is from 8 to 11%, Li2O is from 10 to 15%, and Na2O+K2O is from 0.5 to 6%, or Li2O is from 8 to 15% and Na2O+K2O is from 2 to 6%.

### Claim 10 (depends on 1)

The non-lead glass according to claim 1, wherein as represented by mol %, B2O3 is from 29 to 39%, SiO2 is from 12 to 23%, ZnO is from 20 to 28%, Al2O3 is from 2 to 8%, BaO is at most 14%, Li2O is at most 13%, Na2O+K2O is from 0 to 6%, and CuO+CeO2 is at least 0.2 mol %.

### Claim 11 (depends on 1)

The non-lead glass according to claim 1, which has a softening point of from 450 to 650° C. and an average linear expansion coefficient of from 60×10−7 to 90×10−7/° C. at from 50 to 350° C.

### Claim 12 (depends on 1)

The non-lead glass according to claim 1, which has a specific permittivity of at most 9.5 at 1 MHz.

### Claim 13 (depends on 1)

A plasma display device comprising a front substrate to be used as a display surface, a rear substrate and barrier ribs to define cells, wherein transparent electrodes on a glass substrate constituting the front substrate are covered by the non-lead glass as defined in claim 1.

### Claim 14 (depends on 1)

A plasma display device comprising a front substrate to be used as a display surface, a rear substrate and barrier ribs to define cells, wherein electrodes on a glass substrate constituting the rear substrate are covered by the non-lead glass as defined in claim 1.

### Claim 15 (depends on 1)

A glass powder for covering electrodes, which comprises a powder of the non-lead glass as defined in claim 1.