# US 2005/0229857 A1 · Support fixture for semiconductor wafers and associated fabrication method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0229857 A1
- Document ID: US20050229857A1
- Status: Published application
- Kind: A1
- Application number: 10/826,730
- Filed: 2004-04-16
- Published: 2005-10-20
- Earliest claimed: 2004-04-16
- Assignees: SEH America, Inc.
- Inventors: David Beauchaine; Aaron Newton
- Web page: https://patentgrep.com/patent/US20050229857A1

## CPC

- C23C 16/4581: {characterised by material of construction or surface finish of the means for supporting the substrate}
- C23C 16/24: Deposition of silicon only
- C23C 16/325: {Silicon carbide}
- C23C 16/4587: {the substrate being supported substantially vertically}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A support fixture is provided that includes a boat, a first layer deposited on at least a portion of the boat that has fewer impurities than the boat, and a second layer deposited on at least a portion of the first layer that is formed of a material having one or both of a hardness and a coefficient of thermal expansion that more closely matches the material properties of the wafers to be carried by the support fixture than does those of the boat and the first layer. For example, the boat and the first layer may be formed of silicon carbide and the second layer may be formed of polysilicon. A method of fabricating a support fixture having a boat coated with first and second layers, such as by sequential chemical vapor deposition steps, is also provided.

## Claims

### Claim 1

A support fixture for holding at least one wafer comprising:
a boat comprised of a material selected from the group consisting of silicon carbide and graphite;
a first layer on at least a portion of said boat and comprised of silicon carbide; and
a second layer on at least a portion of said first layer and comprised of polysilicon.

### Claim 2 (depends on 1)

A support fixture according to claim 1 wherein said first layer has a greater purity than said boat.

### Claim 3 (depends on 1)

A support fixture according to claim 1 wherein said second layer has a hardness that more closely matches a hardness of the at least one wafer than a hardness of said boat.

### Claim 4 (depends on 1)

A support fixture according to claim 1 wherein said second layer has a coefficient of thermal expansion that more closely matches a coefficient of thermal expansion of the at least one wafer than a coefficient of thermal expansion of said boat.

### Claim 5 (depends on 1)

A support fixture according to claim 1 wherein said first layer completely surrounds said boat.

### Claim 6 (depends on 1)

A support fixture according to claim 1 wherein said first and second layers are chemical vapor deposition layers.

### Claim 7

A support fixture for holding at least one wafer comprising:
a boat;
a first layer on at least a portion of said boat, wherein said first layer has a greater purity than said boat; and
a second layer on at least a portion of said first layer, wherein said second layer is formed of a different material than said first layer and said boat, and wherein said second layer has at least one material property selected from the group consisting of: (i) a hardness that more closely matches a hardness of the at least one wafer than a hardness of said boat, and (ii) a coefficient of thermal expansion that more closely matches a coefficient of thermal expansion of the at least one wafer than a coefficient of thermal expansion of said boat.

### Claim 8 (depends on 7)

A support fixture according to claim 7 wherein said first layer and said boat are comprised of silicon carbide.

### Claim 9 (depends on 7)

A support fixture according to claim 7 wherein said second layer is comprised of polysilicon.

### Claim 10 (depends on 7)

A support fixture according to claim 7 wherein said first layer completely surrounds said boat.

### Claim 11 (depends on 7)

A support fixture according to claim 7 wherein said first and second layers are chemical vapor deposition layers.

### Claim 12

A method of fabricating a support fixture for holding at least one wafer comprising:
providing a boat comprised of a material selected from the group consisting of silicon carbide and graphite;
depositing a first layer of silicon carbide on at least a portion of said boat; and
depositing a second layer of polysilicon on at least a portion of the first layer.

### Claim 13 (depends on 12)

A method according to claim 12 wherein depositing the first layer comprises depositing the first layer so as to completely surround the boat.

### Claim 14 (depends on 12)

A method according to claim 12 wherein depositing the first layer comprises depositing the first layer via chemical vapor deposition.

### Claim 15 (depends on 12)

A method according to claim 12 wherein depositing the second layer comprises depositing the second layer via chemical vapor deposition.

### Claim 16

A method of fabricating a support fixture for holding at least one wafer comprising:
depositing a first layer on at least a portion of a boat, wherein depositing the first layer comprises depositing a first layer that has a greater purity than the boat; and
depositing a second layer on at least a portion of the first layer, wherein depositing the second layer comprises depositing a second layer that is formed of a different material than the first layer and the boat and that has at least one material property selected from the group consisting of: (i) a hardness that more closely matches a hardness of the at least one wafer than a hardness of the boat, and (ii) a coefficient of thermal expansion that more closely matches a coefficient of thermal expansion of the at least one wafer than a coefficient of thermal expansion of the boat.

### Claim 17 (depends on 16)

A method according to claim 16 wherein the boat is comprised of silicon carbide, and wherein depositing the first layer comprises depositing a first layer comprised of silicon carbide.

### Claim 18 (depends on 16)

A method according to claim 16 wherein depositing the second layer comprises depositing a second layer comprised of polysilicon.

### Claim 19 (depends on 16)

A method according to claim 16 wherein depositing the first layer comprises depositing the first layer so as to completely surround the boat.

### Claim 20 (depends on 16)

A method according to claim 16 wherein depositing the first layer comprises depositing the first layer via chemical vapor deposition.

### Claim 21 (depends on 16)

A method according to claim 16 wherein depositing the second layer comprises depositing the second layer via chemical vapor deposition.